Control of crystallographic orientation of monocrystalline nickel castings heat-resistant alloys by X-ray diffractometry

Kuzmina N.A., Pyankova L.A.
Kuzmina N.A., Pyankova L.A. Control of crystallographic orientation of monocrystalline nickel castings heat-resistant alloys by X-ray diffractometry // Proceedings of VIAM. 2019. No. 12. DOI: 10.18577/2307-6046-2019-0-12-11-19. URL: https://viam-works.ru/en/journal/2019/12/2
Keywords
crystallographic orientation of single crystals, x-ray diffraction, curved position-sensitive detector, control of crystallographic orientation.
Abstract

The article analyzes the methods of x-ray diffraction used to assess the quality of the structure of single-crystal castings of heat-resistant nickel alloys. The results of determination of crystallographic orientation of single crystals of nickel heat-resistant alloys obtained on an x-ray diffractometer equipped with a curved position-sensitive detector are presented. The data of optimal shooting conditions for obtaining a «swing» curve in order to control the crystallographic orientation of single-crystal castings are presented.

Reference list
  1. Petrushin N.V., Ospennikova O.G., Svetlov I.L. Monokristallicheskie zharoprochnye nikelevye splavy dlya turbinnyh lopatok perspektivnyh GTD [Single-crystal Ni-based superalloys for turbine blades of advanced gas turbine engines] // Aviacionnye materialy i tehnologii. 2017. №S. S. 72−103. DOI: 10.18577/2071-9140-2017-0-S-72-103.
  2. Kablov E.N., Sidorov V.V., Kablov D.E., Min P.G. Metallurgicheskie osnovy obespecheniya vysokogo kachestva monokristallicheskih zharoprochnyh nikelevykh splavov [The metallurgical fundamentals for high quality maintenance of single crystal heat-resistant nickel alloys] // Aviacionnye materialy i tehnologii. 2017. №S. S. 55–71. DOI: 10.18577/2071-9140-2017-0-S-55-71.
  3. Tolorayya V.N., Kablov E.N., Demonis I.M. Tekhnologiya polucheniya monokristallicheskikh otlivok turbinnykh lopatok GTD zadannoy kristallograficheskoy oriyentatsii iz reniysoderzhashchikh zharoprochnykh splavov [The technology for producing single-crystal castings of turbine engine turbine blades of a given crystallographic orientation from rhenium-containing heat-resistant alloys] // Liteynyye zharoprochnyye splavy. Effekt S.T. Kishkina. M.: Nauka, 2006. S. 206–219.
  4. Kablov E.N., Bondarenko Yu.A., Kablov D.E. Osobennosti struktury i zharoprochnyh svojstv monokristallov 001> vysokorenievogo nikelevogo zharoprochnogo splava, poluchennogo v usloviyah vysokogradientnoj napravlennoj kristallizacii [Features of structure and heat resisting properties of monocrystals of 001> high-rhenium nickel hot strength alloys received in the conditions of high-gradient directed crystallization] // Aviacionnye materialy i tehnologii. 2011. №4. S. 25–31.
  5. Kablov E.N., Bondarenko Yu.A., Echin A.B. Issledovaniye vliyaniya peremennogo upravlyayemogo temperaturnogo gradiyenta na osobennosti struktury, fazovyy sostav, svoystva vysokotemperaturnykh zharoprochnykh splavov pri ikh napravlennoy kristallizatsii [Investigation of the influence of a variable controlled temperature gradient on structural features, phase composition, and properties of high-temperature heat-resistant alloys during their directed crystallization] // Vestnik MGTU im. N.E. Baumana. Ser.: Mashinostroyeniye. 2016. №6 (111). S. 43–61.
  6. Tolorayya V.N., Kablov E.N., Svetlov I.L., Orekhov N.G., Golubovskiy E.R. Anizotropiya prochnostnykh kharakteristik v monokristallakh nikelevykh zharoprochnykh splavov [Anisotropy of strength characteristics in single crystals of nickel heat-resistant alloys] // Gornyy informatsionno-analiticheskiy byulleten. 2005. Spetsvypusk. S. 225–236.
  7. Toloraya V.N., Kablov E.N., Orekhov N.G., Ostroukhova G.A. Struktura i rostovyye defekty monokristallov nikelevykh zharoprochnykh splavov [Structure and growth defects of single crystals of heat-resistant nickel alloys] // Gornyy informatsionno-analiticheskiy byulleten. 2005. Spetsvypusk. S. 190–202.
  8. Nazarkin R.M., Kolodochkina V.G., Ospennikova O.G., Orlov. M.R. Izmeneniya mikrostruktury monokristallov zharoprochnyh nikelevyh splavov v processe dlitelnoj ekspluatacii turbinnyh lopatok [The microstructure modifications of single crystals of Ni-based superalloys in time-tested turbine blades] // Aviacionnye materialy i tehnologii. 2016. №4 (45). S. 9–17. DOI: 10.18577/2071-9140-2016-0-4-9-17.
  9. Nazarkin R.M. Rentgenodifrakcionnye metodiki precizionnogo opredeleniya parametrov kristallicheskih reshetok nikelevyh zharoprochnyh splavov (kratkij obzor) [X-ray diffraction techniques for precise determination of lattice constants in Ni-based superalloys: a brief review] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 41–48. DOI: 10.18577/2071-9140-2015-0-1-41-48.
  10. Sidokhin E.F., Sidokhin F.A., Khayutin S.G. O substrukture monokristallicheskikh lopatok GTD [About the substructure of single-crystal GTE blades] // Aviatsionnaya promyshlennost. 2009. №1. S. 34–36.
  11. Sidokhin F.A., Sidokhin A.F., Sidokhin E.F. Ob opredelenii kristallograficheskoy oriyentatsii monokristallov metodom Laue [On the determination of the crystallographic orientation of single crystals by the Laue method] // Zavodskaya laboratoriya. Diagnostika materialov. 2009. T. 75. №1. S. 35–37.
  12. Potrakhov N.N., Khayutin S.G., Lifshits V.A., Oses R. Ustanovka PRDU-KROS dlya ekspressnogo opredeleniya kristallograficheskoy oriyentatsii kubicheskikh monokristallov po obratnym lauegrammam [Installation of PRDU-CROS for the express determination of the crystallographic orientation of cubic single crystals by inverse lauegrams] // Zavodskaya laboratoriya. Diagnostika materialov. 2015. T. 81. №8. S. 27–30.
  13. Kuzmina N.A., Lifshits V.A., Potrakhov E.N., Potrakhov N.N. Sravnitelnyj kontrol struktury monokristallicheskikh otlivok nikelevykh zharoprochnykh splavov rentgenovskimi difraktsionnymi metodami «kachaniya» i Laue [Comparative structure control of single-crystal castings of nickel superalloys x-ray diffraction methods of oscillation and Laue] // Trudy VIAM: elektron. nauch.-tekhnich. zhurn. 2019. №9 (81). St. 02. Available at: http://www.viam-works.ru (accessed: October 12, 2019). DOI: 10.18577/2307-6046-2019-0-9-15-25.
  14. Lisoyvan V.I., Zadneprovskiy G.M. K metodike opredeleniya oriyentatsii kristallograficheskoy ploskosti v monokristalle na difraktometre [On the methodology for determining the orientation of the crystallographic plane in a single crystal on a diffractometer] // Apparatura i metody rentgenovskogo analiza. 1969. Vyp. 4. S. 64–70.
  15. Kheyker D.M. Rentgenovskaya difraktometriya monokristallov [X-ray diffractometry of single crystals]. L.: Mashinostroyeniye, 1973. 256 s.
  16. Pyankova L.A., Elokhin V.A., Arkhipov S.N. i dr. Kontrol funktsionalnykh sloyev VTSP-2 s pomoshchyu teksturnoy pristavki rentgenovskogo difraktometra «Difrey-401» [Control of the functional layers of HTSC-2 using the texture attachment of the X-ray diffractometer «Difrey-401»] // Zavodskaya laboratoriya. Diagnostika materialov. 2016. №82 (10). S. 44–46.
  17. Goganov D.A., Kazanskiy B.V., Klimenskaya D.A. i dr. Pozitsionno-chuvstvitelnye detektory myagkogo rentgenovskogo izlucheniya i ikh primeneniye [Position-sensitive soft x-ray detectors and their application] // Pribory i tekhnika eksperimenta. 2015. №1. S. 109–116.
  18. Makro- i mikrostruktura nikelevykh zharoprochnykh splavov, prednaznachennykh dlya monokristalnogo litya lopatok [Macro and microstructure of heat-resistant nickel alloys intended for single-crystal casting of blades]. Available at: https://studme.org/151298/tehnika/ makro_mikrostruktura_nikelevyh_zharoprochnyh_splavov_prednaznachennyh_monokristalnogo_litya_lopatok (accessed: October 14, 2019).