Fractography features of interlaminar crack growth in carbon fibre reinforced plastic under various mode loading

Gulyaev A.I., Yakovlev N.O., Oreshko E.I.
Gulyaev A.I., Yakovlev N.O., Oreshko E.I. Fractography features of interlaminar crack growth in carbon fibre reinforced plastic under various mode loading // Proceedings of VIAM. 2019. No. 12. DOI: 10.18577/2307-6046-2019-0-12-99-108. URL: https://viam-works.ru/en/journal/2019/12/11
Keywords
polymer composite, fracture toughness, mixed mode I+II, fracture mechanics, failure analysis, delamination, phase morphology, fractography.
Abstract

The interlaminar fracture toughness characteristics were experimentally determined under conditions of opening (mode I), forward shear (mode II), and combined loading (at various opening and shear ratios) of unidirectional epoxy polysulfone carbon fiber reinforced plastic. Based on the results of fractographic analysis, the fracture microrelief characteristic elements are identified and the change in the microstructure of the fracture surfaces with changing loading conditions is presented. A scheme is proposed for the formation of a shear microrelief for carbon fiber polymer composite with a matrix continuous phase morphology.

Reference list
  1. Zichenkov M.Ch., Kondakov I.O., Shanygin A.N. Novyy podkhod k sozdaniyu legkikh i nadezhnykh silovykh kompozitnykh aviakonstruktsiy [A new approach to creating lightweight and reliable power composite aircraft structures] // Nauchnyy Vestnik MGTU GA. 2016. №6. S. 127–136.
  2. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  3. Kablov E.N. Kompozity: segodnya i zavtra [Composite materials: today and tomorrow] // Metally Evrazii. 2015. №1. S. 36–39.
  4. Raskutin A.E. Strategiia razvitiia polimernykh kompozitsionnykh materialov [Development strategy of polymer composite materials] // Aviaсionnye materialy i tehnologii. 2017. №S. S. 344–348. DOI: 10.18577/2071-9140-2017-0-S-344-348.
  5. Mukhametov R.R., Petrova A.P. Termoreaktivnyye svyazuyushchiye dlya polimernykh kompozitsionnykh materialov (obzor) [Thermosetting binders for polymer composites (review)] // Aviaсionnye materialy i tehnologii. 2019. №3 (56). S. 48–58. DOI: 10.18577/2071-9140-2019-0-3-48-58.
  6. Kablov E.N., Chursova L.V., Babin A.N., Mukhametov R.R., Panina N.N. Razrabotki FGUP «VIAM» v oblasti rasplavnykh svyazuyushchikh dlya polimernykh kompozitsionnykh materialov [Developments of FSUE VIAM in the field of melt binders for polymer composite materials] // Polimernye materialy i tekhnologii. 2016. №2. S. 37–42.
  7. Ushakov A.E. Obshchaya postanovka i skhema resheniya zadachi obespecheniya bezopasnosti aviakonstruktsiy iz PKM s uchetom ikh povrezhdayemosti [General statement and scheme for solving the problem of ensuring the safety of aircraft structures from PCM, taking into account their damageability] // Izvestiya Samarskogo nauchnogo tsentra Rossiyskoy akademii nauk. 2012. №4. S. 339–347.
  8. Babayevskiy P.G., Kulik S.G. Treshchinostoykost otverzhdennykh polimernykh kompozitsiy [Crack resistance of cured polymer compositions]. M.: Khimiya, 1991. 336 s.
  9. Greenhalgh E.S. Characterisation of mixed-mode delamination growth in carbon-fibre composites: thesis, PhD. London: Imperial College, 1998. 306 p.
  10. Charalambous G., Allegri G., Hallett S.R. Temperature effects on mixed mode I/II delamination under quasi-static and fatigue loading of a carbon/epoxy composite // Composites: Part A. 2015. Vol. 77. P. 75–86.
  11. Panina N.N., Chursova L.V., Babin A.N., Grebeneva T.A., Gurevich YA.M. Osnovnyye sposoby modifikatsii epoksidnykh polimernykh materialov v Rossii [The main methods of modifying epoxy polymeric materials in Russia] // Vse materialy. Entsiklopedicheskiy spravochnik. 2014. №9. S. 10–17.
  12. Mouritz A.P., Chang P., Cox B.N. Flexural properties of z-pinned laminates // Composites Part A. 2007. Vol. 38. P. 244–251.
  13. Platonov A.A. Polimernye kompozicionnye materialy na osnove proshitogo napolnitelya s povyshennoj udarostojkostyu [Polymer composite materials on a base of stitched preforms with high impact resistance] // Aviacionnye materialy i tehnologii. 2014. №4. S. 43–47. DOI: 10.18577/2071-9140-2014-0-4-43-47.
  14. Lin S., Cai Q., Ji J. et. al. Electrospun nanofiber reinforced and toughened composites through in situ nano-interface formation // Composite Science and Technology. 2008. Vol. 68. P. 3322–3329.
  15. Lobanov M.V., Gulyayev A.I., Babin A.N. Povysheniye udaro- i treshchinostoykosti epoksidnykh reaktoplastov i kompozitov na ikh osnove s pomoshch'yu dobavok termoplastov kak modifikatorov [Polymer composite materials based on stitched filler with increased impact resistance] // Vysokomolekulyarnyye soyedineniya. Ser. B. 2016. №1. S. 3–15.
  16. Mimura K., Ito H., Fujioka H. Improvement of thermal and mechanical properties by control of morphologies in PES-modified epoxy resins // Polymer. 2000. Vol. 41. P. 4451–4459.
  17. Pearson R.A., Yee A.F. Toughening mechanisms in thermoplastic-modified epoxies: 1. Modification using poly(phenylene oxide) // Polymer. 1993. Vol. 34. No. 17. P. 3658–3670.
  18. Greenhalgh E.S. Failure analysis and fractography of polymer composites. Cambridge: Woodhead Publishing Limited, 2009. 528 p.
  19. Tamuzh V.P., Kuksenko V.S. Mikromekhanika razrusheniya polimernykh materialov [Micromechanics of the destruction of polymeric materials]. Riga: Zinatne, 1978. 294 s.
  20. Gulyaev A.I., Yakovlev N.O., Krylov V.D., Lashov O.A. Primeneniye fraktograficheskogo analiza pri issledovanii mezhsloyevogo razrusheniya PKM [Application of fractographic analysis in the study of interlayer fracture of PCM] // Aviaсionnye materialy i tehnologii. 2017. №3 (48). S. 65–73. DOI: 10.18577/2071-9140-2017-0-3-65-73.
  21. Chalykh A.E., Gerasimov V.K., Bukhteyev A.E. i dr. Sovmestimost i evolyutsiya fazovoy struktury smesey polisul'fon–otverzhdayushchiyesya epoksidnyye oligomery [Compatibility and evolution of the phase structure of polysulfone – curable epoxy oligomers mixtures] // Vysokomolekulyarnyye soyedineniya. Ser. A. 2003. №7. S. 1148–1159.
  22. Gorbatkina Yu.A., Ivanova-Mumzhiyeva V.G., Kuperman A.M. Adgeziya modifitsirovannykh epoksidnykh matrits k armiruyushchim voloknam [Adhesion of modified epoxy matrices to reinforcing fibers] // Vysokomolekulyarnyye soyedineniya. Ser. A. 2016. №5. S. 439–447.
  23. Gulyaev A.I., Yakovlev N.O., Shurtakov S.V., Lashov O.A. Vliyaniye temperatury i klimaticheskogo vozdeystviya na mekhanizm mezhsloyevogo razrusheniya ugleplastika po mode I [The influence of temperature and climatic effects on the mechanism of interlayer destruction of carbon fiber according to mode I] // Vse materialy. Entsiklopedicheskiy spravochnik. 2017. №10. S. 23–30.