Application of computer modeling methods in the manufacture of complex-contoured shaped casting

Duyunova V.A., Molodtsov S.V., Leonov A.A., Trapeznikov A.V.
Duyunova V.A., Molodtsov S.V., Leonov A.A., Trapeznikov A.V. Application of computer modeling methods in the manufacture of complex-contoured shaped casting // Proceedings of VIAM. 2019. No. 11. DOI: 10.18577/2307-6046-2019-0-11-3-11. URL: https://viam-works.ru/en/journal/2019/11/1
Keywords
ProCast, SolidWorks, computer modeling, foundry equipment, core box, magnesium alloy, porosity, 3D-model.
Abstract

This article discusses the stages of manufacturing models from the magnesium complex, including the development of computer models, the development of models and experimental models, calculation and analysis of the results when developing models of virtual bays using software systems. Various methods of supplying molten metal to a selected embodiment are considered. Work was carried out to prevent possible defects in the ProCast program. As a result, the work was carried out with the help of equipment printed on a 3D-printer, sand forms.

Reference list
  1. Kablov E.N. Nastoyashcheye i budushcheye additivnykh tekhnologiy [Present and future of additive technologies] // Metally Evrazii. 2017. №1. S. 2–6.
  2. Kablov E.N. VIAM: prodolzheniye puti [VIAM: continuation of the path] // Nauka v Rossii. 2012. №3. S. 36–44.
  3. Kablov E.N. Sovremennyye materialy – osnova innovatsionnoy modernizatsii Rossii [Modern materials - the basis of innovative modernization of Russia] // Metally Evrazii. 2012. №3. S. 10–15.
  4. Kablov E.N. Osnovnyye itogi i napravleniya razvitiya materialov dlya perspektivnoy aviatsionnoy tekhniki [The main results and directions of the development of materials for advanced aviation technology] // 75 let. Aviatsionnyye materialy. Izbrannyye trudy «VIAM» 1932–2007: yubil. nauch.-tekhnich. sb. M.: VIAM, 2007. S. 20–26.
  5. Kablov E.N. Klyuchevaya problema – materialy [The key problem is materials] // Tendentsii i oriyentiry innovatsionnogo razvitiya Rossii. M.: 2015. S. 458–470.
  6. Vlasova K.A., Klyukvina T.D., Leonov A.A., Larionov S.A. Vzaimodejstvie modelnykh sostavov s plastikovoj osnastkoj, izgotovlennoj s pomoshchyu tekhnologii 3D-pechati [Interaction of model compositions with plastic equipment made using 3D printing technology] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2018. №2. St. 07. URL: http://www.viam-works.ru (accessed: February 05, 2019). DOI: 10.18577/2307-6046-2018-0-2-7-7.
  7. Tekhnologiya liteynogo proizvodstva: lit'ye v peschanyye formy: ucheb. dlya vuzov / pod red. A.P. Trukhova, Yu.A. Sorokina, M.Yu. Ershova i dr. [Foundry technology: sand casting: textbook. for universities / ed. A.P. Trukhov, Yu.A. Sorokin, M.Yu. Ershov et al.]. M.: Akademiya, 2005. 582 s.
  8. Shangguan H., Kang J., Deng C. et al. 3D-printed shell – truss sand mold for aluminum castings // Journal of Materials Processing Technology. 2017. Vol. 250. P. 247–253.
  9. Duyunova V.A., Nechaykina T.A., Oglodkov M.S., Yakovlev A.L., Leonov A.A. Perspektivnyye razrabotki v oblasti legkikh materialov dlya sovremennoy aviakosmicheskoy tekhniki [Promising developments in the field of light materials for modern aerospace engineering] // Tekhnologiya legkikh splavov. 2018. №4. S. 28–43.
  10. Zuev A.V., Loshchinin Yu.V., Barinov D.Ya., Marakhovskij P.S. Raschetno-eksperimentalnye issledovaniya teplofizicheskikh svojstv [Computational and experimental investigations of thermophysical properties] // Aviacionnye materialy i tehnologii. 2017. №S. S. 575–595. DOI: 10.18577/2071-9140-2017-0-S-575-595.
  11. Fu J., Wang K. Modelling and Simulation of Die Casting Process for A356 Semi-solid Alloy // Procedia Engineering. 2014. Vol. 81. P. 1565–1570.
  12. Ngo T.D., Kashani A., Imbulzano G. et al. Additive manufacturing (3D printing): a review of materials, methods, applications and challenges // Composites Part B: Engineering. 2018. Vol. 143. P. 172–196.
  13. Mikhaylova A.E., Doshina A.D. 3D printer – tekhnologiya budushchego [3D printer – technology of the future] // Molodoy uchenyy. 2015. №20. S. 40–44. Available at: https://moluch.ru/archive/100/22467/ (accessed: February 05, 2019).
  14. Volkova E.F., Duyunova V.A. O sovremennykh tendentsiyakh razvitiya magniyevykh splavov [On current trends in the development of magnesium alloys] // Tekhnologiya legkikh splavov. 2016. №3. S. 94–105.
  15. Trofimov N.V., Leonov A.A. Protivoprigarnyye pokrytiya, ispolzuyemyye dlya litya form i sterzhney iz KhTS, primenyayemykh pri litye magniyevykh splavov (obzor) [Nonstick coating is used for molds and cores of the CTS used in the casting magnesium alloys (review)] // Trudy VIAM: elektron. nauch.-tekhnich. zhurn. 2017. №12 (60). St. 10. Available at: http://www.viam-works.ru (accessed: February 13, 2019). DOI: 10.18577/2307-6046-2017-0-12-10-10.
  16. Klyukvina T.D., Vlasova K.A., Leonov A.A., Yashina S.A. Izuchenie mekhanizma obrazovaniya prochnosti v samotverdeyushchikh smesyakh s fenolnym svyazuyushchim (obzor) [Study of the mechanism of formation of strength in self-hardening mixtures with a phenolic binder (review)] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2018. №3. St. 03. Available at: http://viam-works.ru (accessed: Mart 21, 2019). DOI: 10.18577/2307-6046-2018-0-3-18-27.
  17. Kang H.T., Ostrom T. Mechanical behavior of the cast and forged magnesium alloys and their microstructures // Material Science and Engineering: A. 2008. Vol. 490. Issue 1–2. P. 52–56.
  18. Chen L., Wang Y., Peng L. et al. Study on the interfacial heat transfer coefficient between AZ91D magnesium alloy and silica sand // Experimental Thermal and Fluid Science. 2014. Vol. 54. P. 196–203.
  19. Bruna M., Bolgibruchova D., Pastircak R. Numerical Simulation of Porosity for Al Based Alloys // Procedia Engineering. 2017. Vol. 177. P. 488–495.
  20. Koktsinskaya E.M. Tekhnologiya 3D-pechati: obzor poslednikh novostey [3D printing technology: a review of the latest news] // Videonauka. 2016. №2 (2). Available at: https://cyberleninka.ru/article/n/tehnologiya-3d-pechati-obzor-poslednih-novostey (accessed: February 05, 2019).
  21. Platonov M.M., Petrova G.N., Larionov S.A., Barbotko S.L. Optimizatsiya sostava polimernoy kompozitsii s ponizhennoy pozharnoy opasnostyu na osnove polikarbonata dlya tekhnologii 3D-pechati rasplavlennoy polimernoy nityu [Optimization of the composition of the polymer composition with reduced fire hazard based on polycarbonate for 3D printing technology with molten polymer thread] // Izvestiya vuzov. Ser.: Khimiya i khimicheskaya tekhnologiya. 2017. T. 60. №1. S. 87–94.
  22. Smirnov O.I., Skorodumov S.V. Modelirovaniye tekhnologii posloynogo sinteza pri razrabotke izdeliy slozhnoy formy [Modeling the technology of layer-by-layer synthesis in the development of products of complex shape] // Sovremennyye naukoyemkiye tekhnologii. 2010. №4. S. 83–87.
  23. Dudek P. FDM 3D printing technology in manufacturing composite elements // Archives of Metallurgy and Materials. 2013. Vol. 58. Issue 4. DOI: 10.2478/amm-2013-0186.
  24. Lakedemonskiy A.V., Kvasha F.S., Mendeleyev Ya.I. i dr. Liteynye defekty i sposoby ikh ustraneniya [Foundry defects and methods for their elimination]. M.: Mashinostroyeniye, 1972. 152 s.
  25. Proizvodstvo tochnykh otlivok [Production of precision castings] / I. Doshkarzh, Ya. Gabriyel, M. Gousht, M. Pavelka . M.: Mashinostroyeniye, 1979. 296 s.
  26. Boychuk A.S. Nerazrushayushchiy kontrol detaley i konstruktsiy aviatsionnoy tekhniki iz polimernykh kompozitsionnykh materialov pri ispolzovanii ultrazvukovykh fazirovannykh reshetok [Non-destructive testing of parts and structures of aircraft from polymer composite materials using ultrasonic phased arrays] // Tez. dokl. 19-y Vseros. nauch.-tekhnich. konf. po nerazrushayushchemu kontrolyu i tekhnicheskoy diagnostike. Samara, 2011. S. 289–291.
  27. Zhukovskiy S.S. Kholodnotverdeyushchiye svyazuyushchiye smesi dlya liteynykh sterzhney i form: spravochnik [Cold hardening binders for foundry cores and molds: reference]. M.: Mashinostroyeniye, 2010. 256 s.