Effect of heat treatment on mechanical properties and structure of high-strength metastable β-titanium alloy with experimental composition

Nochovnaya N.A., Shiryaev A.A.
Nochovnaya N.A., Shiryaev A.A. Effect of heat treatment on mechanical properties and structure of high-strength metastable β-titanium alloy with experimental composition // Proceedings of VIAM. 2018. No. 6. DOI: 10.18577/2307-6046-2018-0-6-22-29. URL: https://viam-works.ru/en/journal/2018/6/3
Keywords
heat treatment, microstructure, mechanical properties.
Abstract

The effect of various modes and technological parameters of hardening heat treatment on mechanical properties and structure of sheets from an experimental composition of a high-strength metastable β-titanium alloy doped with rare-earth element yttrium have been studied.

It has been shown the possibility of wide variation within parameters and morphology of structural constituents of the experimental alloy composition. The experimental alloy can be effectively strengthened both by conventional heat treatment and low-temperature thermo-mechanical treatment (LTMT). Long-term low-temperature ageing makes it possible to provide high level of strength characteristics with satisfactory values of elongation and impact toughness.

Reference list
  1. Moiseev V.N. Beta-titanovye splavy i perspektivy ikh razvitiya [Beta titanium alloys and perspectives of their development] // Metallovedenie i termicheskaya obrabotka metallov. 1998. №12. S. 11–14.
  2. Boyer R.R., Briggs R.D. The Use of β Titanium Alloys in the Aerospace Industry // Journal of Materials Engineering and Performance. 2005. Vol. 14 (6). P. 681–685.
  3. Nyakana S.L., Fanning J.C., Boyer R.R. Quick Reference Guide for β Titanium Alloys in the 00s // Journal of Materials Engineering and Performance. 2005. Vol. 14 (6). P. 799–811.
  4. Titanium and titanium alloys. Fundamentals and applications / Ed. by C. Leyens, M. Peters. Wiley–VCH, Germany. 2003. 513 p.
  5. Ilin A.A., Kolachev B.A., Polkin I.S. Titanovye splavy. Sostav, struktura, svojstva: spravochnik [Titanium alloys. Structure, structure, properties: directory]. M.: VILS–MATI. 2009. 520 s.
  6. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  7. Vysokoprochnyj splav na osnove titana i izdelie, vypolnennoe iz vysokoprochnogo splava na osnove titana: pat. 2569285 Ros. Federaciya. №2014153690/02 [High-strength alloy on the basis of titanium and the product executed from high-strength alloy on the basis of titanium: pat. 2569285 Rus. Federation. No. 2014153690/02]; zayavl. 29.12.2014; opubl. 20.11.2015, Byul. №32.
  8. Shiriaev A.A., Antashev V.G. Osobennosti razrabotki vysokoprochnogo samozakalivaiushchegosia vysokotekhnologichnogo psevdo-β-titanovogo splava [Peculiarities of development of advanced high-strength self-hardening high-processable pseudo-β-titanium alloys] // Aviatsionnye materialy i tekhnologii. 2014. №4. S. 23–30. DOI: 10.18577/2071-9140-2014-0-4-23-30.
  9. Kablov E.N., Ospennikova O.G., Vershkov A.V. Redkie metally i redkozemelnye elementy – materialy sovremennyh i budushhih vysokih tehnologij [Rare metals and rare-earth elements are materials for modern and future high technologies] // Aviacionnye materialy i tehnologii. 2013. №S2. S. 3–10.
  10. Kablov E.N., Volkova E.F., Filonova E.V. Vliyanie RZE na fazovyj sostav i svojstva novogo zharoprochnogo magnievogo splava sistemy Mg–Zn–Zr–RZE [Influence of RZE on phase structure and property of new heat resisting magnesium alloy of Mg-Zn-Zr-RZE system] // Metallovedenie i termicheskaya obrabotka metallov. 2017. №7 (745). S. 19–26.
  11. Kashapov O.S., Pavlova T.V., Kalashnikov V.S., Kondrateva A.R. Issledovanie vliyaniya rezhimov termicheskoj obrabotki na strukturu i svojstva opytnykh pokovok iz splava VT41 s melkozernistoj strukturoj [The influence of heat treatment conditions on structure and properties of pilot forgings from VT41 alloy with fine grained structure] // Aviacionnye materialy i tehnologii. 2017. №3. S. 3–7. DOI: 10.18577/2071-9140-2017-0-3-3-7.
  12. El-Chaikh A., Schmidt P., Christ H.-J. Study on the Beneficial Effects of Duplex Aging on Microstructure Phenomena Determining the Fatigue life of the Metastable β-titanium Alloy Ti 38-644 // Ti-2011 Science and Technology: Proceedings of the 12th World Conference on Titanium. Beijing: Science Press Beijing, 2011. Vol. 1. P. 745–749.
  13. Santhosh R., Geetha M., Nageswara Rao M. Recent developments in heat treatment of beta titanium alloys for aerospace applications // Transactions Indian Institute of Metals. 2017. Vol. 70 (7). P. 1681–1688.
  14. Khorev A.I. Kompleksnoe legirovanie i termomekhanicheskaya obrabotka titanovykh splavov: ucheb. posobie [Complex alloying and thermomechanical processing of titanium alloys]. M.: Mashinostroenie, 1979. 228 s.
  15. Suzuki T., Niwa N., Goto K., Kobayashi M. et al. Effect of aging on the mechanical properties of beta titanium alloys of Ti–13V–11Cr–3Al, Ti–15V–3Cr–3Sn–3Al and Ti–3Al–8V–6Cr–4Mo–4Zr // Titanium 95: Science and technology. 1995. P. 1294–1301.