The study of the mechanism of self-hardening mixtures friability (review)
Yashina S.A., Klyukvina T.D. The study of the mechanism of self-hardening mixtures friability (review) // Proceedings of VIAM. 2018. No. 6. DOI: 10.18577/2307-6046-2018-0-6-110-118. URL: https://viam-works.ru/en/journal/2018/6/11
Keywords
sand casting, self-hardening mixtures, friability, casting defects, surface strength of mould, binder.
Abstract
In this work using of self-hardening mixtures to manufacture castings is studied. The information about appliance of different sand mixtures in the world foundry industry is given. Different kinds of resins, advantages and disadvantages of mixtures made with these resins are discussed. Affecting on friability factors are studied. Casting defects caused by increased friability of the mold are analyzed. Optimal values of friability necessary to obtain qualitative forms are given.
Reference list
- Kukuj D.M., Skvortsov V.A., Andrianov N.V. Teoriya i tekhnologiya litejnogo proizvodstva: uchebnik v 2 ch. [Theory and technology of foundry production: the textbook in 2 parts]. Minsk: Novoe znanie; M.: INFRA-M, 2013. Ch. 1: Formovochnye materialy i smesi. 384 s.
- Global Casting Production Growth Salls // Modern Casting Journal. December, 2017. P. 25–28. Available at: https://www.moderncasting.com/issues/december-2017 (accessed: May 15, 2018).
- Leonov A.A., Duyunova V.A., Stupak E.V., Trofimov N.V. Lite magnievyh splavov v razovye formy, poluchennye novymi metodami [Casting of magnesium alloys in disposable moulds produced by new methods] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №12. St. 01. Available at: http://www.viam-works.ru (accessed: May 28, 2018). DOI: 10.18577/2307-6046-2014-0-12-1-1.
- The U.S. Portreit By the Nummers // Modern Casting Journal. January, 2016. P. 35–38. Available at: https://www.moderncasting.com/issues/january-2016 (accessed: May 15, 2018).
- Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace materials science] // Vse materialy. Entsiklopedicheskij spravochnik. 2008. №3. S. 2–14.
- Kablov E.N. Strategicheskie napravleniya razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda [The strategic directions of development of materials and technologies of their processing for the period to 2030] // Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
- Kablov E.N. Osnovnye itogi i napravleniya razvitiya materialov dlya perspektivnoj aviatsionnoj tekhniki [The main results and the directions of development of materials for perspective aviation engineering ] // 75 let. Aviacionnye materialy. Izbrannye trudy «VIAM» 1932–2007: yubil. nauch.-tehnich. sb. M.: VIAM, 2007. S. 20–26.
- Zhukovskij S.S. Kholodnotverdeyushchie svyazuyushchie i smesi dlya litejnykh sterzhnej i form: spravochnik [Cold-hardering binding and mixes for foundry rods and forms: directory]. M.: Mashinostroenie, 2010. 256 s.
- Tekhnologicheskie protsessy i oborudovanie dlya modernizatsii proizvodstva v mashinostroenii (formy, sterzhni): sbornik rukovodyashchikh tekhnicheskikh materialov [Technological processes and the equipment for production modernization in mechanical engineering (forms, rods): collection of leading engineering materials]. M.: Metallurg, 2009. 289 s.
- Duyunova V.A., Mukhina I.YU., Uridiya Z.P. Novye protivoprigarnye prisadochnye materialy dlya litejnykh form magnievykh otlivok [New parting filler materials materials for casting molds of magnesian casting] // Litejnoe proizvodstvo. 2009. №9. S. 18–21.
- Galante G. Formovka s primeneniem KhTS. Nash vzglyad [Molding using CHM. Our look]. Italiya: IMF Luino, 1997. Ch. 2. 343 s.
- Galante G. Formovka s primeneniem KhTS [Molding using CHM. Our look]. Nash vzglyad. Italiya: IMF Luino, 1997. Ch. 1. 161 s.
- Klyukvina T.D., Vlasova K.A., Leonov A.A., Yashina S.A. Izuchenie mekhanizma obrazovaniya prochnosti v samotverdeyushchikh smesyakh s fenolnym svyazuyushchim (obzor) [Study of the mechanism of formation of strength in self-hardening mixtures with a phenolic binder (review)] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2018. №3. St. 03. Available at: http://viam-works.ru (accessed: May 28, 2018). DOI: 10.18577/2307-6046-2018-0-3-3.
- Tekhnologiya litejnogo proizvodstva: Formovochnye i sterzhnevye smesi / pod red. S.S. Zhukovskogo, A.N. Boldina, A.I. Yakovleva i dr. [Technology of foundry production: Forming and rod mixes / ed. by S.S. Zhukovskiy, A.N. Boldin, A.I. Yakovlev et al.]. Bryansk: Izd-vo BGTU, 2003. 470 s.
- Zhukovskij S.S. Prochnost litejnoj formy [Durability of casting mold]. M.: Mashinostroenie, 1989. 288 s.
- Khandewal H., Ravi B. Effect of molding parameters on chemically bonded sand mold properties // Journal of Manufacturing Processes. 2016. Vol. 22. P. 127–133. Available at: https://www.sciencedirect.com/science/article/pii/S1526612516300093 (accessed: May 15, 2018).
- Boldin A.N., Davydov N.I., Zhukovskij S.S. Litejnye formovochnye materialy. Formovochnye, sterzhnevye smesi i pokrytiya: spravochnik [Foundry molding materials. Forming, rod mixes and coverings: directory]. M.: Mashinostroenie, 2006. 507 s.
- Kablov E.N. Sovremennye materialy – osnova innovatsionnoj modernizatsii Rossii [Modern materials – basis of innovative modernization of Russia] // Metally Evrazii. 2012. №3. S. 10–15.
- Kaftannikov A.S., Nuraliev F.A., Stepashkin Yu.A. Svojstva zhidkostekolnykh KhTS s ponizhennym soderzhaniem svyazuyushchego [Properties of liquivitreous y CHM with the lowered maintenance of the binding] // Litejnoe proizvodstvo. 2015. №1. S. 31–33.
- Duyunova V.A., Volkova E.F., Uridiya Z.P., Trapeznikov A.V. Dinamika razvitiya magnievyh i litejnyh alyuminievyh splavov [Dynamics of the development of magnesium and cast aluminum alloys] // Aviacionnye materialy i tehnologii. 2017. №S. S. 225–241. DOI: 10.18577/2071-9140-2017-0-S-225-241.
- Duyunova V.A., Kozlov I.A. Kholodnotverdeyushchie formovochnye smesi: perspektivy ispolzovaniya pri lite magnievykh splavov [Cold-hardening mixture: use perspectives when molding magnesium alloys] // Vse materialy. Entsiklopedicheskij spravochnik. 2011. №1. S. 41–43.
- Volkova E.F. Analiz i itogi Mezhdunarodnoj konferencii «Magnij–21. Novye gorizonty» (obzor) [The analysis and results of the International conference «Magnesium–21. Broad horizons» (review)] // Aviacionnye materialy i tehnologii. 2016. №1 (40). S. 86–94. DOI: 10.18577/2071-9140-2016-0-1-86-94.