Comparative analysis of mechanical properties anisotropy and microstructure of semi-finished products from high-strength magnesium alloys with REE

Volkova E.F., Mostyaev I.V., Akinina M.V.
Volkova E.F., Mostyaev I.V., Akinina M.V. Comparative analysis of mechanical properties anisotropy and microstructure of semi-finished products from high-strength magnesium alloys with REE // Proceedings of VIAM. 2018. No. 5. DOI: 10.18577/2307-6046-2018-0-5-24-33. URL: https://viam-works.ru/en/journal/2018/5/4
Keywords
high strength magnesium alloys, anisotropy of mechanical properties, technology of deformation, structure, phase structure, rare earth elements.
Abstract

In recent years the problem of flight vehicles weight reduction becomes the most actual. At replacement of details from aluminum alloys on detail from high-strength magnesium alloys the weight economy about 20–25% can be reached. One of shortcomings of the deformed semi-finished products of high-strength magnesium alloys is anisotropy of their mechanical properties. It is conditionally possible to consider two types of anisotropy, in view of structural sign: – crystal (homogeneous) anisotropy; – heterogeneous (fibrous) anisotropy. For magnesium alloys both types of anisotropy are inherent. Anisotropy of mechanical properties can be reduced by applying the complicated scheme of deformation of material for receiving better structure and due to alloying magnesium, in particular, by rare earth metals (RE). The comparative analysis of results of microstructure research, phase structure research, mechanical properties and their anisotropy, investigation on example of high strength MA1

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Volkova E.F., Akinina M.V., Mostyaev I.V. Puti povysheniya osnovnyh mehanicheskih harakteristik magnievyh deformiruemyh splavov [The ways of rising of wrought magnesium alloys main mechanical characteristics] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2017. №10 (58). St. 02. Available at: http://www.viam-works.ru (accessed: February 20, 2018). DOI: 10.18577/2307-6046-2017-0-10-2-2.
  3. Velikij V.I., Yaresko K.I., Shalomeev V.A. i dr. Perspektivnye magnievye splavy s povyshennym urovnem svojstv dlya aviadvigatelestroeniya [Perspective magnesium alloys with the raised level of properties for aviaengine building] // Metallovedenie i termicheskaya obrabotka metallov. 2013. №9. C. 32–38.
  4. Kablov E.N., Ospennikova O.G., Vershkov A.V. Redkie metally i redkozemelnye elementy – materialy sovremennyh i budushhih vysokih tehnologij [Rare metals and rare-earth elements are materials for modern and future high technologies] // Aviacionnye materialy i tehnologii. 2013. №S2. S. 3–10.
  5. Kablov E.N. Nauka kak otrasl ekonomiki [Science as economy industry] // Nauka i zhizn. 2009. №10. S. 7–8.
  6. Kablov E.N., Volkova E.F., Filonova E.V. Issledovanie vliyaniya RZE na fazovyj sostav i svojstva novogo zharoprochnogo magnievogo splava sistemy Mg–Zn–Zr–RZE [Research of influence of REE on phase structure and properties of new heat resisting magnesium alloy of Mg–Zn–Zr–REE system] // Metallovedenie i termicheskaya obrabotka metallov. 2017. №7. S. 19–26.
  7. Drits M.E., Rokhlin L.L., Padezhnova E.M. i dr. Magnievye splavy s ittriem [Magnesium alloys with yttrium]. M.: Nauka, 1979. 162 s.
  8. Rokhlin L.L. Magnievye splavy, soderzhashchie redkozemelnye metally [The magnesium alloys containing rare earth metals]. M.: Nauka, 1980. 192 s.
  9. Rokhlin L.L. Struktura i svojstva splavov sistemy Mg–RZM [Structure and properties of alloys of Mg–REM system] // Metallovedenie i termicheskaya obrabotka metallov. 2006. №11. S. 18–22.
  10. Landkof B. Magnesium Alloys and Their Application // Proceedings of International Congress (Germany, Sept. 26–28, 2000). Weinheim, 2000. P. 168–172.
  11. Kainer Karl Ulrich. Magnesium alloys for structural application // Minerals, Metals and Material Society. 2000. Vol. 52. No. 11. P. 198–199.
  12. Volkova E.F. Nekotorye zakonomernosti formirovaniya fazovogo sostava magnievogo splava sistemy Mg–Zn–Zr–Y [Some patterns of forming of phase composition of magnesium alloy of Mg–Zn–Zr–Y system] // Metallovedenie i termicheskaya obrabotka metallov. 2013. №9. C. 22–28.
  13. Bohlen J., Yi S.B., Letzig D., Kainer K.U. Effect of rare earths elements on the microstructure and texture development in magnesium-manganese alloys during extrusion // Materials Science Engineering. 2010. Vol. 527. P. 7092–7098.
  14. Dobroň P., Chmelík F., Yi S. et. al. Grain size effects on deformation twinning in an extruded magnesium alloy tested in compression // Scripta Metallurgica. 2011. No 65. P. 424–427.
  15. Koike I. New Deformation Mechanisms in Fine-Grain Mg Alloys // Proceedings of Conference Magnesium Alloys 2003 // Materials Science Forum. 2003. Vol. 419–422. P. 189–194.
  16. Shao X.H., Yang Z.Q., Ma X.L. Strengthening and toughening mechanisim in Mg–Zn–Y alloy with a long period stacking ordered structure // Acta Metallurgica. 2010. Vol. 58. No. 14. P. 4760–4771.
  17. Jiang L., Zhang D., Fan X. et al. Influence of 0–2 wt.% Sn addition on the microstructure and mechanical properties of extruded AZ80 alloy // Proceedings of the 10th International Conference on Magnesium Alloys and Their Applications (Mg2015). 2015. P. 128–136.
  18. Sasaki T.T., Elsayed F.R., Nakata T. Strong and Ductile Heat-treatable Mg–Sn–Zn–Al Extruded Alloy // Proceedings of the 10th International Conference on Magnesium Alloys and Their Applications (Mg2015). 2015. P. 5–9.
  19. Kochubej A.Ya., Serebryanyj V.N. Vliyanie termomekhanicheskikh parametrov na formirovanie tekstury i struktury pri goryachej obrabotke davleniem splava sistemy Mg–Al–Zn [Influence of thermomechanical parameters on structure and structure forming at hot working pressure of alloy of Mg–Al–Zn system] // Tekhnologiya legkikh splavov. 2007. №2. S. 105–109.
  20. Razuvaev E.I. Novye tekhnologii proizvodstva deformirovannykh polufabrikatov [New production technologies of the deformed semi-finished products] // Aviatsionnye materialy na rubezhe XX–XXI vekov. M.: VIAM, 1994. S. 171–174.
  21. Noda M., Matsumoto R., Kawamura Y. Forging Induces Changes in the Formability and Microstructure of Extruded Mg96Zn2Y2 Alloy with a Long-Period Stacking Order Phase // Materials Science Engineering: A. 2013. Vol. 563. P. 21–27.
  22. Quan G., Ren L., Lv J. et al. The Effect of Processing Procedures on Mechanical Properties of High Strength Mg Alloys // Proceedings of the 10th International Conference on Magnesium Alloys and Their Applications (Mg2015). 2015. P. 923–929.
  23. Kocks U.F., Tome C.N., Wenk H.R. Texture and Anisotropy. Cambridge University Press. 1998. P. 676–677.
  24. Frolov А.V., Mukhina I.Yu., Duyunova V.A., Uridiya Z.P. [An effect of alloying elements and structural factors on heat resistance of magnesium alloys] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №9. St. 07. Available at: http://www.viam-works.ru (accessed: March 22, 2018). DOI: 10.18577/2307-6046-2015-0-9-7-7.