Properties of binder EDT-69N and polymer composites on its basis

Mukhametov R.R., Petrova A.P., Ponomarenko S.A., Dolgova E.V., Pavlyuk B.Ph.
Mukhametov R.R., Petrova A.P., Ponomarenko S.A., Dolgova E.V., Pavlyuk B.Ph. Properties of binder EDT-69N and polymer composites on its basis // Proceedings of VIAM. 2018. No. 4. DOI: 10.18577/2307-6046-2018-0-4-28-37. URL: https://viam-works.ru/en/journal/2018/4/4
Keywords
binder, filler, polymer composites, carbon plastics, fibreglasses, organoplasty, the mechanical, dielectric, heatphysical properties, microspheres glass.
Abstract

The binder EDT-69N is widely and efficiently used in industry as a part of different polymer composites. The article specifies the main types of materials, created on the basis of these binder, their compositions and application fields in the aviation industry. If it is necessary to obtain materials with improved properties, it is also recommended to modify the composition of the binder and its curing program. Evaluation of the influence of the filler type was carried out by comparing physico-chemical characteristics of the curing process of prepregs on the basis of the binder and the fillers used immediately after the preparation of the samples. For the analysis, thermal analysis methods (differential scanning calorimetry, differential thermal analysis (DTA), thermogravimetric analysis (TGA) and differential thermogravimetric analysis) and IR spectroscopy were used. Comparison of IR spectra of the binder before and after curing at different temperatures made it possible to reveal th

Reference list
  1. Kirillov V.N., Kavun N.S. Issledovanie vliyaniya teplovlazhnostnogo vozdejstviya na svojstva epoksidnyh stekloplastikov [Research of influence of hygrothermal impact on properties of epoxy fibreglasses] // Plasticheskie massy. 2008. №9. S. 14–17.
  2. Veshkin E.A. Osobennosti bezavtoklavnogo formovaniya nizkoporistykh PKM [Features of out-of-autoclave forming of poor-porous PCM] // Trudy VIAM elektron. nauch.-tehnich. zhurn. 2016. №2. St. 07. Available at: http://www.viam-works.ru (accessed: March 2, 2018). DOI 10.1857/2307-6046-2016-0-2-7-7
  3. Epoksidnoe svyazuyushhee: pat. 2015997 Ros. Federaciya [The epoxy binding; pat. 2015997 Rus. Federation]; opubl. 15.07.94.
  4. Epoksidnoe svyazuyushhee dlya stekloplastikov: pat. 2028334 Ros. Federaciya [Epoxy binding for fibreglasses: pat. 2028334 Rus. Federation]; opubl. 19.08.91.
  5. Raskutin A.E. Strategiia razvitiia polimernykh kompozitsionnykh materialov [Development strategy of polymer composite materials] // Aviatsionnye materialy i tekhnologii. 2017. №S. S. 344–348. DOI: 10.18577/2071-9140-2017-0-S-344-348.
  6. Kutinov V.F., Kireev V.A., Starcev O.V., Shevaldin V.N. Vliyanie klimaticheskogo stareniya na harakteristiki uprugosti i prochnosti polimernyh kompozicionnyh materialov [Influence of climatic aging on characteristics of elasticity and durability of polymeric composite materials] // Uchenye zapiski CAGI. 2006. №4. T. XXXVII. S. 54–64.
  7. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  8. Kablov E.N. Materialy novogo pokoleniya // Zashhita i bezopasnost. 2014. №4. S. 28–29.
  9. Kablov E.N. Iz chego sdelat budushhee? Materialy novogo pokoleniya, tehnologii ih sozdaniya i pererabotki – osnova innovacij [Of what to make the future? Materials of new generation, technology of their creation and processing – basis of innovations ] // Krylya Rodiny. 2016. №5. S. 8–18.
  10. Postnova M.V., Postnov V.I. Opyt razvitiya bezavtoklavnyh metodov formovaniya PKM [Development experience out-of-autoclave methods of formation PCM]// Trudy VIAM: ehlektron. nauch.-tekhnich. zhurn. 2014. №4. St. 06. Available at: http://www.viam-works.ru (accessed: March 3, 2018). DOI 10.18577/2307-6046-2014-0-4-6-6.
  11. Panina N.N., Kim M.A., Gurevich Ya.M., Grigorev M.M. i dr. Svyazuyushhie dlya bezavtoklavnogo formovaniya izdelij iz polimernyh kompozicionnyh materialov [Binding for nonautoclave formation of products from polymeric composite materials] // Klei. Germetiki. Tehnologii. №10. 2013. S. 18–27.
  12. Kablov E.N., Chursova L.V., Babin A.N., Muhametov R.R., Panina N.N. Razrabotki FGUP «VIAM» v oblasti rasplavnyh svyazuyushhih dlya polimernyh kompozicionnyh materialov [Development of FSUE «VIAM» in the field of molten binding for polymeric composite materials] // Polimernye materialy i tehnologii. 2016. T. 2. №2. S. 37–42.
  13. Mihajlin Yu.A. Konstrukcionnye polimernye kompozicionnye materialy [Constructional polymeric composite materials]. SPb.: NOT, 2008. 822 s.
  14. Spravochnik po kompozicionnym materialam / pod red. Dzh. Lyubina [Directory on composite materials / ed. Jh. Lyubin]. M.: Mashinostroenie, 1988. T. 1. 448 s.
  15. Perepjolkin K.E. Armiruyushhie volokna i voloknistye polimernye kompozity [Reinforcing fibers and fibrous polymeric composites]. SPb.: NOT, 2009. 386 s.
  16. Molchanov B.I., Gudimov M.M. Svojstva ugleplastikov i oblasti ih primeneniya [Properties carbonfibers and areas of their application] // Aviacionnaya promyshlennost. 1997. №3–4. S. 58–60.
  17. Kerber M.L., Vinogradov V.M. Polimernye kompozicionnye materialy: struktura, svojstva, tehnologiya [Polymeric composite materials: structure, properties, technology]. SPb.: Professiya, 2009. 560 s.
  18. Aleksashin V.M., Antyufeeva N.V. Razvitie metodov termicheskogo analiza v issledo-vaniyah polimernyh kompozicionnyh materialov [Development of methods of the thermal analysis in researches of polymeric composite materials] // 75 let. Aviacionnye materialy. Izbrannye trudy «VIAM» 1932–2007: yubil. nauch.-tehnich. sb. M.: VIAM, 2007. S. 245–249.
  19. Antyufeeva N.V., Aleksashin V.M., Zhelezina G.F., Stolyankov Yu.V. Metodicheskie podhody termoanaliticheskih issledovanij dlya ocenki svojstv prepregov i ugleplastikov [Methodical approaches of thermoanalytical researches for assessment of properties of prepregs and carbonfibers] // Prilozhenie k zhurnalu «Vse materialy. Enciklopedicheskij spravochnik». 2012. №4. S. 18–28.
  20. Kutsevich K.E., Aleksashin V.M., Petrova A.P., Antyufeeva N.V. Issledovanie kinetiki reakcij otverzhdeniya kleevyh svyazuyushhih [Research of kinetics of reactions of curing of the glue binding] // Klei. Germetiki. Tehnologii. 2014. №11. S. 27–31.