Anti wear coating with quasicrystal filler

Kuznetsova V.A., Deev I.S., Zheleznyak V.G., Silaeva A.A.
Kuznetsova V.A., Deev I.S., Zheleznyak V.G., Silaeva A.A. Anti wear coating with quasicrystal filler // Proceedings of VIAM. 2018. No. 3. DOI: 10.18577/2307-6046-2018-0-3-68-76. URL: https://viam-works.ru/en/journal/2018/3/8
Keywords
quasicrystals, anti wear coatings, composite materials, metal-polymers, polymeric matrix, paint and varnish materials
Abstract

The paint and varnish material filled with finely divided quasicrystals, and system of coverings on its basis is developed. As basis for polymeric matrix epoxies, as the most demanded material for anti wear coatings have been chosen. Optimum degree of dispersion of quasicrystal fillers and its content in epoxy and polyamide matrix is defined. The paint coatings filled with quasicrystals, possess the increased wear resistance, and its physico-mechanical properties do not concede to let-out analogs.

Reference list
  1. Kablov E.N., Startsev O.V. Fundamentalnye i prikladnye issledovaniya korrozii i stareniya materialov v klimaticheskih usloviyah (obzor) [The basic and applied research in the field of corrosion and ageing of materials in natural environments (review)] // Aviacionnye materialy i tehnologii. 2015. №4 (37). S. 38–52. DOI: 10.18577/2071-9140-2015-0-4-38-52.
  2. Istoriya aviacionnogo materialovedeniya. VIAM – 80 let: gody i lyudi / pod obshh. red. E.N. Kablova [History of aviation materials science. VIAM is 80: years and people / gen. ed. by E.N. Kablov]. M.: VIAM, 2012. 520 s.
  3. Kablov E.N. Materialy i himicheskie tehnologii dlya aviacionnoj tehniki [Materials and chemical technologies for aviation engineering] // Vestnik Rossijskoj akademii nauk. 2012. T. 82. №6. S. 520–530.
  4. Kablov E.N. Aviacionnoe materialovedenie: itogi i perspektivy [Aviation materials science: results and perspectives] // Vestnik Rossijskoj akademii nauk. 2002. T. 72. №1. S. 3–12.
  5. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [In-novative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  6. Kablov E.N. Himiya v aviacionnom materialovedenii [Chemistry in aviation materials science] // Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 3–4.
  7. Abuzin Yu.A., Yudin A.S. Issledovanie osobennostej kvazikristallov pri sozdanii materialov dlya kosmosa, aviacii, motorostroeniya i drugih otraslej narodnogo hozyajstva [Research of features of quasicrystals at creation of materials for space, aircraft, motor industry and other industries of national economy] // Sb. dokl. Pervogo Vseros. soveshhaniya po kvazikristallam. M., 2003. C. 15–18.
  8. Rybin V.V., Ulin I.V., Farmakovskij B.F., Yurkov M.A. Izuchenie vozmozhnosti prakticheskogo ispolzovaniya kvazikristallov v kachestve funkcionalnyh pokrytij [Studying of possibility of practical use of quasicrystals as functional coverings] // Sb. dokl. Pervogo Vseros. soveshhaniya po kvazikristallam. M., 2003. S. 53–56.
  9. Bloom P.D., Baikerikar K.G., Otaigbe J.U., Sheares V.V. Development of novel polymer quasicrystal composite materials // Materials Science and Engineering A. 2000. Vol. 294–296. P. 156–159.
  10. Astruc A., Joliff E., Chailan J.-F. et al. Incorporation of kaolin fillers into an epoxy polyamidoamine matrix for coatings// Progress in Organic Coatings. 2009. Vol. 65. P. 158–168.
  11. Kuznetsova V.A., Kuznetsov G.V., Shapovalov G.G. Issledovanie vliyaniya molekulyarnoj massy epoksidnoj smoly na adgezionnye, fiziko-mehanicheskie svojstva i erozionnuyu stojkost pokrytij [Investigation of epoxy resin molecular mass influence by physiomechanical property and erosive resistant of coatings] // Trudy VIAM: elektron. nauchn.-tehnich. zhurn. 2014. №8. St. 08. Available at: http://www.viam-works.ru (accessed: January 31, 2018). DOI: 10.18577/2307-6046-2014-0-8-8-8.
  12. Kondrashov E.K., Bejder E.Ya., Vladimirskij V.N. Erozionnostojkie lakokrasochnye pokrytiya [Erosion resistant paint coatings]. M.: Himiya, 1989. 135 s.
  13. Gohardani O. Impact of erosion testing aspects on current and future flight conditions // Progress in Aerospace Science. 2011. Vol. 47. P. 280–303.
  14. Tibor «Anpassung–Integration–Offenheit» // Werkstatt und Betr. 2011. Vol. 144. No. 7–8. P. 46–49.
  15. Deev I.S., Kablov E.N., Kobets L.P., Chursova L.V. Issledovanie metodom skaniruyushhej elektronnoj mikroskopii deformacii mikrofazovoj struktury polimernyh matric pri me-hanicheskom nagruzhenii [Research of the scanning electron microscopy method deformation of microphase structure of polymeric matrix at mechanical loading] // Trudy VIAM: elektron. nauch-tehnich. zhurn. 2014. №7. St. 06. Available at: http://www.viam-works.ru (accessed: January 31, 2018). DOI: 10.18577/2307-6046-2014-0-7-6-6.