Influence of woven fibrous fillers of various types on properties of cured binder VS-2526K

Mukhametov R.R., Petrova A.P., Ponomarenko S.A., Akhmadieva K.R., Pavlyuk B.Ph.
Mukhametov R.R., Petrova A.P., Ponomarenko S.A., Akhmadieva K.R., Pavlyuk B.Ph. Influence of woven fibrous fillers of various types on properties of cured binder VS-2526K // Proceedings of VIAM. 2018. No. 3. DOI: 10.18577/2307-6046-2018-0-3-28-36. URL: https://viam-works.ru/en/journal/2018/3/4
Keywords
binder, filler, polymer composite, carbon plastics, fibreglasses, organoplasty, the mechanical, dielectric, heatphysical properties, adhesion parameters.
Abstract

The article describes properties of epoxy binder VS-2526K in an initial condition and after curing, and influence of fillers of various types on properties polymer composites on their basis. The results of research of binder and some materials on its basis by methods of differential thermal analysis, thermogravimetric analysis and IR-spectroscopy are given and discussed. It is shown the influence of filler nature on structure and water resistance of polymer composites. The polymer matrix between glass fibers is characterized be more tension, than for carbon fibers.

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [In-novative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N. Materialy novogo pokoleniya [Materials of new generation] // Zashhita i bezopasnost'. 2014. №4. S. 28–29.
  3. Kablov E.N. Iz chego sdelat budushhee? Materialy novogo pokoleniya, tehnologii ih sozdaniya i pererabotki – osnova innovacij [Of what to make the future? Materials of new generation, technology of their creation and processing – basis of innovations] // Krylya Rodiny. 2016. №5. S. 8–18.
  4. Postnova M.V., Postnov V.I. Opyt razvitiya bezavtoklavnyh metodov formovaniya PKM [Development experience out-of-autoclave methods of formation PCM] // Trudy VIAM: ehlektron. nauch.-tekhnich. zhurn. 2014. №4. St. 06. Available at: http://www.viam-works.ru (accessed: January 25, 2018). DOI: 10.18577/2307-6046-2014-0-4-6-6.
  5. Panina N.N., Kim M.A., Gurevich Ya.M., Grigorev M.M., Chursova L.V., Babin A.N. Svyazuyushhie dlya bezavtoklavnogo formovaniya izdelij iz polimernyh kompozicionnyh materialov [Binding for non-autoclave formation of products from polymeric composite materials] // Klei. Germetiki. Tehnologii. 2013. №10. S. 18–27.
  6. Kablov E.N., Chursova L.V., Babin A.N., Muhametov R.R., Panina N.N. Razrabotki FGUP «VIAM» v oblasti rasplavnyh svyazuyushhih dlya polimernyh kompozicionnyh materialov [Development of FSUE «VIAM» in the field of molten binding for polymeric composite materials] // Polimernye materialy i tehnologii. 2016. T. 2. №2. S. 37–42.
  7. Doneckij K.I., Hrulkov A.V. Principy «zelenoj himii» v perspektivnyh tehnologiyah izgotovleniya izdelij iz PKM [Principles of «green chemistry» in perspective manufacturing technologies of PCM articles] // Aviacionnye materialy i tehnologii. 2014. №S2. S. 24–28.
  8. Kablov E.N., Chursova L.V., Lukina N.F., Kucevich K.E., Rubcova E.V., Petrova A.P. Issledovanie epoksidno-polisulfonovyh polimernyh sistem как osnoveу vysokoprochnyh kleev aviacionnogo naznacheniya [Research of epoxy and polysulfonic polymeric systems as the base of high-strength adhesives of aviation assignment] // Klei. Germetiki. Tehnologii. 2017. №3. S. 7–12.
  9. Vorobev A. Poliefirnye smoly [Polyester resin] // Komponenty i tehnologii. 2003. №32. S. 182–185.
  10. Dholakiya B. Unsaturated Polyester Resin for Specialty Applications // Polyester in Technology. 2012. P. 400.
  11. Aviacionnye materialy: spravochnik v 13 t. / pod obshh. red. E.N. Kablova. [Aviation materials: reference book. in 13 vol. / gen. ed. by E.N. Kablov]. M.: VIAM, 2010. T. 7: Po-limernye kompozicionnye materialy. S. 22–35.
  12. Gooch J.W. Vinyl Ester Resin // Encyclopedic Dictionary of Polymers. Springer, Sci-ence+Business Media, LLC, 2011. P. 794.
  13. Chursova L.V., Grebeneva T.A., Panina N.N., Cybin A.I. Svyazuyushhie dlya polimernyh kompozicionnyh materialov stroitelnogo naznacheniya [Binders for polymer composites materials for construction purposes] // Vse materialy. Enciklopedicheskij spravochnik. 2015. №8. S. 13–17.
  14. Kucevich K.E., Aleksashin V.M., Petrova A.P., Antyufeeva N.V. Issledovanie kinetiki reakcij otverzhdeniya kleevyh svyazuyushhih [Research of the kinetics of the curing reaction of the adhesive binders] // Klei. Germetiki. Tehnologii. 2014. №11. S. 27–31.
  15. Mishkin S.I., Raskutin A.E., Evdokimov A.A., Gulyaev I.N. Tehnologii i osnovnye etapy stroitel'stva pervogo v Rossii arochnogo mosta iz kompozicionnyh materialov [Technologies and the main stages of construction of the arch bridge first in Russia from composite materials] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2017. №6 (54). St. 05. Available at: http://www.viam-works.ru (accessed: January 25, 2018). DOI: 10.18577/2307-6046-2017-0-6-5-5.
  16. Doneckij K.I., Karavaev R.Yu., Raskutin A.E., Panina N.N. Svojstva ugle- i stekloplastikov na osnove pletenyh preform [Properties of carbon fiber and fiberglass on the basis of braiding preforms] // Aviacionnye materialy i tehnologii. 2016. №4 (45). S. 54–59. DOI: 10.18577/2071-9140-2016-0-4-54-59.