The problem of low-temperature plasticity of molybdenum and alloys based on it (review)

Batienkov R.V., Bolshakova A.N., Efimochkin I.Yu.
Batienkov R.V., Bolshakova A.N., Efimochkin I.Yu. The problem of low-temperature plasticity of molybdenum and alloys based on it (review) // Proceedings of VIAM. 2018. No. 3. DOI: 10.18577/2307-6046-2018-0-3-12-17. URL: https://viam-works.ru/en/journal/2018/3/2
Keywords
molybdenum, alloy, destruction, plasticity, alloyage, fine-grained structure.
Abstract

The main methods of making billets from molybdenum and its alloys were examined in this paper such as powder metallurgy and vacuum remilting. The influence of the methods making billets on the formation of the strength and plastic characteristics of molybdenum alloys is analyzed. To increase the low-temperature plasticity of molybdenum alloys, it is necessary to use more pure raw materials, rational alloying and technological methods which make it possible to obtain an alloy with a fine-grained structure.

Reference list
  1. Kablov E.N. Strategicheskie napravleniya razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda [The strategic directions of development of materials and technologies of their processing for the period to 2030] // Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  2. Morgunova N.N., Klypin B.A., Boyarshnov V.A. i dr. Splavy molibdena [Molybdenum alloys]. M.: Metallurgiya, 1975. 392 s.
  3. Molibden. Per. s angl. / pod. red. A.K. Natansona [Molybdenum. Trans. from Engl. / ed. by A.K. Natanson]. M.: Izd-vo inost. lit., 1959. 304 s.
  4. Ershova I.O., Akimenko V.B., Fedotenkova O.B. Poroshkovyj molibdenovyj splav marki MIt-MP [Powder molybdenum alloy of brand MEATH-MEGAPIXEL] // Problemy chernoj metallurgii i materialovedeniya. 2016. №2. S. 1–10.
  5. Grashchenkov D.V., Efimochkin I.Yu., Bolshakova A.N. Vysokotemperaturnye metallomatrichnye kompozicionnye materialy, armirovannye chasticami i voloknami tugoplavkih soedinenij [High-temperature metal-matrix composite materials reinforced with particles and fibers of refractory compounds] // Aviacionnye materialy i tehnologii. 2017. №S. S. 318–328. DOI: 10.18577/2071-9140-2017-0-S-318-328.
  6. Savickij E.M., Burhanov G.S. Metallovedenie tugoplavkih metallov i splavov [Metallurgical science of refractory metals and alloys]. M.: Metallurgiya, 1967. 345 s.
  7. Agte K., Vacek I. Volfram i molibden [Tungsten and molybdenum]. L.: Energiya, 1964. 455 s.
  8. Korneev N.I., Pevzner S.B., Razuvaev E.I., Skugarev I.G. Obrabotka davleniem tugoplavkih metallov i splavov [Processing by pressure of refractory metals and alloys]. M.: Metallurgiya, 1967. 267 s.
  9. Kablov E.N. Konstrukcionnye i funkcionalnye materialy – osnova ekonomicheskogo i nauch-no-tehnicheskogo razvitiya Rossii [Constructional and functional materials – basis of economic and scientific and technical development of Russia] // Voprosy materialovedeniya. 2006. №1. S. 64–67.
  10. Trefilov V.I., Milman Yu.V., Firstov S.A. Fizicheskie osnovy prochnosti tugoplavkih metallov [Physical bases of durability of refractory metals]. Kiev: Naukova dumka, 1975. 315 s.
  11. 11 Materials // Plansee. Available at: https://www.plansee.com/en/materials/ molybdenum.html (accessed: February 02, 2018).
  12. Product Information Molybdenum // HC Starck. Available at: https://www.hcstarck.com/molybdenum_alloy (accessed: February 02, 2018).
  13. Application of molybdenum metal and its alloys // International molybdenum association. Available at: http://www.imoa.info/download_files/molybdenum/Applications_Mo_Metal.pdf (accessed: February 02, 2018).
  14. Molibdenovye splavy MoW, MoLa i drugie [Molybdenum alloys MoW, MoLa and others] // AO «Polema». Available at: http://www.polema.net/molibdenovye-splavy-mv30-mp-mv10-mp-mv-2-mp-mvd-mp-ml-mp-mit--mp-izdelija.html (accessed: February 02, 2018).
  15. Trefilov V.I., Drachinskij A.S., Moiseev V.F. Perehod ot interkristallitnogo k tran-skristallitnomu razrusheniyu v molibdene [Transition from inter crystal to trans-crystalline destruction in molybdenum] // Mehanizm plasticheskoj deformacii. Kiev: Naukova dumka, 1965. S. 42–53.
  16. Kablov E.N., Ospennikova O.G., Vershkov A.V. Redkie metally i redkozemelnye elementy – materialy sovremennyh i budushhih vysokih tehnologij [Rare metals and rare-earth ele-ments are materials for modern and future high technologies] // Aviacionnye materialy i tehnologii. 2013. №S2. S. 3–10.
  17. Kablov D.E., Panin P.V., Shiryaev A.A., Nochovnaya N.A. Opyt ispolzovaniya vakuumno-dugovoj pechi ALD VAR L200 dlya vyplavki slitkov zharoprochnyh splavov na osnove aljuminidov titana [The use of ADL VAR L200 vacuum-arc furnace for ingots fabrication of high-temperature titanium aluminides base alloys] // Aviacionnye materialy i tehnologii. 2014. №2. S. 27–33. DOI: 10.18577/2071-9140-2014-0-2-27-33.
  18. Krupin A.V., Solovev V.Ya. Plasticheskaya deformaciya tugoplavkih metallov [Plastic strain of refractory metals]. M.: Metallurgiya, 1971. 352 s.
  19. Kolesnikov A.G., Shinkarev A.S. Analiz sposobov izmelcheniya struktury pri poluchenii metallicheskih konstrukcionnyh materialov [The analysis of ways of crushing of structure when receiving metal constructional materials] // Nauka i Obrazovanie: elektron. zhurn. / MGTU im. N.E. Baumana. 2014. №11. S. 34–44. DOI: 10.7463/1114.0738880.
  20. Valiev R.Z., Islamgaliev R.K., Alexandrov I.V. Bulk nanostructured materials from sever plastic deformation// Progress in Material Science., 2000. Vol. 45. P. 103–189.
  21. Mathaudhu S.N., Kecskes L.J., Maupin H.E. et al. Severe plastic deformation processing of refractory metals by equal channel angular extrusion // Proceedings of the Army Science Conference (26th) Held in Orlando, Florida (December 1–4, 2008). 2008. P. 1–4.
  22. Alymov M.I. Konsolidirovannye poroshkovye nanomaterialy (obzor) [Consolidated powder nanomaterials] // Aviacionnye materialy i tehnologii. 2014. №S4. S. 34–39. DOI: 10.18577/2071-9140-2014-0-s4-34-39.