Anti-adhesive coatings and their properties

Mukhametov R.R., Petrova A.P., Ponomarenko S.A.
Mukhametov R.R., Petrova A.P., Ponomarenko S.A. Anti-adhesive coatings and their properties // Proceedings of VIAM. 2018. No. 12. DOI: 10.18577/2307-6046-2018-0-12-88-96. URL: https://viam-works.ru/en/journal/2018/12/10
Keywords
anti-adhesive properties, hydrophobicity, anti-adhesive coatings, organosilicon compounds, adhesive strength.
Abstract

The creation and development of new polymer composites requires continuous improvement of their physicomechanical and performance characteristics. PCMs breakdown begins from their surface often and it is important to provide its solidity and water repellent properties, including for improvement of performance characteristics of materials.

In the aviation industry, hydrophobic compounds are mainly applied at present to tooling processing at molding processes of polymer binders to prevent their adhesion.

Compounds based on organosilicon monomers and oligomers are the most widely used due to their efficiency and availability. One of the essential disadvantages of the use of such compositions is the need for curing to prevent their transfer to material moldable. Therefore, it is important to research the influence of cold curing catalysts on coatings properties and choose optimal ones.

In this work, the anti-adhesive characteristics of several organosilicon compounds – K-21 anti-adhesive lubricant, 136-157M water repellent liquid and GK-10 polymethylphenylsiloxane with hydride groups – were estimated and compared. Coatings were prepared from a solution in hexane by dipping. The best coating was chosen by adhesive strength of materials cured glued together by polyurethane glue PU-2. The completeness of curing of the anti-adhesive coatings was also estimated according to adhesive strength of materials cured before and after extraction with hexane in a Soxhlet device.

The work shows the effective use of catalysts 230-15 and AGM-9 and their optimal content is selected, the optimal composition and concentration of the anti-adhesive coating, as well as the curing mode to achieve the required characterist

Reference list
  1. Sobolevskiy M.V., Muzovskaya O.A., Popeleva G.S. Svoystva i oblasti primeneniya kremniyorganicheskikh produktov [Properties and applications of organosilicon products]. M.: Khimiya, 1975. 296 s.
  2. Nefedov N.I., Haskov M.A., Petrova A.P., Buznik V.M. Issledovanie termicheskih svojstv ftorparafinov i gidrofobnyh pokrytij na ih osnove [Study of the thermal properties of fluori-nated paraffins and hydrophobic coatings on their base] // Trudy VIAM: elektron. nauch.-tehnich. zhurnal. 2017. №2. St. 11. Available at: http://www.viam-works.ru (accessed: Octo-ber 25, 2018). DOI: 10.18577/2307-6046-2017-0-2-11-11.
  3. Zhdanov A.A. Gidrofobizatory kremniyorganicheskiye: entsiklopediya polimerov [Orga-nosilicon water repellents: polymers encyclopedia]. M.: Sovetskaya entsiklopediya, 1972. T. 1. S. 625–632.
  4. Voronkov M.G., Lasskaya E.A., Pashenko A.A. O prirode svyazi vodoottalkivayushchikh kremniyorganicheskikh pokrytiy s poverkhnostyu gidrofobizirovannykh materialov [On the nature of the connection of water-repellent silicone coatings with the surface of hydro-phobized materials] // Zhurnal prikladnoy khimii. 1965. T. 38. Vyp. 7. S. 1483–1487.
  5. Deryagin B.V., Churayev N.V., Muller V.M. Poverkhnostnyye sily [Surface forces]. M.: Nauka, 1985. 398 s.
  6. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innova-tive developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  7. Kablov E.N. Materialy novogo pokoleniya [New generation materials] // Zashchita i bezopasnost. 2014. №4. S. 28–29.
  8. Kablov E.N. Iz chego sdelat budushcheye? Materialy novogo pokoleniya, tekhnologii ikh soz-daniya i pererabotki – osnova innovatsiy [What to make the future from? Materials of the new generation, technologies of their creation and processing - the basis of innovation] // Krylya Rodiny. 2016. №5. S. 8–18.
  9. Panina N.N., Kim M.A., Gurevich Ya.M., Grigoryev M.M., Chursova L.V., Babin A.N. Svyazuyushchiye dlya bezavtoklavnogo formovaniya izdeliy iz polimernykh kompozitsionnykh materialov [Binders for non-autoclaving molding products from polymer composite materials] // Klei. Germetiki. Tekhnologii. 2013. №10. S. 18–27.
  10. Kablov E.N., Chursova L.V., Babin A.N., Mukhametov R.R., Panina N.N. Razrabotki FGUP «VIAM» v oblasti rasplavnykh svyazuyushchikh dlya polimernykh kompozitsionnykh materialov [Developments of FSUE «VIAM» in the field of melt binders for polymer composite materials] // Polimernyye materialy i tekhnologii. 2016. T. 2. №2. S. 37–42.
  11. Doneckij K.I., Hrulkov A.V. Principy «zelenoj himii» v perspektivnyh tehnologiyah izgotovleniya izdelij iz PKM [Principles of «green chemistry» in perspective manufacturing technologies of PCM articles] // Aviacionnye materialy i tehnologii. 2014. №S2. S. 24–28.
  12. Kablov E.N., Chursova L.V., Lukina N.F., Kutsevich K.E., Rubtsova E.V., Petrova A.P. Is-sledovaniye epoksidno-polisulfonovykh polimernykh sistem na osnove vysokoprochnykh kleyev aviatsionnogo naznacheniya [Study of epoxy-polysulfone polymer systems based on high-strength adhesives for aviation purposes] // Klei. Germetiki. Tekhnologii. 2017. №3. S. 7–12.
  13. Vorobyev A. Poliefirnyye smoly [Polyester resins] // Komponenty i tekhnologii. 2003. №32. S. 182–185.
  14. Dholakiya B. Unsaturated Polyester Resin for Specialty Applications // Polyester. Intechopen access publisher. 2012. P. 167–202. DOI: 10.5772/48479.
  15. Gooch J.W. Vinyl Ester Resin // Encyclopedic Dictionary of Polymers. Springer, Sci-ence+Business Media, LLC, 2011. P. 794.
  16. Babin A.N., Guseva M.A. Ispolzovaniye reologicheskogo metoda dlya issledovaniya oso-bennostey rastvorimosti komponentov v polimernom svyazuyushchem [The use of rheo-logical methods for study of the solubility of components in polymeric binder] // Trudy VIAM: elektron. nauch.-tekhnich. zhurn. 2016. №6 (42). St. 05. Available at: http://www.viam-works.ru (accessed: October 25, 2018). DOI: 10.18577/2307-6046-2016-0-6-5-5.
  17. Kitaeva N.S., Mukhanova E.E., Deyev I.S. Vysokoteplostoykiye gidrofobnyye pokrytiya dlya teplozashchitnogo materiala na osnove kvartsevogo volokna [High-heatresistant water-proof covering for heat-shielding material on the base of quartz fiber] // Trudy VIAM: el-ektron. nauch.-tekhnich. zhurn. 2013. №6. St. 03. Available at: http://www.viam-works.ru (accessed: October 25, 2018).
  18. Boynovich L.B., Emelyanenko A.M., Muzafarov A.M. i dr. Sozdaniye pokrytiy dlya pridaniya supergidrofobnykh svoystv poverkhnosti silikonovykh rezin [Creating coatings to impart superhydrophobic surface properties of silicone rubbers] // Rossiyskiye nanotekhnologii. 2008. T. 3. №9–10. S. 100–105.
  19. Galyamov M.O., Nikitin L.N., Nikolayev A.Yu. i dr. Formirovaniye ultragidrofobnykh poverkhnostey osazhdeniyem pokrytiy iz sverkhkriticheskoy dvuokisi ugleroda [Formation of ultrahydrophobic surfaces by deposition of supercritical carbon dioxide coatings] // Kolloidnyy zhurnal. 2007. T. 69. №4. S. 448–462.
  20. Bespalov A.S., Buznik V.M., Grashchenkov D.V. i dr. Gidrofobizatsiya poristykh keramich-eskikh materialov s primeneniyem dioksida ugleroda [Hydrophobization of porous ceramic materials using carbon dioxide] // Neorganicheskiye materialy. 2016. T. 52. №4. S. 431–437.
  21. Buznik V.M., Kablov E.N., Koshurina A.A. Materialy dlya slozhnykh tekhnicheskikh ustroystv arkticheskogo primeneniya [Materials for complex technical devices of arctic use] // Nauchno-tekhnicheskiye problemy osvoyeniya Arktiki. M.: Nauka, 2015. S. 275–285.
  22. Kablov E.N. Materialy i khimicheskiye tekhnologii dlya aviatsionnoy tekhniki [Materials and chemical technologies for aviation technology] // Vestnik Rossiyskoy akademii nauk. 2012. T. 82. №6. S. 520–530.
  23. Boynovich L.B., Emelyanenko A.M. Gidrofobnyye materialy i pokrytiya: printsipy soz-daniya. Svoystva i primeneniye [Hydrophobic materials and coatings: the principles of crea-tion. Properties and application] // Uspekhi khimii. 2008. T. 77. №7. S. 619–638.
  24. Emelyanenko A.M., Boynovich L.B. Primeneniye dinamicheskoy porogovoy obrabotki videoizobrazheniy dlya opredeleniya poverkhnostnogo natyazheniya zhidkostey i uglov smachivaniya [The use of dynamic threshold video processing to determine the surface ten-sion of liquids and wetting angles] // Pribory i tekhnika eksperimenta. 2002. №1. S. 52–57.
  25. Postnova M.V., Postnov V.I. Opyt razvitiya bezavtoklavnyh metodov formovaniya PKM [Development experience out-of-autoclave methods of formation PCM]// Trudy VIAM: eh-lektron. nauch.-tekhnich. zhurn. 2014. №4. St. 06. Available at: http://www.viam-works.ru (accessed: October 25, 2018). DOI 10.18577/2307-6046-2014-0-4-6-6.