Heat treatment effect on structure and properties of welded large-dimensioned semi-finished products from VT23 titanium alloy

Dzunovich D.А., Panin P.V., Lukinа E.A., Shiryaev A.A.
Dzunovich D.А., Panin P.V., Lukinа E.A., Shiryaev A.A. Heat treatment effect on structure and properties of welded large-dimensioned semi-finished products from VT23 titanium alloy // Proceedings of VIAM. 2018. No. 1. DOI: 10.18577/2307-6046-2018-0-1-7-7. URL: https://viam-works.ru/en/journal/2018/1/7
Keywords
titanium alloy VT23, electron-beam welding, annealing, large-dimensioned semi-finished product, phase composition, structure, mechanical properties.
Abstract

The effect of heating temperature and cooling rate on phase composition, structure, and hardness has been studied for bulk metal and weld joint as well as the hereinbefore mentioned parameters influence on bulk metal mechanical properties for a 80 mm thickness plate of VT23 (Ti–5,5Al–2Mo–4,5V–1Cr–0,6Fe, wt.%) titanium alloy. It has been shown, that two-step heat treatment including annealing at a temperature 100–130С lower than polymorphic transformation temperature with a subsequent air cooling and ageing at 625С gives the opportunity both to form a homogeneous structure along the weld joint section and to obtain bulk metal tensile strength higher than 1100 MPa wherein impact toughness is more than 0,3 MJ/m2.

Reference list
  1. Kablov E.N. Iz chego sdelat budushhee? Materialy novogo pokoleniya, tehnologii ih soz-daniya i pererabotki – osnova innovacij [Of what to make the future? Materials of new generation, technology of their creation and processing – basis of innovations ] // Krylya Rodiny. 2016. №5. S. 8–18.
  2. Frolov V.A. Tehnologiya svarki plavleniem i termicheskoj rezki metallov: ucheb. posobie [Welding technology melting and thermal cutting of metals: manual]. M.: Alfa M, Infra-M. 2011. 447 s.
  3. Vozdvizhenskij V.M., Zhukov A.A., Postnova A.D., Vozdvizhenskaya M.V. Splavy cvetnyh metallov dlya aviacionnoj tehniki [Non-ferrous alloys for aviation engineering]. Rybinsk: RGATA, 2002. 219 s.
  4. Kolachev B.A., Polkin I.S., Talalaev V.D. Titanovye splavy raznyh stran [Titanium alloys of the different countries]. M.: VILS, 2000. 318 s.
  5. Kolachev B.A., Becofen S.Ya., Bunin S.Ya., Volodin V.A. Fiziko-mehanicheskie svojstva legkih konstrukcionnyh materialov [Physicomechanical properties of easy constructional materials]. M.: Metallurgiya, 1995. 442 s.
  6. Kablov E.N. Materialy i himicheskie tehnologii dlya aviacionnoj tehniki [Materials and chemical technologies for aviation engineering ] // Vestnik Rossijskoj akademii nauk. 2012. T. 82. №6. S. 520–530.
  7. Bratuhin A.G., Kolachev B.A., Sadkov V.V. i dr. Tehnologiya proizvodstva titanovyh samoletnyh konstrukcij [Production technology of titanic aircraft designs]. M.: Mashi-nostroenie, 1995. 448 s.
  8. Horev A.I. Fundamentalnye i prikladnye raboty po konstrukcionnym titanovym splavam i perspektivnye napravleniya ih razvitiya [Fundamental and applied works on structural titanium alloys and perspective directions of their development] //Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №2. St. 04. Available at: http://www.viam-works.ru (accessed: November 28, 2017).
  9. Ilin A.A., Kolachev B.A., Polkin I.S. Titanovye splavy. Sostav, struktura, svojstva: spravochnik [Titanium alloys. Structure, structure, properties: directory]. M.: VILS–MATI, 2009. 520 s.
  10. Frolov V.A., Peshkov V.V., Salikov V.A. i dr. Tehnologicheskie osnovy svarki i pajki v avi-astroenii: uchebnik dlya studentov vuzov. 2-e izd. [Technological bases of welding and the soldering in aircraft industry: the textbook for students of higher education institutions. 2nd ed.]. M.: Intermet Inzhiniring, 2004. 576 s.
  11. Lyasockaya V.S. Termicheskaya obrabotka svarnyh soedinenij titanovyh splavov [Thermal processing of welded compounds of titanium alloys]. M.: Ekomet, 2003. 352 s.
  12. Kollerov M.Yu., Il'in A.A., Filatov A.A., Mamaev V.S. Uprochnyayushhaya termicheskaya obrabotka krupnogabaritnyh polufabrikatov i izdelij iz vysokoprochnyh titanovyh splavov [Strengthening thermal processing of large-size semi-finished products and products from high-strength titanium alloys] // Metallovedenie i termicheskaya obrabotka metallov. 2002. №5. S. 14–17.
  13. Nochovnaya N.A., Panin P.V. Analiz ostatochnyh makronapryazhenij v svarnyh soedineniyah titanovyh splavov raznyh klassov [Residual Macrostress Analysis in Welded Junctions of Different Titanium Alloys] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №5. St. 02. Available at: http://www.viam-works.ru. (accessed: November 28, 2017). DOI: 10.18577/2307-6046-2014-0-5-2-2.
  14. Ilin A.A., Skvorcova S.V., Popova Yu.A., Kudelina I.M. Vliyanie termicheskoj obrabotki na formirovanie struktury i svojstv krupnogabaritnyh polufabrikatov iz splava VT23 [Influence of thermal processing on forming of structure and properties of large-size semi-finished products from alloy ВТ23] // Titan. 2010. №4. S. 48–53.
  15. Skvorcova S.V., Popova Yu.A., Panin P.V. i dr. Vliyanie termicheskoj obrabotki na strukturu i svojstva svarnyh soedinenij iz titanovogo splava VT23 [Influence of thermal pro-cessing on forming of structure and properties of large-size semi-finished products from alloy VT23] // Titan. 2011. №2. S. 16–21.
  16. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  17. Kablov E.N. Materialy novogo pokoleniya – osnova innovacij, tehnologicheskogo liderstva i nacionalnoj bezopasnosti Rossii [Materials of new generation – basis of innovations, technological leadership and national security of Russia] // Intellekt i tehnologii. 2016. №2 (14). S. 16–21.
  18. Moiseev V.N., Kulikov F.R., Kirillov Yu.G., Vaskin Yu.V. Svarnye soedineniya titanovyh splavov (struktura i svojstva) [Welded compounds of titanium alloys (structure and properties)]. M.: Metallurgiya, 1979. 248 s.
  19. Novikov I.I. Teoriya termicheskoj obrabotki metallov: uchebnik dlya vuzov. 3-e izd., ispr. i dop. [Theory of thermal processing of metals: the textbook for higher education institutions. 3rd ed., rev. and add.] M.: Metallurgiya, 1978. 392 s.