The influence of BaO–Al2O3–SiO2-glasses addition on reaction-cured coatings properties for nickel alloys protection

Solntsev St.S., Denisova V.S., Agarkov A.B., Gavrilov S.V.
Solntsev St.S., Denisova V.S., Agarkov A.B., Gavrilov S.V. The influence of BaO–Al2O3–SiO2-glasses addition on reaction-cured coatings properties for nickel alloys protection // Proceedings of VIAM. 2018. No. 1. DOI: 10.18577/2307-6046-2018-0-1-11-11. URL: https://viam-works.ru/en/journal/2018/1/11
Keywords
heat-resisant coatings, nickel alloys, glass, barium-aluminium-silicate system, silicon tetraboride, slurry.
Abstract

The results of heat-resisant coatings containing the additives of refractory glasses in BaO–Al2O3–SiO2 system are explained. The optimal technological parameters of refractory glasses are estimated, and that was found that the additive of 25% BaO–25% Al2O3–50% SiO2 provides the increase of heat resistance and thermal stability. The compositions of reaction cured coatings provide solid gas-proof non-defective coatings designed to heat-resistant nickel alloys protection at temperatures up to 1250°C.

Reference list
  1. Solncev S.S., Denisova V.S., Rozenenkova V.A. Reakcionnoe otverzhdenie – novoe napravlenie v tehnologii vysokotemperaturnyh kompozicionnyh pokrytij i materialov [Reac-tion cure – the new direction in technology ofhigh-temperature composite coatings and materials] // Aviacionnye materialy i tehnologii. 2017. №S. S. 329–343. DOI: 10.18577/2071-9140-2017-0-S-329-343.
  2. Kablov E.N. Materialy dlya izdeliya «Buran» – innovacionnye resheniya formirovaniya shestogo tehnologicheskogo uklada [Materials for «Buran» spaceship – innovative solutions of formation of the sixth technological mode] // Aviacionnye materialy i tehnologii. 2013. №S1. S. 3–9.
  3. Solncev S.S., Denisova V.S., Rozenenkova V.A. Zharostojkie emali dlya zashhity nikelevyh splavov i stalej [Heat resisting enamels for protection of nickel alloys and steels] // Vse materialy. Enciklopedicheskij spravochnik. 2016. №1. S. 22–28.
  4. Kablov E.N. Materialy novogo pokoleniya [Materials of new generation] // Zashhita i bezopasnost. 2014. №4. S. 28–29.
  5. Ovsepyan S.V., Lukina E.A., Filonova E.V., Mazalov I.S. Formirovanie uprochnyayushhej fazy v processe vysokotemperaturnogo azotirovaniya svarivaemogo zharoprochnogo deformiruemogo splava na osnove sistemy Ni–Co–Cr [Formation of the Strengthening Phase during the High-Temperature Nitriding of Ni–Co–Cr Weldable Wrought Superalloy] // Aviacionnye materialy i tehnologii. 2013. №1. S. 3–8.
  6. Grashhenkov D.V. Strategiya razvitiya nemetallicheskih materialov, metallicheskih kompozicionnyh materialov i teplozashhity [Strategy of development of non-metallic materials, metal composite materials and heat-shielding] // Aviacionnye materialy i tehnologii. 2017. №S. S. 264–271. DOI: 10.18577/2071-9140-2017-0-S-264-271.
  7. Goldstein Н.В. еt аl. Reaction cured borosilicate glass coating for low-density fibrous insulation // Borate glasses. Structure, properties, application: plenum press. New York, 1978. P. 623–634.
  8. Garofalini S.H., Banas R., Creedon J. Development of high viscosity coatings for advances Space Shuttle application // 11th National SAMPE technical conference. Boston, 1979. P. 114–124.
  9. Petcold A., Peshman G. Emal i emalirovanie. Per. s nem. [Enamel and covering enamels. Trans. from Germ.]. M.: Metallurgiya, 1990. 576 s.
  10. Shelbi Dzh. Struktura, svojstva i tehnologiya stekla. Per. s angl. [The structure, properties and technology of glass]. M.: Mir, 2006. 288 s.
  11. Dembovskij S.A., Chechetkina E.A. Stekloobrazovanie [Glass formation]. M.: Nauka, 1990. 276 s.
  12. Toropov N.A., Barakovskij V.K., Lapini V.V. i dr. Diagrammy sostoyaniya silikatnyh sistem: spravochnik [Charts of condition of silicate systems: directory]. L.: Nauka, 1972. Vyp. 3: Trojnye silikatnye sistemy. 448 s.
  13. Karimbaev T.D., Mezencev M.A., Ezhov A.Yu. Razrabotka i eksperimentalnye issledovaniya nemetallicheskih detalej i uzlov goryachej chasti perspektivnogo gazoturbinnogo dvigatelya [Development and pilot studies of nonmetallic details and nodes of hot part of the perspective gas turbine engine] // Vestnik Samarskogo universiteta. Aerokosmicheskaya tehnika, tehnologii i mashinostroenie. 2015. T. 14. №3–1. S. 128–138.
  14. Kablov E.N. Kompozity: segodnya i zavtra [Composites: today and tomorrow] // Metally Evrazii. 2015. №1. S. 36–39.
  15. Bankovskaya I.B., Kolovertnov D.V. Razvitie rabot po sozdaniyu pokrytij dlya zashhity uglerodnyh materialov pri vysokih temperaturah [Development of works on creation of coverings for protection of carbon materials at high temperatures] // Fizika i himiya stekla. 2017. T. 43. №2. S. 156–171.