Research of welded joints under conditions of controlled heating of close areas

Parshukov L.I.
Parshukov L.I. Research of welded joints under conditions of controlled heating of close areas // Proceedings of VIAM. 2017. No. 8. DOI: 10.18577/2307-6046-2017-0-8-6-6. URL: https://viam-works.ru/en/journal/2017/8/6
Keywords
electron-beam welding, residual stresses, stress-strain calculation and temperature state.
Abstract

The effect of external loads and the type of welded joint on the stress-strain state in the seam at the electron beam welding. It is shown that the argon arc welding, which is characterized by multilayer during welding of large thickness and a large residual strain in the welded joint leads to a weakening of the retention of structural elements. In some cases, the technical task conditions on structural elements should not be heated above a certain temperature during welding. This constraint greatly increases the TIG welding, since the imposition of a weld produced in small areas. The efficiency of electron beam welding with respect to TIG. Calculated temperature field and the stress-strain state of welded joint during welding and after.

Reference list
  1. Kablov E.N. Rossii nuzhny materialy novogo pokoleniya [Materials of new generation are necessary to Russia] // Redkie zemli. 2014. №3. S. 8–13.
  2. Kablov E.N. Aviacionnoe materialovedenie: itogi i perspektivy [Aviation materials science: results and perspectives] // Vestnik Rossijskoj akademii nauk. 2002. T. 72. №1. S. 3–12.
  3. Kablov E.N. Tendencii i orientiry innovacionnogo razvitiya Rossii: sb. nauch.-inform. mater. [Tendencies and reference points of innovative development of Russia: collection of scientific information materials]. M.: VIAM, 2013. 543 s.
  4. Kablov E.N., Lukin V.I., Ospennikova O.G. Svarka i pajka v aviakosmicheskoj promyshlennosti [Welding and the soldering in the aerospace industry] // Sb. mater. Vseros. nauch.-praktich. konf. «Svarka i bezopasnost». 2012. T. 1. S. 21–30.
  5. Kablov E.N., Ospennikova O.G., Vershkov A.V. Redkie metally i redkozemelnye elementy – materialy sovremennyh i budushhih vysokih tehnologij [Rare metals and rare earth elements – materials of modern and future high technologies] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №2. St. 01. Available at: http://www.viam-works.ru (accessed: June 30, 2017).
  6. Kablov E.N., Petrushin N.V., Svetlov I.L., Demonis I.M. Nikelevye litejnye zharoprochnye splavy novogo pokoleniya [Nickel foundry heat resisting alloys of new generation] // Aviacionnye materialy i tehnologii. 2012. №S. C. 36–52.
  7. Kablov E.N., Bondarenko Yu.A., Kablov D.E. Osobennosti struktury i zharoprochnyh svojstv monokristallov 001> vysokorenievogo nikelevogo zharoprochnogo splava, poluchennogo v usloviyah vysokogradientnoj napravlennoj kristallizacii [Features of structure and heat resisting properties of monocrystals of 001> high-rhenium nickel hot strength alloys received in the conditions of high-gradient directed crystallization] // Aviacionnye materialy i tehnologii. 2011. №4. S. 25–31.
  8. Ospennikova O.G. Strategiya razvitiya zharoprochnyh splavov i stalej specialnogo naznacheniya, zashhitnyh i teplozashhitnyh pokrytij [Strategy of development of hot strength alloys and steels special purpose, protective and heat-protective coverings] // Aviacionnye materialy i tehnologii. 2012. №S. S. 19–36.
  9. Lukin V.I., Ospennikova O.G., Ioda E.N., Panteleev M.D. Svarka alyuminievyh splavov v aviakosmicheskoj promyshlennosti [Welding of aluminum alloys in the aerospace industry] // Svarka i diagnostika. 2013. №2. S. 47–52.
  10. Sorokin L.I., Lukin V.I., Bagdasarov Yu.S. Optimizaciya svarochnoj remontnoj tehnologii detalej gazoturbinnyh dvigatelej (GTD) iz zharoprochnyh splavov [Optimization of welding repair technology of details of gas turbine engines (GTD) from hot strength alloys] // Svarochnoe proizvodstvo. 1997. S. 19–23.
  11. Lukin V.I., Sorokin L.I., Bagdasarov Yu.S. Svarivaemost litejnyh zharoprochnyh nikelevyh splavov tipa ZhS6 [Bondability of cast heat resisting nickel alloys of the ZhS6 type] // Svarochnoe proizvodstvo. 1997. №6. S. 12–17.
  12. Lukin V.I., Semenov V.N., Starova L.L. i dr. Obrazovanie goryachih treshhin pri svarke zharoprochnyh splavov [Formation of hot cracks when welding hot strength alloys] // MiTOM. 2007. №12. S. 7–14.
  13. Lukin V.I., Ioda E.N., Panteleev M.D., Skupov A.A. Svarka plavleniem titanovogo splava VT18U [Fusion welding of VT18U titanium alloy] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №5. St. 03. Available at: http://www.viam-works.ru (accessed: June 30, 2017). DOI: 10.18577/2307-6046-2015-0-5-3-3.
  14. Lukin V.I., Voznesenskaya N.M., Kovalchuk V.G. Svarka vysokoprochnoj korrozionnostojkoj stali VNS-72 [Welding of high-strength VNS-72 corrosion-resistant steel] // Svarochnoe proizvodstvo. 2012. №10. S. 31–35.
  15. Kablov E.N. Strategicheskie napravleniya razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda [The strategic directions of development of materials and technologies of their processing for the period to 2030] // Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  16. Lihachev V.A., Malinin V.G. Strukturno-analiticheskaya teoriya prochnosti [Structural and analytical failure theory]. L.: Nauka, 1992. 400 s.
  17. Gurevich S.M., Zamkova V.N. i dr. Metallurgiya i tehnologiya svarki titana i ego splavov / pod red. V.N. Zamkova [Metallurgy and welding technology of titanium and its alloys]. Kiev: Naukova dumka, 1986. 240 s.
  18. Svarka elektronno-luchevaya izdelij tyazhelogo mashinostroeniya: RD 24.949.04–90 [Welding electron beam products of heavy mechanical engineering: Regulating Document 24.949.04–90]: utv. Min-vom tyazhelogo mashinostroeniya SSSR. M: CNIITMASh, 1990.