Selective laser melting of aluminium alloy (review)

Dynin N.V., Ivanova A.O., Khasikov D.V., Oglodkov M.S.
Dynin N.V., Ivanova A.O., Khasikov D.V., Oglodkov M.S. Selective laser melting of aluminium alloy (review) // Proceedings of VIAM. 2017. No. 8. DOI: 10.18577/2307-6046-2017-0-8-2-2. URL: https://viam-works.ru/en/journal/2017/8/2
Keywords
selective laser melting, aluminium alloys, additive manufacturing.
Abstract

The article presents a review of studies of different research teams on the technology of selective laser melting of aluminum alloys. The review considers features of aluminum alloys, including the presence of stable oxide films, high reflectivity, thermal conductivity and low fluidity of the powder composition, influencing the fusion process and obtains high-quality structure. The presented results on the influence of different parameters and the chemical composition of materials to their characteristics. Brief description of the main systems of alloying of aluminum alloys used for the manufacturing samples and prototypes using additive technologies.

Reference list
  1. Kablov E.N. Additivnye tehnologii – dominanta nacionalnoj tehnologicheskoj iniciativy [The additive technologies are the dominant of national technological initiative] // Intellekt i tehnologii. 2015. №2 (11). S. 52–55.
  2. Buchbinder D. Rapid Manufacturing of Aluminium Parts for serial Production via Selective Laser Melting // Proc. of International User’s Conference on Rapid Prototyping-Tooling&Manufacturing «Euro-uRapid 2007» (Dec. 3–4, 2007, Frankfurt/Main, Germany). 2007. P. 2:2394–2400.
  3. Sercombe T.B., Li X. Selective laser melting of aluminium and aluminium metal matrix composites: review // Materials Technology, 2016. Vol. 31 (2). P. 77–85. DOI: 10.1179/1753555715Y.0000000078.
  4. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  5. Aboulkhair E.T., Tuck C., Ashcroft I., Maskery I., Everitt N.M. On the precipitation hardening of selective laser melted AlSi10Mg // Metallurgical and Materials Transactions: A. 2015. Vol. 46. Issue 8. P. 3337–3341. DOI: 10.1007/s11661-015-2980-7.
  6. Aversa A., Lorusso M., Cattano G., Manfredi D. A study of the microstructure and the mechanical properties of an Al-Si-Ni alloy produced via selective laser melting // Journal of Alloys and Compounds. 2016. Vol. 695. P. 1470–1478. DOI: 10.1016/j.jallcom.2016.10.285.
  7. Jia Y.D., Ma P., Prashanth K.G., Wang G. Microstructure and thermal expansion behavior of Al-50Si synthesized by selective laser melting // Journal of Alloys and Compounds. 2017. Vol. 699. P. 548–553. DOI: 10.1016/j.jallcom.2016.12.429.
  8. Casati R., Lemke J.N., Alarcon A.Z. Aging behavior of high-strength al alloy 2618 produced by selective laser melting // Metallurgical and materials transactions A. December, 2016. DOI: 10.1007/s11661-016-3883-y.
  9. Shaobo Sun, Lijing Zheng, Yingying Liu. Characterization of Al–Fe–V–Si heat-resistant aluminum alloy components fabricated by selective laser melting // Materials Research Society. 2015. Vol. 30. No. 10. DOI:10.1557/jmr.2015.110.
  10. Zhang H., Zhu H. Fabrication and heat treatment of high strength Al-Cu-Mg alloy processed using selective laser melting // Proc. of SPIE. Vol. 9738: Laser 3D Manufacturing III, 97380X. 2016. DOI:10.1117/12.2211362.
  11. Spierings A.B., Dawson K., Heeling T. Microstructural features of Sc- and Zr-modified Al-Mg alloys processed by selective laser melting // Materials and Design. 2017. Vol. 115. P. 52–63. DOI: 10.1016/j.matdes.2016.11.040.
  12. Montero Sistiaga M.L., Mertens R., Vrancken B. et al. Changing the alloy composition of Al7075 for better processability by selective laser melting // Journal of Materials Processing Technology. 2016. Vol. 238. P. 437–445. DOI: 10.1016/j.jmatprotec.2016.08.003.
  13. Aboulkhai N.T., Maskery I., Tuck C. The microstructure and mechanical properties of selectively laser melted AlSi10Mg: The effect of a conventional T6-like heat treatment // Materials Science & Engineering: A. 2016. Vol. 667. P. 139–146. DOI: 10.1016/j.msea.2016.04.092.
  14. Maskery I., Aboulkhair N.T., Aremu A.O. A mechanical property evaluation of graded density Al-Si10-Mg lattice structures manufactured by selective laser melting // Materials Science & Engineering A. 2016. Vol. 670. P. 264–274. DOI:10.1016/j.msea.2016.06.013.
  15. Reschetnik W. Fatigue crack growth behavior and mechanical properties of additively processed EN AW-7075 aluminium alloy // Procedia Structural Integrity. 2016. Vol. 2. P. 3040–3048. DOI:10.1016/j.prostr.2016.06.380.
  16. Tang M., Pistorius P.C. Anisotropic Mechanical Behavior of AlSi10Mg Parts Produced by Selective Laser Melting // Journal of Metals. 2017. Vol. 69. No. 3. DOI: 10.1007/s11837-016-2230-5.
  17. Rosenthal I., Stern A., Frage N. Strain rate sensitivity and fracture mechanism of AlSi10Mg parts produced by selective laser melting // Materials Science & Engineering: A. 2017. Vol. 682. P. 509–517. DOI: 10.1016/j.msea.2016.11.070.
  18. Noriko Read, Wei Wang, Khamis Essa. Selective laser melting of AlSi10Mg alloy: Process optimisation and mechanical properties development // Materials and Design. 2015. Vol. 65. P. 417–424. DOI: 10.1016/j.matdes.2014.09.044.
  19. Maskery I., Aboulkhair N.T., Corfield M.R. Quantification and characterisation of porosity in selectively lasermelted Al–Si10–Mg using X-ray computed tomography // Materials Characterization. 2016. Vol. 111. P. 193–204. DOI: 10.1016/j.matchar.2015.12.001.
  20. Ryabov D.K., Antipov V.V., Korolev V.A., Medvedev P.N. Vliyanie tehnologicheskih faktorov na strukturu i svojstva silumina, poluchennogo s ispolzovaniem tehnologii selektivnogo lazernogo sinteza [Effect of technological factors on structure and properties of Al–Si alloy obtained by selective laser melting] // Aviacionnye materialy i tehnologii. 2016. №S1. S. 44–51. DOI: 10.18577/2071-9140-2016-0-S1-44-51.
  21. Kempen K., Thijs L., Yasa E., Badrossamay M., Verheecke W., Kruth J. Process optimization and microstructural analysis for selective laser melting of AlSi10Mg // Solid Freeform Fabrication Symposium. 2011. Vol. 22. P. 484–495.
  22. Kimura T. Effect of silicon content on densification, mechanical and thermal properties of Al-xSi binary alloys fabricated using selective laser melting // Materials Science & Engineering: A. 2017. Vol. 682. P. 593–602. DOI: 10.1016/j.msea.2016.11.059.
  23. Aboulkhair N.T., Everitt N.M., Ashcroft I., Tuck C. Reducing porosity in AlSi10Mg parts processed by selective laser melting // Additive Manufacturing. 2014. Vol. 1–4. P. 77–86.
  24. Prashanth K.G., Scudino S., Klauss H.J. Microstructure and mechanical properties of Al–12Si produced by selective laser melting: Effect of heat treatment // Materials Science & Engineering: A. 2014. Vol. 590. P. 153–160.
  25. Weingarten С., Buchbinder D. Formation and reduction of hydrogen porosity during selective laser melting of AlSi10Mg // Journal of Materials Processing Technology. 2015. Vol. 221. P. 112–120.
  26. Kablov E.N., Lukina E.A., Sbitneva S.V., Hohlatova L.B., Zajcev D.V. Formirovanie metastabilnyh faz pri raspade tverdogo rastvora v processe iskusstvennogo stareniya Al-splavov [Forming of metastable phases at disintegration of solid solution in the course of artificial aging of Al-alloys] // Tehnologiya legkih splavov. 2016. №3. S. 7–17.
  27. Kablov E.N., Shchetanov B.V., Grashhenkov D.V., Shavnev A.A., Nyafkin A.N. Metallomatrichnye kompozicionnye materialy na osnove Al–SiC [Metalmatrix composite materials on the basis of Al–SiC] // Aviacionnye materialy i tehnologii. 2012. №S. S. 373–380.
  28. Lukina E.A., Filonova E.V., Treninkov I.A. Mikrostruktura i preimushhestvennye kristallograficheskie orientirovki zharoprochnogo nikelevogo splava, sintezirovannogo metodom SLS, v zavisimosti ot energeticheskogo vozdejstviya i termoobrabotki [The microstructure and preferential crystallographic orientation of nickel superalloy, synthesized by SLM method, depending of the energy impact and heat treatment] // Aviacionnye materialy i tehnologii. 2017. №1 (46). S. 38–44. DOI: 10.18577/2071-9140-2017-0-1-38-44.
  29. Berezovskij V.V., Shavnev A.A., Lomov S.B., Kurganova Yu.A. Poluchenie i analiz struktury dispersno-uprochnennyh kompozicionnyh materialov sistemy Al–SiC s razlichnym soderzhaniem armiruyushhej fazy [Receiving and the analysis of structure of the disperse strengthened composite materials of Al–SiC system with the different maintenance of the reinforcing phase] // Aviacionnye materialy i tehnologii. 2014. №S6. S. 17–23. DOI: 10.185577/2071-9140-2014-0-S6-17-23.
  30. Gu D., Wang H., Dai D. et al. Rapid fabrication of Al-based bulk-form nanocomposites with novel reinforcement and enhanced performance by selective laser melting // Scr. Mater. 2015. Vol. 96. P. 25–28.
  31. Gu D., Wang H., Chang F. et al. Selective laser melting additive manufacturing of TiC/AlS–i10Mg bulk-form nanocomposites with tailored microstructures and properties // Phys. Procedia. 2014. Vol. 56. P. 108–116.
  32. Ghosh S.K., Saha P. Crack and wear behavior of SiC particulate reinforced aluminium based metal matrix composite fabricated by direct metal laser sintering process // Mater. Des. 2011. Vol. 32 (1). P. 139–145.
  33. Dadbakhsh S., Hao L. Effect of Fe2O3 content on microstructure of Al powder consolidated parts via selective laser melting using various laser powers and speeds // Int. J. Adv. Manuf. Technol. 2014. Vol. 73 (9–12). P. 1453–1463.
  34. Ocelik V., Vreeling J.A., De Hosson J.T.M. EBSP study of reaction zone in SiC/Al metal matrix composite prepared by laser melt injection. // J. Mater. Sci. 2001. Vol. 36 (20). P. 4845–4849.
  35. Li X.P., Ji G., Chen Z. Selective laser melting of nano-TiB2 decorated AlSi10Mg alloy with high fracture strength and ductility // Acta Materialia. 2017. Vol. 129. P. 183–193. DOI: 10.1016/j.actamat.2017.02.062.