Investigation of welding seals of martency steel steel type 03n18k9m5t after local thermocyclic treatment

Parshukov L.I., Gilmutdinov F.Z., Skupov A.A.
Parshukov L.I., Gilmutdinov F.Z., Skupov A.A. Investigation of welding seals of martency steel steel type 03n18k9m5t after local thermocyclic treatment // Proceedings of VIAM. 2017. No. 7. DOI: 10.18577/2307-6046-2017-0-7-6-6. URL: https://viam-works.ru/en/journal/2017/7/6
Keywords
maraging steel, electron-beam welding, residual stresses, weld seam, mechanical properties.
Abstract

Theoretical and experimental studies of the stress-strain, chemical and structural-phase state of martensitic aging steel after electron beam welding and subsequent heat treatment are carried out. It is established that the chemical, phase composition, structure, and stress-strain state of the martensitic-aging steel seam depend on the speed of electron beam welding. From the analysis of stressed states of the welded seam, it follows that with a higher welding speed, the residual stresses in the weld seam are greater. Thermocyclic treatment of the seam in a jammed state leads to its hardening and reduction of residual stresses.

Reference list
  1. Kablov E.N. Kontrol kachestva materialov – garantiya bezopasnosti ekspluatacii aviacionnoj tehniki [Quality control of materials is the security accreditation of operation of aviation engineering] // Aviacionnye materialy i tehnologii. 2001. №1. S. 3–8.
  2. Kablov E.N. Konstrukcionnye i funkcionalnye materialy – osnova ekonomicheskogo i nauchno-tehnicheskogo razvitiya Rossii [Constructional and functional materials is the base of economic and scientific and technical development of Russia] // Voprosy materialovedeniya. 2006. №1. S. 64–67.
  3. Kablov E.N., Petrushin N.V., Svetlov I.L., Demonis I.M. Nikelevye litejnye zharoprochnye splavy novogo pokoleniya [Nickel foundry heat resisting alloys of new generation] // Aviacionnye materialy i tehnologii. 2012. №S. C. 36–52.
  4. Markova E.S., Yakusheva N.A., Pokrovskaja N.G., Shalkevich A.B. Tehnologicheskie osobennosti proizvodstva martensitostareyushhej stali VKS-180 [Technological features of the production of maraging steel VKS-180] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №7. St. 01. Available at: http://www.viam-works.ru (accessed: March 21, 2017).
  5. Vylezhnev V.P., Kokovyakina S.A., Simonov Yu.N., Suhih A.A. Povyshenie harakteristik nadezhnosti martensitostareyushhej stali 03N18K9M5T putem sozdaniya struktury tipa «nanotripleks» [Increase of characteristics of reliability of maraging steel 03N18K9M5T by creation of structure of the nanotriplex type] // Metallovedenie i termicheskaya obrabotka metallov. 2010. №11. S. 20–24.
  6. Petrakov A.F., Shalkevich A.B. Vysokoprochnye stali v aviastroenii [High-strength became in aircraft industry] // Aviacionnye materialy. Izbrannye trudy «VIAM» 1932–2002: yubil. nauch.-tehnich. sb. M.: VIAM, 2002. S. 180–191.
  7. Ospennikova O.G. Strategiya razvitiya zharoprochnyh splavov i stalej specialnogo naznacheniya, zashhitnyh i teplozashhitnyh pokrytij [Strategy of development of hot strength alloys and steels special purpose, protective and heat-protective coverings] // Aviacionnye materialy i tehnologii. 2012. №S. S. 19–36.
  8. Shalkevich A.B., Voznesenskaya N.M., Pokrovskaya N.G., Markova E.S. Vysokoprochnye konstrukcionnye i korrozionnostojkie stali dlya samoletov novogo pokoleniya [High-strength constructional and corrosion-resistant became for airplanes of new generation] // 75 let. Aviacionnye materialy. Izbrannye trudy «VIAM» 1932–2007: yubil. nauch.-tehnich. sb. M.: VIAM, 2007. S. 142–150.
  9. Markova E.S., Pokrovskaya N.G., Shalkevich A.B., Gromov V.I. Martensitostareyushhie stali ‒ novye perspektivnye materialy dlya valov GTD [Maraging became ‒ new perspective materials for GTE shaft] // Aviacionnye materialy i tehnologii. 2012. №S. S. 81–84.
  10. Krylov S.A., Markova E.S., Shcherbakov A.I., Yakusheva N.A. Metallurgicheskie osobennosti vyplavki vysokoprochnoj martensitostarejushhej stali VKS-180-ID [Development of technology for smelting high-strength maraging steel VKS180-ID microalloyed REM] // Aviacionnye materialy i tehnologii. 2015. №4. S. 14–20. DOI: 10.18577/2071-9140-2015-0-4-14-20.
  11. Kablov E.N. Materialy dlya izdeliya «Buran» – innovacionnye resheniya formirovaniya shestogo tehnologicheskogo uklada [Materials for the product «Buran» are the innovative solutions of forming of the sixth technological way] // Aviacionnye materialy i tehnologii. 2013. №S1. S 3–9.
  12. Kablov E.N., Lukin V.I., Ospennikova O.G. Svarka i pajka v aviakosmicheskoj promyshlennosti [Welding and the soldering in the aerospace industry] // Mater. Vseros. nauch.-praktich. konf. «Svarka i bezopasnost». 2012. T. 1. S. 21–30.
  13. Lukin V.I., Banas I.P., Kovalchuk V.G., Golev E.V. Argono-dugovaya svarka vysokoprochnoj cementuemoj stali VNS-63 [TIG welding of high-strengthened cemented steel VNS-63] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №8. St. 01. Available at: http://www.viam-works.ru (accessed: December 10, 2016).
  14. Lukin V.I., Ioda E.N., Panteleev M.D., Skupov A.A. Svarka plavleniem titanovogo splava VT18U [Fusion welding of VT18U titanium alloy] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №5. St. 03. Available at: http://www.viam-works.ru (accessed: December 10, 2016). DOI: 10.18577/2307-6046-2015-0-5-3-3.
  15. Lukin V.I., Voznesenskaya N.M., Kovalchuk V.G. Svarka vysokoprochnoj korrozionnostojkoj stali VNS-72 [Welding of high-strength VNS-72 corrosion-resistant steel] // Svarochnoe proizvodstvo. 2012. №10. S. 31–35.
  16. Kablov E.N. Strategicheskie napravleniya razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda [The strategic directions of development of materials and technologies of their processing for the period to 2030] // Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  17. Lihachev V.A., Malinin V.G. Strukturno-analiticheskaya teoriya prochnosti [Structural and analytical failure theory]. L.: Nauka, 1992. 400 s.