Research and modification of the heat-resistant sealing composition and the development of manufacturing technology of the tape sealant based on it

Krasnov L.L., Еliseev O.A., Kirina Z.V., Venediktova M.A., Rogovitskiy V.A.
Krasnov L.L., Еliseev O.A., Kirina Z.V., Venediktova M.A., Rogovitskiy V.A. Research and modification of the heat-resistant sealing composition and the development of manufacturing technology of the tape sealant based on it // Proceedings of VIAM. 2017. No. 4. DOI: 10.18577/2307-6046-2017-0-4-8-8. URL: https://viam-works.ru/en/journal/2017/4/8
Keywords
band sealer, silicone elastomer, hydrophobic liquid.
Abstract

This article describes the results of experimental work to clarify the formulation of paste-like sealant brand VIKSINT U-2-28 replacement part hydrophobic and the structuring of the liquid GKZh 136-41 on the hydrophobic liquid Penta 808А or Penta 804. The reason for this replacement is due to the problem of getting liquid polyethylsiloxane GKZh 136-41 due to the lack of raw materials – product ethyldichlorosilane. The results of comparative analysis of technological, physical, mechanical properties of band sealers are fabricated using a variety of waterproofing fluids.

Reference list
  1. Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace materials science] // Vse materialy. Enciklopedicheskij spravochnik. 2008. №3. S. 2–14.
  2. Kablov E.N. Strategicheskie napravleniya razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda [The strategic directions of development of materials and technologies of their processing for the period to 2030] // Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  3. Erasov V.S., Kotova E.A. Erozionnaya stojkost aviacionnyh materialov k vozdejstviyu tverdyh (pylevyh) chastic [Erosion resistance of aviation materials to influence of solid (dust) particles] // Aviacionnye materialy i tehnologii. 2011. №3. S. 30–36.
  4. Naumov I.S., Petrova A.P., Chajkun A.M. Reziny uplotnitel'nogo naznacheniya i snizhenie ih goryuchesti [Rubbers of sealing assignment and decrease in their combustibility] // Vse materialy Enciklopedicheskij sbornik. 2013. №5. S. 28–35.
  5. Kablov E.N. Himiya v aviacionnom materialovedenii [Chemistry in aviation materials science] // Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 3–4.
  6. Pinchuk L.S., Neverov A.S. Germetiziruyushhie polimernye materialy [Pressurizing polymeric materials]. M.: Mashinostroenie, 1995. 159 s.
  7. Smyslova R.A., Shvec V.M., Sarishvili I.G. Primenenie otverzhdayushhihsya germetikov v stroitel'noj tehnike [Application of hardening hermetics in construction equipment] // Obzor informacii VNIINTIEPSM. M., 1991. Ser. 6. №2. S. 1–50.
  8. Valeev R.R., Bylev V.A., Hakimulin Yu.N., Liakumovich A.G. Tehnicheskie svojstva germetikov na osnove TPM-2 polimera [Engineering properties of hermetics on basis TPM-2 of polymer] // Sb. statej 9-j Vseros. konf. «Struktura i dinamika molekulyarnyh sistem». Yal'chik, 2002. S. 84–87.
  9. Gerasimov D.M., Eliseev O.A., Smirnov D.N. Sovremennye tendencii razvitiya kremnijorganicheskih germetikov i kompaundov za rubezhom [Current trends of development of organic silicon hermetics and compounds abroad ] // Sb. tr. konf. «Materialy i tehnologii germetizacii». M.: VIAM, 2005. St. 12 (CD).
  10. Istoriya aviacionnogo materialovedeniya. VIAM – 80 let: gody i lyudi / pod obshh. red. E.N. Kablova [History of aviation materials science. VIAM is 80: years and people / gen. ed. by E.N. Kablov]. M.: VIAM, 2012. S. 349–355.
  11. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  12. Eliseev O.A., Krasnov L.L., Zajceva E.I., Savenkova A.V. Razrabotka i modificirovanie elastomernyh materialov dlya primeneniya vo vseklimaticheskih usloviyah [Development and modifying of elastomeric materials for application in all weather conditions] // Aviacionnye materialy i tehnologii. 2012. №S. S. 309–314.
  13. Gladkih S.N., Barashina E.N., Troickaya O.L. Novye polimernye materialy dlya germetizacii elektroradioizdelij bortovoj apparatury [New polymeric materials for sealing of electroradio products of onboard equipment] // Sb. tr. konf. «Materialy i tehnologii germetizacii». M.: VIAM, 2005. St. 11 (CD).
  14. Grashhenkov D.V., Chursova L.V. Strategiya razvitiya kompozicionnyh i funkcionalnyh materialov [Strategy of development of composite and functional materials] // Aviacionnye materialy i tehnologii. 2012. №S. S. 231–242.
  15. Nizkovyazkaya siloksanovaya kompoziciya: pat. 2356117 Ros. Federaciya. №2007122941/09 [Low-viscous siloxane composition: pat. 2356117 Rus. Federation. No. 2007122941/09]; zayavl. 20.06.07; opubl. 20.05.09, Byul. №14. 8 s.
  16. Kulichihin S.G., Reutov A.S., Miroshnikova I.I. i dr. Reologicheskie zakonomernosti geleobrazovaniya kremnijorganicheskih oligomerov [Rheological patterns of gelation of organic silicon oligomers] // Vysokomolekulyarnye soedineniya. 1992. №5. S. 57–62.
  17. Suzdalcev E.I., Mironova E.V. Poisk alternativy gidrofobiziruyushhej zhidkosti 136-41 pri ee ispolzovanii v kleevom soedinenii «metall–keramika» [Search of alternative of waterproof liquid 136-41 at its use in glued joint «metal–ceramics»] // Vse materialy. 2013. №7. S. 28–31.
  18. Shah V. Spravochnoe rukovodstvo po ispytaniyam i analizu prichin ih razrusheniya [Reference guide on tests and the analysis of the reasons of their destruction]. SPb.: NAT, 2009. S. 178–191.