Some features of liquid formation of polymeric composite materials (review)

Dushin M.I., Donetskiy K.I., Karavaev R.Y., Korotkov I.A.
Dushin M.I., Donetskiy K.I., Karavaev R.Y., Korotkov I.A. Some features of liquid formation of polymeric composite materials (review) // Proceedings of VIAM. 2017. No. 2. DOI: 10.18577/2307-6046-2017-0-2-8-8. URL: https://viam-works.ru/en/journal/2017/2/8
Keywords
porosity, non-autoclave molding, infusion, reinforcing fillers, capillary and vacuum pressure.
Abstract

Features of molding of products from polymeric composite materials by methods of impregnation of dry reinforcement by liquid resin under vacuum pressure are considered. Values of capillary pressure and form factor on the device while studying permeability are experimentally determined. Influence of resin feed rate and capillary pressure on formation of porosity in plastic is investigated. Recommendations about resin feed rate to obtain the minimum porosity in plastic are given.

Reference list
  1. Kablov E.N. Konstruktsionnye i funktsionalnye materialy – osnova ekonomicheskogo i nauchno-tekhnicheskogo razvitiya Rossii [Constructional and functional materials – basis of economic and scientific and technical development of Russia] // Voprosy materialovedeniya. 2006. №1. S. 64–67.
  2. Kablov E.N. Rossii nuzhny materialy novogo pokolenija [Materials of new generation are neces-sary to Russia] // Redkie zemli. 2014. №3. S. 8–13.
  3. Dushin M.I., Hrulkov A.V., Platonov A.A., Ahmadieva K.R. Bezavtoklavnoe formovanie ugleplastikov na osnove prepregov, poluchennyh po rastvornoj tehnologii [Out-of-autoclave formation carbon plastics on the basis of the prepregs received on solution technology] // Aviacionnye materialy i tehnologii. 2012. №2. S. 43–48.
  4. Doneckij K.I., Hrulkov A.V. Principy «zelenoj himii» v perspektivnyh tehnologiyah izgotovleniya izdelij iz PKM [Principles of «green chemistry» in perspective manufacturing technologies of PCM articles] //Aviacionnye materialy i tehnologii. 2014. №S2. S. 24–28.
  5. Tavares S.S., Michaud V., Manson J.A.E. Assessment of semi-impregnated fabrics in honeycomb sandwich structures // Composites. A. 2010. Vol. 41. P. 8–15.
  6. Dushin M. I., Hrulkov A.V., Muhametov R.R., Chursova L.V. Osobennosti izgotovleniya izdelij iz PKM metodom propitki pod davleniem [Features of manufacturing of products from PCM impregnation method under pressure] // Aviacionnye materialy i tehnologii. 2012. №1. S. 18–26.
  7. Repecka L., Boyd J. Vacuum-bag-only-curable prepregs that produce void-free parts // 47-th International SAMPLE Symposium. 2002. P. 1862–1875.
  8. Plastic transfer molding techniques for the production of fiber reinforced plastic structures: pat. 4902215 US; publ. 20.02.90.
  9. Loos A.C. Low-cost fabrication of advanced polymeric composites by resin infusion processes. Adv. Composite Mater. 2001. Vol. 10. No. 2–3. P. 99–106.
  10. Dexter H.B. Development of Textile Reinforced Composites for Aircraft Structures // 4th Internat. Symp. For Textile Composites. Kyoto, Japan, Kyoto Institute of Technology, 1998. P. 36–45.
  11. Metod Marko [Marko's method]: pat. 2495640 SShA; opubl. 12.09.50.
  12. Beckwith S.W., Hyland C.R. Resin Transfer Molding: A Decade of Technology Advances // SAMPLE J. 1998. Vol. 34 (6). P. 7–19.
  13. Composite materials handbook. Ford Belvour, 2002. Vol. 3–5: Polimer matrix composites materials usage, design, and analysis. P. 693.
  14. Resin film infusion process and apparatus: pat. 4622091 US; publ. 03.11.86.
  15. Donetskij K.I., Hrulkov A.V., Kogan D.I., Belinis P.G., Lukyanenko Yu.V. Primenenie obemno-armiruyushhih preform pri izgotovlenii izdelij iz PKM [Use of three-dimensional reinforcing preforms during the production of polymer composite products] // Aviacionnye materialy i tehnologii. 2013. №1. S. 35–39.
  16. Dushin M.I., Chursova L.V., Khrulkov A.V., Kogan D.I. Osobennosti izgotovleniya polimernykh kompozitsionnykh materialov metodom vakuumnoy infuzii [Features of manufacturing of polymeric composite materials method of vacuum infusion] // Voprosy materialovedeniya. 2013. №3. S. 33–40.
  17. Ouahbi T., Saouab А., Breard J., Ouagne P., Chaten S. Modeling of hydro-mechanical coupling in infusion process // Composites: part A. 2007. Vol. 38. P. 1646–1654.
  18. Kablov E.N., Startsev O.V., Deev I.S., Nikishin E.F. Svoystva polimernykh kompo-zitsionnykh materialov posle vozdeystviya otkrytogo kosmosa na okolozemnykh orbitakh [Properties of polymeric composite materials after influence of outer space on earth orbits] // Vse materialy. Entsiklopedicheskiy spravochnik. 2012. №11. S. 2–16.
  19. Gunyaev G.M., Kablov E.N., Aleksashin V.M. Modifitsirovanie konstruktsionnykh ugleplastikov uglerodnymi nanochastitsami [Modifying constructional ugleplastikov carbon nanoparticles] // Rossiyskiy khimicheskiy zhurnal. 2010. T. LIV. №1. S. 5–11.
  20. Donetskiy K.I., Raskutin A.E., Khilov P.A. i dr. Obemnye tekstilnye prefor-my, ispol'zuemye pri izgotovlenii polimernykh kompozitsionnykh materialov (obzor) [Volume textile preformy, used when manufacturing polymeric composite materials (review)] // Bezavtoklavnye tekhnologii pererabotki polimernykh kompozitsionnykh materialov novogo pokoleniya: sb. dokl. konf. M.: VIAM, 2015. S. 13.
  21. Dushin M.I., Khrulkov A.V., Gusev Yu.A., Karavaev R.Yu. Rol kapillyarnogo chisla v protsessakh propitki preform zhidkimi svyazuyushchimi [Role of capillary number in impregnation processes preform the liquid binding] // Voprosy materialovedeniya. 2013. №4. S. 86–91.
  22. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the develop-ment of materials and technologies of their processing for the period until 2030»] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  23. Wood J.R., Bader M.G. Void control for polymer-matrix composites (1) theoretical and experimental evaluation of a diffusion model for the growth and collapse of gas bubbles // Compos. Manuf. 1994. №5 (3). P. 149–158.
  24. Visconti I.C., Langella A., Durante M. The influence of injection pressure on the permeability of unidirectional fibre preforms in RTM // 8th European Conference on Composite Materials (ECCM-8). Naples, Italy. June 3–6, 1998. P. 737–43.
  25. Gauvin R., Trochu F., Lemenn Y., Diallo L. Permeability measurement and flow simulation through fiber reinforcement // Polymer Composites. 1996. Vol. 17 (1). P. 34–42.
  26. Griffin P.R., Grove S.M., Russell P., Short D., Summerscales J., Guild F.J., Taylor E. The effect of reinforcement architecture on the long-range flow in fibrous reinforcement // Composites Manufacturing. 1995. Vol. 6 (3–4). P. 221–235.
  27. Steenkamer D.A., Wilkins D.J., Karbhari V.M. Influence of test fluid on fabric permeability measurements and implications for processing of liguid moulded composites // Journal of Materials Science Letters. 1993. Vol. 12 (13). P. 971–973.
  28. Chan A.W., Larive D.E., Morgan R.J. Anisotropic permeability of fiber preforms: constant flow rate measurement // Journal of Composite Materials. 1993. Vol. 27 (10). P. 996–1008.
  29. Lykov A.V. Teoriya sushki [Drying theory]. M.: Energiya, 1968. 123 s.
  30. Ahn K.J., Seferis J.C., Berg J.C. Simultaneous measurements of permeability and capillary pressure of thermosetting matrices in woven fabric reinforcements // Polymer Composites. 1991. Vol. 12 (3). P. 146–52.
  31. Amico S., Lekakou C. An experimental study the permeability and capillary pressure in resin-transfer moulding // Composites Sceince and Technology. 2001. Vol. 61. P. 1945–1959.
  32. Rudobashta S.P. Massoperenos v sisteme s tverdoy fazoy [Weighttransfer in system with solid phase]. M.: Khimiya, 1980. S. 18.
  33. Mikhaylin Yu.A. Konstruktsionnye polimernye kompozitsionnye materialy [Constructional polymeric composite materials]. SPb.: Nauchnye osnovy i tekhnologi, 2008. 822 s.
  34. Brautman L. Razrushenie i ustalost [Destruction and fatigue]. M.: Mir, 1978. 153 s.
  35. Vacuum resin impregnation process: pat. 4942013 US; publ. 17.07.90.
  36. Double bag vacuum in fusion process: pat. 7413694 US; publ. 07.12.00.
  37. Method and device for producing fiber – reinforced components am injection method: pat. 68353 WO; publ. 20.09.01.
  38. Process and Performance Evaluation of the Vacuum-Assisted Process: pat.1181149 EUR; publ. 01.10.03.
  39. Sposob izgotovleniya voloknistykh kompozitov vakuumnoy infuziey i ustroystvo dlya osushchestvleniya sposoba [Way of manufacturing of fibrous composites vacuum infusion and the device for implementation of way]: pat. 2480335 Ros. Federatsiya; opubl. 20.10.06.
  40. Patel N., Rohatgi V., Lee L.J. Micro scale flow behavior and void formation mechanism during impregnation through a unidirectional stitched fiberglass mat // Polym. Eng. Sci. 1995. Vol. 35 (10). P. 837–851.
  41. Rohatgi V., Patel N., Lee L.J. Experimental investigation of flow induced microvoids during impregnation of unidirectional stitched fiberglass mat // Polym. Compos. 1996. Vol. 17 (2). P. 161–170.
  42. Ruiz E., Achim V., Bread J., Chatel S., Trouchu F. A fast numerical approach to reduce voud formation in liquid composite molding // The 8-th International Conference on Flow Processes in Composite Materials (FPCM-8). Douai, 2006. P. 251–260.
  43. Bread J., Henzel Y., Trouch F., Gauvin R. Analysis of dynamic flow through porous media. Part I: Comparison between saturated and unsaturated flows in fibrous reinforcements // Polym. Compos. 2003. Vol. 24. No. 3. P. 409–421.
  44. Lee G.W., Lee K.J. Mechanism of void formation in composite processing with woven fabrics // Polymer and Polymer Composites. 2003. Vol. 11. No. 7. P. 563–570.
  45. Patel N., Lee L.J. Effect of fiber mat architecture on void formation and removal in liquid composite molding // Polym. Compos. 1995. Vol. 16 (5). P. 386–399.
  46. Patel N., Rohatgi V., Lee L.J. Modeling of void formation and removal in liquid composite molding. Part II. Model development // Polym. Compos. 1996. Vol. 17 (1). P. 104–114.
  47. Dushin M.I., Donetskiy K.I., Karavaev R.Yu. Ustanovlenie prichin obrazovaniya po-ristosti pri izgotovlenii PKM [Establishment of the reasons of formation of porosity when manufacturing PСM] // Trudy VIAM: elektron. nauch.-tekhnich. zhurn. 2016. №6 (42). St. 08. Available at: http://www.viam-works.ru (accessed: September 26, 2016). DOI: 10.18577/2307-6046-2016-0-6-8-8.
  48. Kavkazov Yu.L. Vzaimodeystvie kozhi s vlagoy [Skin interaction with moisture]. M.: Gilegprom, 1952. 258 s.