Semipermeable membranes for vacuum infusion molding of polymer composite materials (review)

Ivanov M.S., Nesterova T.A., Platonov M.M.
Ivanov M.S., Nesterova T.A., Platonov M.M. Semipermeable membranes for vacuum infusion molding of polymer composite materials (review) // Proceedings of VIAM. 2017. No. 2. DOI: 10.18577/2307-6046-2017-0-2-7-7. URL: https://viam-works.ru/en/journal/2017/2/7
Keywords
semipermeable membrane, vacuum infusion, out-of-autoclave molding, polymer composites.
Abstract

In article the overview of structures and compositions of membrane fabrics for manufacturing of polymeric composite materials by method of vacuum infusion is provided. Production methods and materials for manufacturing membrane fabrics are considered. The main firms–manufacturers of membrane fabrics for vacuum infusion and properties of membrane fabrics produced by them are also presented. The membrane fabric applied in the course of vacuum infusion is permeable to gases but not permeable for binding, therefore decontamination of package of filler occurs during all process of infusion, porosity thus decreases to 0,2% and the volume content of fiber increases to 65% that allows applying vacuum infusion with the use of semi-permeable membrane for production of elements of airframe structure. In accordance with this technology production of full composite products or so-called «black wings» of MS-21 airplane is planned.

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N. Materialy i khimicheskie tekhnologii dlya aviatsionnoy tekhniki [Materials and chemical technologies for aviation engineering] // Vestnik Rossiyskoy akademii nauk. 2012. T. 82. №6. S. 520–530.
  3. Kablov E.N. Kompozity: segodnya i zavtra [Composites: today and tomorrow] // Metally Evrazii. 2015. №1. S. 36–39.
  4. Nesterova T.A., Barbotko S.L., Nikolaeva M.F., Gerter Yu.A. Mnogoslojnyj zashhitno-dekorativnyj material dlya dekorirovaniya detalej v salonah samoletov i vertoletov [Multi-layer protective and decorative material for decorating details in the cabin of aircraft and helicopters] // Trudy VIAM: elektron. nauch.-tehni. zhurn. 2013. №8. St. 04. Available at: http://www.viam-works.ru (accessed: October 21, 2016).
  5. Platonov M.M., Nesterova T.A., Nazarov I.A., Bejder E.Ya. Pozharobezopasnyj material na tekstilnoj osnove s poliuretanovym pokrytiem dlya naduvnoj obolochki spasatelnogo trapa [Fabric-based fireproof material with polyurethane coating for inflatable shell of rescue ladder] // Aviacionnye materialy i tehnologii. 2013. №2. S. 50–54.
  6. Nesterova T.A., Platonov M.M., Nazarov I.A., Gerter Yu.A. Pozharobezopasnyy tkaneplenochnyy material dlya dorozhki skolzheniya spasatelnogo trapa [Fireproof fabrics film material for path of sliding of rescue ladder] // Trudy VIAM: elektron. nauch.-tekhnich. zhurnal. 2014. №6. St. 11. Available at: http://www.viam-works.ru (accessed: October 21, 2016). DOI: 10.18577/2307-6046-2014-0-6-11-11.
  7. Chursova L.V., Dushin M.I., Kogan D.I., Panina N.N., Kim M.A., Gurevich Ya.M., Platonov A.A. Plenochnye svyazuyushchie dlya RFI-tekhnologii [Film binding for RFI technology] // Rossiyskiy khimicheskiy zhurnal. 2010. T. LΙV. №1. C. 63–66.
  8. Muhametov R.R., Ahmadieva K.R., Kim M.A., Babin A.N. Rasplavnye svyazujushhie dlya perspektivnyh metodov izgotovleniya PKM novogo pokoleniya [Melt binding for perspective methods of production of PCM of new generation] // Aviacionnye materialy i tehnologii. 2012. №S. S. 260–265.
  9. Grigorev M.M., Hrulkov A.V., Gurevich Ya.M., Panina N.N. Izgotovlenie stekloplastikovyh obshivok metodom vakuumnoj infuzii s ispolzovaniem epoksiangidridnogo svyazuyushhego i polupronicaemoj membrany [Manufacture of fiberglass skins using vacuum infusion using epoksiangidrid resin and a semipermeable membrane] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №2. St. 04. Available at: http://viam-works.ru (accessed: October 21, 2016). DOI: 10.18577/2307-6046-2014-0-2-4-4.
  10. Hrulkov A.V., Dushin M.I., Popov Yu.O., Kogan D.I. Issledovaniya i razrabotka avtoklavnyh i bezavtoklavnyh tehnologij formovaniya PKM [Researches and development autoclave and out-of-autoclave technologies of formation of PCM] //Aviacionnye materialy i tehnologii. 2012. №S. S. 292–301.
  11. Khrulkov A.V., Grigorev M.M., Yazvenko L.N. Perspektivy vnedreniya bezavtoklavnykh tekhnologiy dlya izgotovleniya konstruktsionnykh materialov (obzor) [Implementation perspec-tives without autoclave technologies for manufacturing of constructional materials (review)] // Trudy VIAM: elektron. nauch.-tekhnich. zhurn. 2016. №2. St. 06. Available at: http://www.viam-works.ru (accessed: October 21, 2016). DOI: 10.18577/2307-6046-2016-0-2-6-6.
  12. Vacuum injection process for manufacturing fiber reinforced сcomposite products involves evacuating second chamber causing resin to flow into preform in adjacent evacuated first chamber: pat. 10013409 DE; appl. 17.03.00; publ. 23.11.00.
  13. Dzhogan O.M., Kostenko O.P. Prakticheskaya klassifikatsiya metodov izgotovleniya detaley iz polimernykh kompozitsionnykh materialov propitkoy v osnastke [Practical classification of methods of manufacturing of details from polymeric composite materials impregnation in equipment] // Voprosy proektirovaniya i proizvodstva konstruktsiy letatelnykh apparatov. Kharkov: KhAI, 2013. Vyp. 1 (73). S. 21–32.
  14. Li W., Krehl J., Gillespie J.W., Heider D. Process and Performance Evaluation of the Vacuum-Assisted Process // Journal of Composite Materials. 2004. Vol. 38. No. 20. P. 1803.
  15. Raskutin A.E., Goncharov V.A. Kompyuternoe modelirovanie tekhnologicheskogo protsessa izgotovleniya PKM metodom vakuumnoy infuzii [Computer modeling of technological process of manufacturing of PСM by method of vacuum infusion] // Aviatsionnye materialy i tekhnologii. 2012. №S. S. 286–291.
  16. Amouroux S.C., Heider D., Gillespie Jr. J.W. Membrane-based VARTM: membrane and resin interactions // JEC Magazine. 2006. No. 24. URL: http://www. jeccompo-sites.com/knowledge/international-composites-news/membrane-based-vartm-membrane-and-resin-interactions (accessed: October 21, 2016).
  17. Sposob izgotovleniya izdeliy iz voloknistogo polimernogo kompozitsionnogo materiala poverkhnostnym infuzionnym protsessom i ustroystvo dlya osushchestvleniya sposoba [Way of manufacturing of products from fibrous polymeric composite material surface infusional process and the device for implementation of way]: pat. 2480334 Ros. Federatsiya; zayavl. 07.02.12; opubl. 27.04.13.
  18. Sposob izgotovleniya voloknistykh kompozitov vakuumnoy infuziey i ustroystvo dlya osushchestvleniya sposoba [Way of manufacturing of fibrous composites vacuum infusion and the device for implementation of way]: pat. 2480335 Ros. Federatsiya; zayavl. 07.02.12; opubl. 27.04. 13.
  19. Gardiner G. Semipermeables: Next trend in infusion? // Composites technology. 2014. URL: http://www.compositesworld.com/articles/semipermeables-next-trend-in-infusion (accessed: October 21, 2016).
  20. Amouroux S.C., Heider D., Gillespie Jr.J.W. Characterization of membranes used in pressure driven composite processing // Composites: Part A. 2010. Vol. 41. P. 207–214.
  21. Porous products and process therefor: pat. 4187390 US; appl. 21.07.77, publ. 5.02.80.
  22. Sposob polucheniya poristoy membrany i sloistyy material na ee osnove [Way of receiving porous membrane and layered material on its basis]: pat. 2167702 Ros. Federatsiya; zayavl. 20.08.00; opubl. 27.05.01.
  23. Company W.L. Gore & Associates: ofits. sayt. Available at: http://www.gore-tex.ru/ru-ru/tekhnologii/membrana-gore-tex (accessed: October 21, 2016).
  24. Laminated articles having discontinuous bonded regions: pat. WO 2014/151223; appl.13.03.14, publ. 25.09.14.
  25. Gibkiy listovoy material dlya ogranicheniya prostranstva podachi matrichnogo materiala i sposob ego polucheniya [Flexible sheet material for restriction of space of giving of matrix material and way of its receiving]: pat. 2532573 Ros. Federatsiya; zayavl. 09.03.11, opubl. 20.04.14.
  26. VAP-tekhnologiya [Elektronnyy resurs]. Available at: www.vap-info.com (accessed: October 21, 2016).
  27. Company Composyst GMBH: ofits. sayt. Available at: www.composyst.com/download-en/ (accessed: October 21, 2016).
  28. George A. Optimization of Resin Infusion Processing for Composite Materials: Simulation and Characterization Strategies. Institute of Aircraft Design, University of Stuttgart, 2011. 243 p.
  29. Zhang J., Li J., Han Y. Superhydrophobic PTFE surfaces by extension // Macromol. Rapid Commun. 2004. Vol. 25. P. 1105–1108.