High-strength wrought aluminum weldable V-1963 alloy for details of primary structure of modern aviation engineering

Selivanov A.A., Tkachenko E.A., Popova O.I., Babanov V.V.
Selivanov A.A., Tkachenko E.A., Popova O.I., Babanov V.V. High-strength wrought aluminum weldable V-1963 alloy for details of primary structure of modern aviation engineering // Proceedings of VIAM. 2017. No. 2. DOI: 10.18577/2307-6046-2017-0-2-1-1. URL: https://viam-works.ru/en/journal/2017/2/1
Keywords
V-1963 alloy, high strength wrought aluminum alloy of Al–Zn–Mg–Cu system, microadditionof silver, scandium and zirconium, welding of aluminum alloys.
Abstract

High-strength V-1963 alloy of Al–Zn–Mg–Cu system with small additions of zirconium, scandium and silver, developed by FSUE «VIAM», made for massive highly stressed parts (such as frames, fittings, beams, etc.) of primary structure of modern aviation engineering. Alloying with small additions of silver and scandium allowed to simultaneously increase the strength characteristics (by 10–20%), and fatigue resistance (1,8–2,3 times) in comparison with serial domestic and foreign alloys. Unlike the other high strength alloys of Al–Zn–Mg–Cu system, weldability characteristics of V-1963 were improved as compared to similar alloys without silver, and V-1963 also has an acceptable level of corrosion resistance characteristics. Within the terms of the federal target programs at FSUE «VIAM» and the implementation of an integrated scientific direction 8.1. «High-strength welded aluminum and aluminum-lithium alloys of low density with high fracture toughness» («Strategic directions of development

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N. Strategicheskie napravleniya razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda [The strategic directions of development of materials and technologies of their processing for the period to 2030] // Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  3. Aviacionnye materialy: spravochnik v 13 t.; 7-e izd., pererab. i dop. /pod obshh. red. E.N. Kablova [Aviation materials: the directory in 13 vol.; 7th ed., corr. and add. / gen. ed. by E.N. Kablov]. M.: VIAM, 2008. T. 4, kn. 1. 263 s.
  4. Kablov E.N. Aviacionnoe materialovedenie: itogi i perspektivy [Aviation materials science: results and perspectives] // Vestnik Rossijskoj akademii nauk. 2002. T. 72. №1. S. 3–12.
  5. Antipov V.V., Senatorova O.G., Tkachenko E.A., Vahromov R.O. Alyuminievye deformiruemye splavy [Aluminum deformable alloys / gen. ed. by E.N. Kablov] // Aviacionnye materialy i tehnologii. 2012. №S. S. 167–182.
  6. Alyuminievye splavy v aviakosmicheskoj tehnike / pod obshh. red. E.N. Kablova [Aluminum alloys in aerospace equipment / gen ed. by E.N. Kablov]. M.: Nauka. 2001. 192 s.
  7. Davydov V.G., Elagin V.I., Zaharov V.V., Rostova T.D. O legirovanii alyuminievyh splavov dobavkami skandiya i cirkoniya [About alloying of aluminum alloys scandium and zirconium additives] // MiTOM. 1996. №8. S. 25–30.
  8. Tkachenko E.A., Fridlyander I.N., Matveyets E.N., Kaigorodova L.I. The effect of rare earth metal minor addition on structure and properties of Al–Zn–Mg–Cu alloy // Proceed. ICAA6. Toyohashi, Japan. 1998. Vol. 3. P. 2049–2054.
  9. Kajgorodova L.I., Selnihina E.I., Tkachenko E.A., Senatorova O.G. Vliyanie malyh dobavok skandiya i cirkoniya na strukturu i mehanicheskie svojstva splava Al–Zn–Mg–Cu [Influence of small additives of scandium and zirconium on structure and mechanical properties of alloy of Al-Zn-Mg-Cu] // FMM. 1996. T. 81. Vyp. 5. S. 78–86.
  10. Polmer I.J. Nucliation from Supersaturated Solid Solution // The Journal of the Australian Institute of Metals. 1966. Vol. 11. No. 14. P. 246.
  11. Fridlyander I.N., Dobromyslov A.V., Tkachenko E.A., Senatorova O.G. Perspektivnye vysokoprochnye materialy na alyuminievoj osnove [Perspective high-strength materials on aluminum basis] // MiTOM. 2005. №7. S. 17–23.
  12. Vysokoprochnyj splav na osnove alyuminiya i izdelie, vypolnennoe iz etogo splava: pat. 2233902 Ros. Federaciya [High-strength alloy on the basis of aluminum and the product executed from this alloy: pat. 2233902 Rus. Federation]; opubl. 10.08.04.
  13. Vysokoprochnyj splav na osnove alyuminiya i sposob polucheniya izdeliya iz nego: pat. 2443793 Ros. Federaciya [High-strength alloy on the basis of aluminum and way of receiving product from it: pat. 2443793 Rus. Federation]; opubl. 08.10.10.
  14. Ogura Т., Hirosawa S., Sato T. Quantitative Analysis of the Vicinity of Grain Boundaries with Precipitate Free Zones in Al–Zn–Mg(–Ag) Alloys // Proceed. ICAA9. Australia. 2004. P. 1061–1066.
  15. Vakhromov R.O., Antipov V.V., Tkachenko E.A. Research and Development of High-strength of Al–Zn–Mg–Cu Alloys // Proc. of ICAA-13. Pittsburg. USA. 2012. P. 1515–1520.
  16. Skornyakov V.I., Antipov V.V. Innovacionnyj harakter sotrudnichestva OAO «KUMZ» i FGUP «VIAM» [Innovative nature of cooperation of JSC «KUMZ» and FSUE «VIAM»] // Aviacionnye materialy i tehnologii. 2012. №2. S. 11–14.
  17. Kablov E.N., Lukin V.I., Zhegina I.P., Ioda E.N., Loskutov V.M. Osobennosti i perspektivy svarki alyuminijlitievyh splavov [Features and perspectives of welding of alyuminiylitiyevy alloys] // Aviacionnye materialy i tehnologii. 2002. №4. S. 3–12.
  18. Erasov V.S., Yakovlev N.O., Nuzhnyj G.A. Kvalifikatsionnye ispytaniya i issledovaniya prochnosti aviatsionnyh materialov [Qualification tests and researches of durability of aviation materials] // Aviacionnye materialy i tehnologii. 2012. №S. S. 440–448.