Analysis of continuously reinforced polymer composites production methods using out-of-autoclave technologies (review)

Timoshkov P.N., Khrulkov A.V.
Timoshkov P.N., Khrulkov A.V. Analysis of continuously reinforced polymer composites production methods using out-of-autoclave technologies (review) // Proceedings of VIAM. 2017. No. 11. DOI: 10.18577/2307-6046-2017-0-11-8-8. URL: https://viam-works.ru/en/journal/2017/11/8
Keywords
non-autoclave molding methods, impregnation under pressure, vacuum infusion, impregnation of the filler with a film binder, prepreg, binder.
Abstract

The main non-autoclave technologies for the production of parts made of polymer composite materials (PCM) based on glass and carbon fillers and melt thermosetting binders for use in the aviation and automotive industry, as well as their advantages and disadvantages are considered. Basic schemes of assembling packages for various types of molding are presented, with the use of appropriate equipment and hardware design.

Reference list
  1. Kablov E.N. V istorii VIAM Petr Dementev zanimaet osoboe mesto [In the history of VIAM Peter Dementyev takes special place] // Krylya Rodiny. 2017. №1. S. 1–2.
  2. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  3. Kablov E.N. Materialy novogo pokoleniya – osnova innovacij, tehnologicheskogo liderstva i nacionalnoj bezopasnosti Rossii [Materials of new generation – basis of innovations, technological leadership and national security of Russia] // Intellekt & Tehnologii. 2016. №4. S. 41–46.
  4. Kablov E.N. Materialy i tehnologii VIAM dlya «Aviadvigatelya» [Materials and VIAM technologies for «Aviadvigatel»] // Permskie aviacionnye dvigateli: inform. byul. 2014. №31. S. 43–47.
  5. Kablov E.N. O nastoyashhem i budushhem VIAM i otechestvennogo materialovedeniya: intervyu [About the real and future VIAM and domestic materials science: interview] // Rossijskaya akademiya nauk. 2015. 19 yanvarya.
  6. Kablov E.N. Kompozity: segodnya i zavtra [Composites: today and tomorrow] // Metally Evrazii. 2015. №1. S. 36–39.
  7. Postnova M.V., Postnov V.I. Opyt razvitiya bezavtoklavnyh metodov formovaniya PKM [Development experience out-of-autoclave methods of formation PCM]// Trudy VIAM: ehlektron. nauch.-tekhnich. zhurn. 2014. №4. St. 06. Available at: http://www.viam-works.ru (accessed: June 10, 2017). DOI 10.18577/2307-6046-2014-0-4-6-6.
  8. Timoshkov P.N., Platonov A.A., Hrulkov A.V. Propitka plenochnym svyazuyushhim (RFI) kak perspektivnaya bezavtoklavnaya tehnologiya polucheniya izdelij iz PKM [Film resin infusion as an advanced method for out-of-autoclave processing of polymer composites] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №5. St. 09. Available at: http://www.viam-works.ru (accessed: June 10, 2017). DOI: 10.18577/2307-6046-2015-0-5-9-9.
  9. Kablov E.N. Strategicheskie napravleniya razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda [The strategic directions of development of materials and technologies of their processing for the period to 2030] // Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  10. Kogan D.I., Chursova L.V., Petrova A.P. Polimernye kompozicionnye materialy, poluchennye putem propitki plenochnym svyazuyushhim [The polymeric composite materials received by impregnation by the film binding] // Kompozicionnye materialy. 2011. №11. S. 2–6.
  11. Hrulkov A.V., Dushin M.I., Popov Yu.O., Kogan D.I. Issledovaniya i razrabotka avtoklavnyh i bezavtoklavnyh tehnologij formovaniya PKM [Researches and development autoclave and out-of-autoclave technologies of formation of PCM] //Aviacionnye materialy i tehnologii. 2012. №S. S. 292–301.
  12. Timoshkov P.N., Kogan D.I. Sovremennye tehnologii proizvodstva polimernyh kompozicionnyh materialov novogo pokoleniya [Modern production technologies of polymeric composite materials of new generation] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №4. St. 07. Available at: http://www.viam-works.ru (accessed: June 05, 2017).
  13. Dushin M.I., Hrulkov A.V., Muhametov R.R. Vybor tehnologicheskih parametrov avtoklavnogo formovaniya detalej iz polimernyh kompozicionnyh materialov [A choice of technological parameters of autoclave formation of details from polymeric composite materials] // Aviacionnye materialy i tehnologii. 2011. №3. S. 20–26.
  14. Chursova L.V., Dushin M.I., Hrulkov A.V., Muhametov R.R. Osobennosti tehnologii izgotovleniya detalej iz kompozicionnyh materialov metodom propitki pod davleniem [Features of manufacturing techniques of details from composite materials impregnation method under pressure] // Kompozicionnye materialy v aviakosmicheskom materialovedenii: sb. tez. dokl. mezhotras. nauch.-tehnich. konf. M.: VIAM, 2009. S. 17.
  15. Raskutin A.E., Hrulkov A.V., Yazvenko L.N. Polimernoe plenochnoe pokrytie dlya konstrukcij iz PKM (obzor) [Polymer film coating for PCM structures] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2017. №2 (50). St. 05. Available at: http://www.viam-works.ru (accessed: October 25, 2017). DOI: 10.18577/2307-6046-2017-0-2-5-5.