Research of properties of cured adhesive binders

Petrova A.P., Lukina N.F., Melnikov D.A., Besednov K.L., Pavlyuk B.Ph.
Petrova A.P., Lukina N.F., Melnikov D.A., Besednov K.L., Pavlyuk B.Ph. Research of properties of cured adhesive binders // Proceedings of VIAM. 2017. No. 10. DOI: 10.18577/2307-6046-2017-0-10-6-6. URL: https://viam-works.ru/en/journal/2017/10/6
Keywords
adhesive binders, strength of adhesive bonds, rheological properties, physic and mechanical properties
Abstract

Here are physical and mechanical properties, rheological properties of two adhesive binders of melting type VSK-14-2m and VSK-14-2mR. Here are next properties: tensile strength, bending strength, relative extension, fracture viscosity, glass transition temperature, modulus of elasticity under tension and bending. Shown the influence of selected technology for processing of binder to demands for rheological properties. Processing technologies of bindings in PCM are proposed on the basis of rheological properties.

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N. Kontrol kachestva materialov – garantiya bezopasnosti ekspluatacii aviacionnoj tehniki [Quality control of materials – security accreditation of operation of aviation engineering] // Aviacionnye materialy i tehnologii. 2001. №1. S. 3–8.
  3. Anihovskaya L.I., Minakov V.T. Klei i kleevye prepregi dlya perspektivnyh izdelij aviakosmicheskoj tehniki [Glues and glue prepregs for perspective products of aerospace equipment] // Aviacionnye materialy. Izbrannye trudy «VIAM» 1932–2002: yubil. nauch.-tehnich. sb. M.: MISiS–VIAM, 2002. S. 315–326.
  4. Kirienko T.A., Lukina N.F., Kucevich K.E., Petrova A.P. Issledovanie reologicheskih svojstv kleevyh svyazuyushhih [Research of rheological properties of the glue binding] // Klei. Germetiki. Tehnologii. 2016. №2. S. 6–8.
  5. Kablov E.N., Chursova L.V., Lukina N.F., Petrova A.P. Issledovanie epoksidno-polisulfonovyh polimernyh sistem kak osnovy vysokoprochnyh kleev aviacionnogo naznacheniya [Research of epoxy and polysulfonic polymeric systems as bases of high-strength adhesives of aviation assignment] // Klei. Germetiki. Tehnologii. 2017. №3. S. 7–12.
  6. Dementeva L.A., Kucevich K.E., Lukina N.F., Petrova A.P. Ispolzovanie kleevyh svyazuyushhih dlya polucheniya polimernyh kompozicionnyh materialov [The use of adhesive binders for production of polymeric composite materials] // Novosti materialovedeniya. Nauka i tehnika: elektron. nauch.-tehnich. zhurn. 2016. №2 (20). St. 03. Available at: http://materialsnews.ru (accessed: August 02, 2017).
  7. Melnikov D.A., Gromova A.A., Raskutin A.E., Kurnosov A.O. Teoreticheskij raschet i eksperimentalnoe opredelenie modulya uprugosti i prochnosti stekloplastika VPS-53/120 [Theoretical calculation and experimental determination of modulus of elasticity and strength of GRP VPS-53/120] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2017. №1 (49). St. 08. Available at: http://www.viam-works.ru (accessed: August 03, 2017). DOI: 10.18577/2307-6046-2017-0-1-8-8.
  8. Haskov M.A., Melnikov D.A., Dementeva L.A. Optimizaciya rezhimov otverzhdeniya epoksidnyh kompozicij s uchetom masshtabnogo faktora [Optimization of modes of curing of epoxy compositions taking into account large-scale factor] // Novye materialy i tehnologii glubokoj pererabotki syr'ya – osnova innovacionnogo razvitiya ekonomiki Rossii: sb. dokl. II Mezhdunar. nauch.-tehnich. konf. M.: VIAM, 2017. S. 30.
  9. Lukina N.F., Dement'eva L.A., Petrova A.P., Kirienko T.A., Chursova L.V. Kleevye svyazuyushhie dlya detalej iz PKM sotovoj konstrukcii [Glue binding for details from PCM of cellular design] // Klei. Germetiki. Tehnologii. 2016. №5. S. 12–16.
  10. Babin A.N., Petrova A.P. Metody ispytanij i issledovanij osnovnyh svojstv polimernyh svyazuyushhih dlya konstrukcionnyh PKM [Test methods and researches of the main properties polymeric binding for constructional PCM] // Vse materialy. Enciklopedicheskij spravochnik. 2016. №3. S. 52–59.
  11. Kirienko T.A., Lukina N.F., Kutsevich K.E., Petrova A.P. A study of the rheological properties of adhesive binders // Polymer Science. D. 2016. Vol. 9. No. 3. P. 295–297.
  12. Deev I.S., Kablov E.N., Kobets L.P., Chursova L.V. Issledovanie metodom skaniruyushhej elektronnoj mikroskopii deformacii mikrofazovoj struktury polimernyh matric pri mehanicheskom nagruzhenii [Research of the scanning electron microscopy method deformation of microphase structure of polymeric matrix at mechanical loading] // Trudy VIAM: elektron. nauch-tehnich. zhurn. 2014. №7. St. 06. Available at: http://www.viam-works.ru (accessed: July 20, 2017). DOI: 10.18577/2307-6046-2014-0-7-6-6.
  13. Sharova I.A., Petrova A.P. Obzor po materialam mezhdunarodnoj konferencii po kleyam i germetikam (WAC-2012, Franciya) [Review of world adhesive and sealant conference (WAC-2012, France] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №8. St. 06. Available at: http://www.viam-works.ru (accessed: July 19, 2017).
  14. Grashhenkov D.V., Chursova L.V. Strategiya razvitiya kompozicionnyh i funkcionalnyh materialov [Strategy of development of composite and functional materials] // Aviacionnye materialy i tehnologii. 2012. №S. S. 231–242.
  15. Lukina N.F., Dementeva L.A., Petrova A.P., Serezhenkov A.A. Konstrukcionnye i termostojkie klei [Constructional and heat-resistant glues] // Aviacionnye materialy i tehnologii. 2012. №S. S. 328–335.
  16. Petrova A.P., Dementeva L.A., Lukina N.F., Chursova L.V. Kleevye svyazuyushhie dlya polimernyh kompozicionnyh materialov na ugle- i steklonapolnitelyah // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №9. St. 11. URL: http//www.viam-works.ru (data obrashheniya: 20.07.2017). DOI: 10.18577/2307-6046-2015-0-9-11-11.
  17. Lukina N.F., Dementeva L.A., Serezhenkov A.A., Kotova E.V., Senatorova O.G., Sidelnikov V.V., Kucevich K.E. Kleevye prepregi i kompozicionnye materialy na ih osnove [Glue prepregs and composite materials on their basis] // Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 53–56.