Effect of cooling rate on phase composition and structure of VT6 titanium alloy after hydrogenating annealing

Panin P.V., Dzunovich D.А.
Panin P.V., Dzunovich D.А. Effect of cooling rate on phase composition and structure of VT6 titanium alloy after hydrogenating annealing // Proceedings of VIAM. 2017. No. 10. DOI: 10.18577/2307-6046-2017-0-10-4-4. URL: https://viam-works.ru/en/journal/2017/10/4
Keywords
titanium alloy VT6, hydrogenating annealing, cooling rate, phase composition, structure.
Abstract

The effect of cooling rate on structure formation processes upon hydrogenating annealing of VT6 alloy (Ti–6,25Al–4,1V% wt.) has been studied, the mentioned processes being governed by mechanism and kinetics of transformations in hydrogen-containing β-phase. It has been shown that cooling rate of 1 K/s gives the opportunity to reduce diffusion-based decomposition of hydrogen-containing β-phase in the samples subjected to hydrogenation at 850–900°С to a concentration of 0,6% wt. H and higher. Thus a single-phase β-structure is formed at room temperature, which is uncommon for the VT6 alloy upon equilibrium conditions.

Reference list
  1. Ilin A.A., Kolachev B.A., Nosov V.K., Mamonov A.M. Vodorodnaya tehnologiya titanovyh splavov [Hydrogen technology of titanium alloys]. M.: MISiS, 2002. 392 s.
  2. Kolachev B.A., Ilin A.A., Nosov V.K., Mamonov A.M. Dostizheniya vodorodnoj tehnologii titanovyh splavov [Achievements of hydrogen technology of titanium alloys] // Tehnologiya legkih splavov. 2007. №3. s. 10–26.
  3. Ilin A.A., Skvorcova S.V., Mamonov A.M., Kollerov M.Yu. Fazovye i strukturnye prevrashheniya v titanovyh splavah raznyh klassov pod dejstviem vodoroda [Phase and structural transformations in titanium alloys of different classes under the influence of hydrogen] // Titan. 2007. №1. S. 32–37.
  4. Panin P.V., Dzunovich D.A., Alekseev E.B. Sposoby opisaniya fazovogo sostava titanovyh splavov, dopolnitelno legirovannyh vodorodom (obzor) [Ways of phase areas representation in titanium alloys additionally doped with hydrogen (review)] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №3. St. 03. Available at: http://www.viam-works.ru (accessed: August 03, 2017). DOI: 10.18577/2307-6046-2015-0-3-3-3.
  5. Ilin A.A. Mehanizm i kinetika fazovyh i strukturnyh prevrashhenij v titanovyh splavah [The mechanism and kinetics of phase and structural transformations in titanium alloys]. M.: Nauka, 1994. 304 s.
  6. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  7. Kablov E.N. Tendencii i orientiry innovacionnogo razvitiya Rossii: sb. nauch.-inform. mater. 3-e izd. [Tendencies and reference points of innovative development of Russia: collection of scientific and technical information. 3rd ed.]. M.: VIAM, 2015. 720 s.
  8. Kablov E.N. Iz chego sdelat budushhee? Materialy novogo pokoleniya, tehnologii ih sozdaniya i pererabotki – osnova innovacij [What the future to make of? Materials of new generation, technology of their creation and processing – basis of innovations] // Krylya Rodiny. 2016. №5. s. 8–18.
  9. Kablov D.E., Panin P.V., Shiryaev A.A., Nochovnaya N.A. Opyt ispolzovaniya vakuumno-dugovoj pechi ALD VAR L200 dlya vyplavki slitkov zharoprochnyh splavov na osnove aljuminidov titana [The use of ADL VAR L200 vacuum-arc furnace for ingots fabrication of high-temperature titanium aluminides base alloys] //Aviacionnye materialy i tehnologii. 2014. №2. S. 27–33. DOI: 10.18577/2071-9140-2014-0-2-27-33.
  10. Nochovnaya N.A., Panin P.V., Kochetkov A.S. Problemy polucheniya himicheski i strukturno odnorodnyh slitkov iz zharoprochnyh splavov na osnove gamma-alyuminida titana [Receiving problems chemically and structurally uniform ingots from hot strength alloys on the basis of titanium gamma aluminide] // Mater. konf. «Problemy proizvodstva slitkov i polufabrikatov iz slozhnolegirovannyh i intermetallidnyh titanovyh splavov» (30 okt. 2015 g.). M.: VIAM, 2015. St. 03. 1 elektron. opt. disk (CD).
  11. Ovchinnikov A.V., Nosov V.K., Afonin V.E., Panin P.V. Osnovnye zakonomernosti deformacii splavov titan-vodorod [Main patterns of deformation of alloys titanium-hydrogen] // Tehnologiya legkih splavov. 2007. №3. S. 96–99.
  12. Skvorcova S.V., Ilin A.A., Becofen S.Ya., Filatov A.A., Dzunovich D.A., Panin P.V. Anizotropiya mehanicheskih svojstv i tekstura listovyh polufabrikatov iz titanovyh splavov [Anisotropy of mechanical properties and structure of sheet semi-finished products from titanium alloys] // Tehnologiya legkih splavov. 2006. №1–2. S. 81–87.
  13. Panin p.v. zakonomernosti formirovaniya fazovogo sostava i struktury v titanovyh splavah pri termovodorodnoj obrabotke i plasticheskoj deformacii: avtoref. dis. … kand. tehn. nauk [Patterns of forming of phase structure and structure in titanium alloys at thermohydrogen treating and plastic strain: thesis, PhD (Tech.)]. M.: MATI, 2009. 24 s.
  14. Panin P.V., Dzunovich D.A., Zasypkin V.V. Sozdanie dvuhfaznoj kompozitnoj struktury v alfa-splave Ti–6Al s pomoshhyu termovodorodnoj obrabotki [Creation of diphasic composite structure in Ti–6Al alpha alloy by means of thermohydrogen treating] // Nauchnye trudy (Vestnik MATI). 2012. №19 (91). S. 33–37.
  15. Panin P.V., Dzunovich D.A., Lukina E.A. Upravlenie strukturoj i svojstvami titanovyh splavov pri obratimom legirovanii vodorodom i plasticheskoj deformacii [Management of structure and properties of titanium alloys at reversible alloying hydrogen and plastic strain] // Sb. nauch. tr. RKK «Energiya» im. S.P. Koroleva. Korolev, 2012. Ser. xii. Vyp. 1–2: Materialy XIX nauch.-tehnich. konf. molodyh uchenyh i specialistov. S. 103–107.
  16. Panin P.V., Manohin S.S., Dzunovich D.A. Poluchenie i issledovanie submikrokristallicheskoj struktury v titanovyh splavah pri obratimom legirovanii vodorodom i plasticheskoj deformacii [Receiving and research of submicrocrystalline structure in titanium alloys at reversible alloying hydrogen and plastic strain] // Voprosy materialovedeniya. 2016. №4 (88). S. 7–17.
  17. Skvorcova S.V., Panin P.V., Nochovnaya N.A., Grushin I.A., Mitropolskaya N.G. Vliyanie vodoroda na fazovye i strukturnye prevrashheniya v titanovom splave VT6 [Influence of hydrogen on phase and structural transformations in BT6 titanium alloy] // Tehnologiya legkih splavov. 2011. №4. S. 35–40.
  18. Panin P.V., Grushin I.A., Mitropolskaya N.G. Issledovanie zakonomernostej izmeneniya strukturno-fazovogo sostoyaniya titanovogo splava VT6 pri dopolnitelnom legirovanii vodorodom [Research of patterns of change of structural and phase condition of VT6 titanium alloy at additional alloying hydrogen] // Nauchnye trudy (Vestnik MATI). 2013. №20 (92). S. 31–34.
  19. Panin P.V., Shiryaev A.A., Dzunovich D.A. Postroenie temperaturno-koncentracionnoj diagrammy fazovogo sostava titanovogo splava VT6, dopolnitelno legirovannogo vodorodom [Creation of the temperature and concentration chart of phase composition of the BT6 titanium alloy which has been in addition alloyed by hydrogen] // Tehnologiya mashinostroeniya. 2014. №3 (141). S. 5–9.
  20. Panin P.V., Dzunovich D.A., Alekseev E.B. Fazovyj sostav i struktura titanovogo splava VT6, dopolnitelno legirovannogo vodorodom, posle vakuumnogo otzhiga [Phase composition and structure of hydrogenated titanium alloy VT6 after vacuum annealing] // Trudy VIAM: jelektron. nauch.-tehnich. zhurn. 2016. №2 (38). St. 05. Available at: http://www.viam-works.ru (accessed: August 03, 2017). DOI: 10.18577/2307-6046-2016-0-2-5-5.
  21. Panin P.V., Dzunovich D.A., Shiryaev A.A. Issledovanie termicheskoj stabilnosti struktury titanovogo splava VT6 posle termovodorodnoj obrabotki [Research on thermal stability of VT6 titanium alloy structure after thermohydrogen treatment] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №3. St. 06. Available at: http://www.viam-works.ru (accessed: August 03, 2017). DOI: 10.18577/2307-6046-2016-0-3-6-6.
  22. Dzunovich D.A., Shalin A.V., Panin P.V. Struktura, tekstura i mehanicheskie svojstva deformirovannyh polufabrikatov iz splava VT6, poluchennyh po promyshlennym i opytnym tehnologiyam [Structure, structure and mechanical properties of the deformed semi-finished products from alloy of VT6 received on industrial and pilot technologies] // Deformaciya i razrushenie materialov. 2017. №6. S. 19–27.