Investigation of the effect of the barrier layer on heat-resistant protective coating for turbine blades from ZhS32 alloy

Smirnov A.A., Budinovskiy S.A.
Smirnov A.A., Budinovskiy S.A. Investigation of the effect of the barrier layer on heat-resistant protective coating for turbine blades from ZhS32 alloy // Proceedings of VIAM. 2017. No. 1. DOI: 10.18577/2307-6046-2017-0-1-2-2. URL: https://viam-works.ru/en/journal/2017/1/2
Keywords
heat-resistant coatings, ion-plasma technology, high-temperature nickel alloys, secondary reaction zone, topologically close-packed phases.
Abstract

The effect of the nitride and carbide barrier layers on heat resistance of the compositions of superalloy ZhS32 with heat-resistant coatings was studied. Investigations of the barrier layer microstructure in the coating structure in original form and after heat resistance test at temperatures 1150 and 1200°C on the basis of 500 and 100 hours accordingly were carried out. Kinetics change of the barrier layers and their influence on the protective properties of the coating was studied. It has been found that the use of the nitride barrier in the structure of heat-resistant protective coating composition Ni–Cr–Al–Ta–Re–Y–Hf+Al–Ni–Y improves the heat resistance of composition «ZhS32–coating». The work is executed within the implementation of the complex scientific direction 17.3. «Multilayer heat-resisting and heat-protective coatings, nanostructural strengthening erosion, corrosion, wear-resistant and antifretting coatings for protection of hot section parts and GTЕ/GTU compressor» («The

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  2. Kablov E.N., Petrushin N.V., Svetlov I.L., Demonis I.M. Nikelevye litejnye zharoprochnye splavy novogo pokoleniya [Nickel foundry heat resisting alloys of new generation] // Aviacionnye materialy i tehnologii. 2012. №S. C. 36–52.
  3. Zharoprochnyj splav na nikelevoj osnove dlya monokristallicheskogo litya: pat. 2439184 Ros. Federaciya [Hot strength alloy on nickel basis for single-crystal molding: pat. 2439184 Russian Federation]; opubl. 05.10.10.
  4. Zharoprochnyj splav na osnove nikelya: pat. 2402624 Ros. Federaciya [Hot strength alloy on the basis of nickel: pat. 2402624 Russian Federation]; opubl. 16.06.09.
  5. Zharoprochnyj litejnyj splav na osnove nikelya i izdelie, vypolnennoe iz nego: pat. 2365656 Ros. Federaciya [Heat resisting cast alloy on the basis of nickel and the product which has been executed of it: pat. 2365656 Russian Federation]; opubl. 30.01.08.
  6. Petrushin N.B., Ospennikova O.G., Visik E.M. i dr. Zharoprochnye nikelevye splavy nizkoj plotnosti [Heat resisting nickel alloys of low density] // Litejnoe proizvodstvo. 2012. №6. S. 5–11.
  7. Kablov E.N., Muboyadzhyan S.A. Zharostojkie i teplozashhitnye pokrytiya dlya lopatok turbiny vysokogo davleniya perspektivnyh GTD [Heat resisting and heat-protective coverings for turbine blades of high pressure of perspective GTE] //Aviacionnye materialy i tehnologii. 2012. №S. S. 60–70.
  8. Matveev P.V., Budinovskij S.A., Muboyadzhyan S.A., Kosmin A.A. Zashhitnye zharostojkie pokrytiya dlya splavov na osnove intermetallidov nikelya [High-temperature coatings for intermetallic nickel-based alloys] //Aviacionnye materialy i tehnologii. 2013. №2. S. 12–15.
  9. Kablov E.N., Muboyadzhyan S.A. Heat-resistant coatings for the high-pressure turbine blades of promising GTES // Russian metallurgy (Metally). 2012. №1. P. 1–7.
  10. Budinovskij S.A., Matveev P.V., Smirnov A.A. Issledovanie zharostojkosti litejnyh zharoprochnyh nikelevyh splavov v oblasti temperatur 1000–1200°C [Research of heat resistance of cast heat resisting nickel alloys in the field of temperatures 1000-1200°C] // Aviacionnaya promyshlennost. 2014. №2. S. 48–52.
  11. Kablov E.N., Muboyadzhyan S.A., Budinovskij S.A., Lutsenko A.N. Ionno-plazmennye zashhitnye pokrytiya dlya lopatok gazoturbinnyh dvigatelej [Ion-plasma protecting covers for blades of gas turbine engines] // Metally. 2007. №5. S. 23–34.
  12. Muboyadzhyan S.A., Kablov E.N. Vacuum plasma technique of protective coatings production of complex alloys // Metal Sciens and Heat Treatment. 1995. №2. P. 15–18.
  13. Suzuki A., Rae C.M.F. Secondary reaction zone formations in coated Ni-base single crystal superalloys // Journal of Physics: Conference Series. 2009. V. 165. P. 78–83.
  14. Suzuki A., Rae C.M.F., Hobbs R.A., Murakami H. Secondary reaction zone formations in Pt-Aluminised fourth generation Ni-base single crystal superalloys // Advanced Materials Research. 2011. V. 278. P. 78–83.
  15. Muboyadzhyan S.A., Budinovskij S.A., Gayamov A.M., Matveev P.V. Vysokotemperaturnye zharostojkie pokrytiya i zharostojkie sloi dlya teplozashhitnyh pokrytij [High-temperature heat resisting coverings and heat resisting layers for heat-protective coverings] //Aviacionnye materialy i tehnologii. 2013. №1. S. 17–20.
  16. Budinovskij S.A., Muboyadzhyan S.A., Gayamov A.M., Kosmin A.A. Zharostojkie ionno-plazmennye pokrytiya dlya lopatok turbin iz nikelevyh splavov, legirovannyh reniem [Heat resisting ion-plasma coverings for blades of turbines from the nickel alloys alloyed by reniye] // MiTOM. 2008. №6. C. 31–36.
  17. Budinovskij S.A., Muboyadzhyan S.A., Gayamov A.M., Stepanova S.V. Ionno-plazmennye zharostojkie pokrytiya s kompozicionnym bar'ernym sloem dlya zashhity ot okisleniya splava ZhS36-VI [Ion-plasma heat resisting coverings with composition barrier layer for protection against oxidation of alloy ZhS36-VI] // MiTOM. 2011. №1. C. 34–40.
  18. Gayamov A.M. Zharostojkoe pokrytie s kompozicionnym bar'ernym sloem dlya zashhity vneshnej poverhnosti rabochih lopatok GTD iz renijsoderzhashhih zharoprochnyh nikelevyh splavov [Heat resisting covering with composition barrier layer for protection of exterior surface of working blades of GTD from reniysoderzhashchy heat resisting nickel alloys] / V sb. materialov XI Rossijskoj ezhegodnoj konf. molodyh nauch. sotrudnikov i aspirantov «Fiziko-himiya i tehnologiya neorganicheskih materialov». M.: IMET RAN, 2012. C. 473–475.
  19. Gayamov A.M., Budinovskij S.A., Muboyadzhyan S.A., Kosmin A.A. Vybor zharostojkogo pokrytija dlya zharoprochnogo nikelevogo renij-rutenijsoderzhashhego splava marki VZhM4 [Selection of heat-resistant coating with metalloceramic barrier layer for protection of Re-Ru nickel-based superalloy] // Trudy VIAM : elektron. nauch.-tehnich. zhurn. 2014. №1. St. 01. Available at: http://viam-works.ru (accessed: March, 02 2015). DOI: 10.18577/2307-6046-2014-0-1-1-1.