Particular properties of deformation behavior of alloy V-1469 in conditions of joint influence of applied loading and active corrosion environment

Morozova L.V., Zhegina I.P., Grigorenko V.B.
Morozova L.V., Zhegina I.P., Grigorenko V.B. Particular properties of deformation behavior of alloy V-1469 in conditions of joint influence of applied loading and active corrosion environment // Proceedings of VIAM. 2016. No. 9. DOI: 10.18577/2307-6046-2016-0-9-10-10. URL: https://viam-works.ru/en/journal/2016/9/10
Keywords
hard loading cycle, surface, damage accumulation, corrosive environment, microstructure, fragmentation, slip lines.
Abstract

The deformation behavior of Al-Li alloy V-1469 in conditions of joint influence of applied load and active corrosion environment after carrying out tests according to six schemes is considered. Research of alternation of destruction nature and relief of the alloy surface is conducted; plastic zones of deformation localization which differ on density of strips of sliding, the size and density of corrosion pettings are allocated. The work is executed within implementation of integrated scientific direction 8.1. «High-strength welded aluminum and aluminum-lithium alloys of lowered density with increased fracture toughness» («The strategic directions of development of materials and technologies of their processing for the period till 2030»)

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace materials science] // Vse materialy. Enciklopedicheskij spravochnik. 2008. №3. S. 2–14.
  3. Kablov E.N. Konstrukcionnye i funkcionalnye materialy – osnova ekonomicheskogo i nauchno-tehnicheskogo razvitiya Rossii [Constructional and functional materials – basis of economic and scientific and technical development of Russia] // Voprosy materialovedeniya. 2006. №1. S. 64–67.
  4. Orlov M.R. Strategicheskie napravleniya razvitiya Ispytatelnogo centra FGUP «VIAM» [Strategic directions of development of the Test center FSUE «VIAM»] // Aviacionnye materialy i tehnologii. 2012. №S. S. 387–393.
  5. Panin V.E. Fizicheskaya mezomehanika materialov [Physical mesomechanics of materials]. Tomsk: Izd. dom TGU, 2015. 920 s.
  6. Panin V.E., Kablov E.N., Pochivalov Yu.I., Panin S.V., Kolobnev N.I. Vliyanie nanostrukturirovaniya poverhnostnogo sloya alyuminij-litievogo splava 1424 na mehanizmy deformacii, tehnologicheskie harakteristiki i ustalostnuyu dolgovechnost. Povyshenie plastichnosti i tehnologicheskih harakteristik [Influence of nanostructuring surface layer aluminum - lithium alloy 1424 on deformation mechanisms, technical characteristics and fatigue life. Increase of plasticity and technical characteristics] // Fizicheskaya mezomehanika. 2012. T. 15. №6. S. 107–111.
  7. Seong-Woong Kim, Huck Beng Chew, K. SharvanKumar. In situ TEM study of crack-grain boundary interactions in thin copper foils // Scripta Materialia. 2013. Vol. 68. P. 154–157.
  8. Dun Yu., Aleksandrov I.V., Vang D. Vysokoskorostnoe deformacionnoe povedenie ultramelkozernistoj medi [High-speed deformation behavior of ultrafine-grained copper] // Vestnik Ufimskogo gos. aviacionnogo tehnicheskogo un-ta. 2012. T. 16. №1 (46). S. 98–105.
  9. Belikova A.F., Buravova C.N., Gordopolov Yu.A. Lokalizaciya deformacii i svyaz ee s deformirovannym sostoyaniem materiala [Localization of deformation and its communication with the deformed condition of material] // Zhurnal tehnicheskoj fiziki. 2013. T. 83. №2. S. 153–155.
  10. Shibkov A.A., Zolotov A.E., Zheltov M.A., Shuklinov A.V., Denisov A.A. Dinamika deformacionnyh polos i razrushenie alyuminij-magnievogo splava AMg6 [Dynamics of deformation strips and destruction Amg6 aluminum-magnesium alloy] // Fizika tverdogo tela. 2011. T. 53. №10. S. 1873–1878.
  11. Glezer A.M., Shurygina N.A., Zajchenko S.G., Permyakova I.E. Vzaimodejstvie polos deformacionnogo sdviga i nanochastic v amorfno-nanokristallicheskih splavah [Interaction of strips of deformation shift and nanoparticles in amorphous nanocrystalline alloys] // Deformaciya i razrushenie materialov. 2012. №4. S. 2–12.
  12. Shibkov A.A., Zolotov A.E., Zheltov M.A., Denisov A.A. Deformacionnyj haos i samoorganizaciya na stadii predrazrusheniya splava AMg6 [Deformation chaos and self-organization at stage of predestruction of alloy АМg6] // Fizika tverdogo tela. 2011. T. 53. №10. S. 1879–1884.
  13. Fridlyander I.N., Grushko O.E., Shamraj V.F., Klochkov G.G. Vysokoprochnyj konstrukcionnyj Al–Cu–Li–Mg splav ponizhennoj plotnosti, legirovannyj serebrom [The high-strength constructional Al–Cu–Li–Mg alloy of the lowered density alloyed by silver] // MiTOM. 2007. №6 (624). S. 3–7.
  14. Fridlyander I.N., Grushko O.E., Antipov V.V., Kolobnev N.I., Hohlatova L.B. Alyuminijlitievye splavy [Aluminum lithium alloys] // 75 let. Aviacionnye materialy. Izbrannye trudy «VIAM» 1932–2007: yubilejnyj nauchn.-tehn. sb. M.: VIAM, 2007. S. 163–171.
  15. Turchenkov V.A., Baranov D.E., Gagarin M.V., Shishkin M.D. Metodicheskij podhod k provedeniju ekspertizy materialov [Methodical approach to carrying out examination of materials] // Aviacionnye materialy i tehnologii. 2012. №1. S. 47–53.
  16. Chabina E.B., Alekseev A.A., Filonova E.V., Lukina E.A. Primenenie metodov analiticheskoj mikroskopii i rentgenostrukturnogo analiza dlya issledovaniya strukturno-fazovogo sostoyaniya materialov [Application of methods of analytical microscopy and X-ray of the structural analysis for research of structural and phase condition of materials] //Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №5. St. 06. Available at: http://www.viam-works.ru (accessed: July 20, 2016).