The influence of plasticizating additives on rheology of slip for porous ceramic materials based on aluminum oxide
Buchilin N.V., Prager E.P., Ivakhnenko Yu.A. The influence of plasticizating additives on rheology of slip for porous ceramic materials based on aluminum oxide // Proceedings of VIAM. 2016. No. 8. DOI: 10.18577/2307-6046-2016-0-8-6-6. URL: https://viam-works.ru/en/journal/2016/8/6
Keywords
rheology, slurry, slip suspensions, oxide ceramics, alumina, ceramic filters.
Abstract
In the present article the results of rheology characteristics investigations of alumina-based slurries for foam-ceramics production are presented. It is shown that replacement of water, that is used as technological ligament, by water solution of carbamide and aluminum oxychloride, leads to decrease of thickness of corundum particles electric dou-ble layer, that facilitates green bodies formability and improves mechanical characteristics of ceramic materials. The ratios of solid phase (sintering powders) to liquid phase (technological ligament) where either coagulation contacts or direct contacts between solid phase particles appears to form are determined.
Reference list
- Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
- Gasparyan M.D., Grunskiy V.N., Bespalov A.V., Popova N.A. i dr. Primenenie keramicheskikh vysokoporistykh blochno-yacheistykh palladievykh katalizatorov v protsesse okisleniya izotopov vodoroda [Use of ceramic high-porous block and cellular palladic catalysts in the course of oxidation of isotopes of hydrogen] // Steklo i keramika. 2014. №11. S. 22–25.
- Buntushkin V.P., Kablov E.N., Bazyleva O.A., Morozova G.I. Splavy na osnove alyuminidov nikelya [Alloys on the basis of nickel aluminides] // MiTOM. 1999. №1. S. 32–34.
- Kablov E.N., Petrushin N.V., Svetlov I.L., Demonis I.M. Nikelevye litejnye zharoprochnye splavy novogo pokoleniya [Nickel foundry heat resisting alloys of new generation] // Aviacionnye materialy i tehnologii. 2012. №S. C. 36–52.
- Keramicheskiy filtr, soderzhashchiy uglerodnoe pokrytie, i sposob ego izgotovleniya: pat. 2456056 Ros. Federatsiya [The ceramic filter containing carbon covering, and way of its manufacturing: pat. 2456056 Rus. Federation]; zayavl. 28.01.08; opubl. 20.07.12. Byul. №20. 15 s.
- Yang W., Jiang B., Wang A., Shi H. Effect of Negatively Charged Ions on the Formation of Microarc Oxidation Coating on 2024 Aluminium Alloy // Journal of Material Science and Technology. 2012. №28 (8). P. 707–712.
- Vogt U.F., Gorbar M., Dimopoulos-Eggenschwiler P., Broenstrup A., Wagner G., Colombod P. Improving the properties of ceramic foams by a vacuum infiltration process // Journal of the European Ceramic Society. 2010. №30. P. 3005–3011.
- Antsiferov V.N. Problemy poroshkovogo materialovedeniya [Problems of powder materials science]. Ekaterinburg: UrO RAN, 2002. Chast II. 263 s.
- Khimicheskaya tekhnologiya keramiki: uch. posob. dlya vuzov / pod red. I.Ya. Guzmana [Chemical technology of ceramics: uch. posob. for higher education institutions / ed. by I.Ya.Guzman]. M.: Stroymaterialy, 2003. 496 s.
- Kablov E.N. Korroziya ili zhizn [Corrosion or life] // Nauka i zhizn. 2012. №11. S. 16–21.
- Kablov E.N., Shchetanov B.V., Ivahnenko Yu.A., Balinova Yu.A. Perspektivnye armiruyushhie vysokotemperaturnye volokna dlya metallicheskih i keramicheskih kompozicionnyh materialov [Perspective reinforcing high-temperature fibers for metal and ceramic composite materials] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №2. St. 05. Available at: http://www.viam-works.ru (accessed: April 19, 2016).
- Markova S.V., Turlova O.V., Ponomarenko A.A. Primenenie PAV v proizvodstve silikatnykh materialov [Application of PEAHENS in production of silicate materials] // Steklo i keramika. 2013. №3. S. 20–22.
- Buchilin N.V., Prager E.P. Reologicheskie harakteristiki shlikernyh suspenzij na osnove oksida alyuminiya [Rheology of alumina-based slurry suspensions] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №5. St. 06. Available at: http://www.viam-works.ru (accessed: April 19, 2016). DOI: 10.18577/2307-6046-2015-0-5-6-6.
- Shchukin E.D., Pertsov A.V., Amelina E.A. Kolloidnaya khimiya. 3-e izd., pererab. i dop. [Colloid chemistry. 3rd ed., processed and added]. M.: Vysshaya shkola. 2004. 445 s.
- Praktikum i zadachnik po kolloidnoy khimii / pod red. V.V. Nazarova, A.S. Grodskogo [Workshop and the book of problems on colloid chemistry / ed. by V. V. Nazarov, A.S.Grodsky]. M.: Akademkniga, 2007. 374 s.
- Malkin A.Ya., Isaev A.I. Reologiya: kontseptsii, metody, prilozheniya [Rheology: concepts, methods, appendices]. SPb: Professiya, 2007. 560 s.
- Kirienko T.A., Balinova Yu.A. Vliyanie atmosfernoj vlazhnosti na reologiju tonkih sloev koncentrirovannyh vodnyh rastvorov sistemy «neorganicheskie soli–organicheskij polimer» [Influence of atmospheric humidity on a rheology of thin layers of the concentrated water solutions of system «inorganic salts–organic polymer»] // Aviacionnye materialy i tehnologii. 2014. №2. S. 56–58.
- Shchetanov B.V., Balinova Yu.A., Lyulyukina G.Yu., Soloveva E.P. Struktura i svojstva nepreryvnyh polikristallicheskih volokon α-Al2O3 [Structure and properties of continuous polycrystalline fibers α-Al2O3] // Aviacionnye materialy i tehnologii. 2012. №1. S. 13–17.
- Kirienko T.A., Balinova Yu.A. Fiziko-himicheskie svojstva mnogokomponentnyh rastvorov dlya keramicheskih materialov, soderzhashhih polivinilovyj spirt [Physical and chemical properties of multicomponent solutions for ceramic materials containing polyvinyl alcohol] // Aviacionnye materialy i tehnologii. 2014. №1. S. 34–38.
- Tekhnologiya stekla. 3-e izd./ pod red. I.I. Kitaygorodskogo [The technology has flown down. 3rd ed. / ed. by I.I.Kitaigorodsky]. M.: Gos. izd-vo lit-ry po str-vu, arkh. i str-nym mater. 1961. 624 s.
- Pikalov E.S., Sysoev E.P., Sidneva Yu.V. Reologicheskie svoystva shlikerov na osnove glin Msterskogo mestorozhdeniya [Rheological properties of slip on basis clays the Mstersky deposit] // Steklo i keramika. 2014. №6. S. 28–33.
- Uvarova N.E., Grashchenkov D.V., Isaeva N.V., Orlova L.A., Sarkisov P.D. Vysokotemperaturnye radioprozrachnye materialy: segodnya i zavtra [High-temperature radio transparent materials: today and tomorrow] // Aviacionnye materialy i tehnologii. 2010. №1. S. 16–21.
- Balinova Yu.A., Shheglova T.M., Lyulyukina G.Yu., Timoshin A.S. Osobennosti formirovaniya α-Al2O3 v polikristallicheskih voloknah s soderzhaniem oksida alyuminiya 99% v prisutstvii dobavok Fe2O3, MgO, SiO2 [Features of formation α-Al2O3 in polycrystalline fibers containing 99% alumina doped with Fe2O3, MgO, SiO2] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №3. St. 03. Available at: http://www.viam-works.ru (accessed: April 19, 2016). DOI: 10.18577/2307-6046-2014-0-3-3-3.
- Shramm G. Osnovy prakticheskoy reologii i reometrii [Bases of practical rheology and rheometry]. M.: KolosS. 2003. 312 s.