The research of interfaces in metallic composite material based on aluminum alloy reinforced by alumina fibers

Serpova V.M., Shavnev A.A., Solyaev Y.О., Prokofiev M.V., Rabinskiy L.N.
Serpova V.M., Shavnev A.A., Solyaev Y.О., Prokofiev M.V., Rabinskiy L.N. The research of interfaces in metallic composite material based on aluminum alloy reinforced by alumina fibers // Proceedings of VIAM. 2016. No. 8. DOI: 10.18577/2307-6046-2016-0-8-5-5. URL: https://viam-works.ru/en/journal/2016/8/5
Keywords
metal matrix composite material, interface, interfacial layers (spinel).
Abstract

The paper presents results of investigation of interfaces in composite metal material (MMC) based on aluminum alloy reinforced by alumina fiber. The continuous fibers of alumina and Al–Mg–Cu alloy are used as precursor components. The chemical compo-sition and structure of the investigated materials, estimation of the volume fraction of interfacial zones in microns is performed by methods of x-ray and x-ray fluorescence analysis. The work is executed within implementation of the complex scientific direction 12.1. «Metal composite materials (MCM) reinforced by particles and fibers of refractory compounds» («The strategic directions of development of materials and technologies of their processing for the period till 2030») [1].

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  2. Alyuminievye splavy [Aluminum alloys] // Istoriya aviacionnogo materialovedeniya. VIAM – 80 let: gody i lyudi / pod obshh. red. E.N. Kablova. M.: VIAM, 2012. S. 143–156.
  3. Kablov E.N. Materialy i himicheskie tehnologii dlya aviacionnoj tehniki [Materials and chemical technologies for aviation engineering] // Vestnik Rossijskoj akademii nauk. 2012. T. 86. №6. S. 520–530.
  4. Kablov E.N. Sovremennye materialy – osnova innovacionnoj modernizacii Rossii [Modern materials – basis of innovative modernization of Russia] // Metally Evrazii. 2012. №3. S. 10–15.
  5. Kablov E.N., Shchetanov B.V., Ivahnenko Yu.A., Balinova Yu.A. Perspektivnye armiruyushhie vysokotemperaturnye volokna dlya metallicheskih i keramicheskih kompozicionnyh materialov [Perspective reinforcing high-temperature fibers for metal and ceramic composite materials] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №2. St. 05. Available at: http://www.viam-works.ru (accessed: June 10, 2015).
  6. Kablov E.N., Gerasimov V.V., Visik E.M., Demonis I.M. Rol napravlennoj kristallizacii v resursosberegayushhej tehnologii proizvodstva detalej GTD [Role of the directed crystallization in the resource-saving production technology of details of GTE] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №3. St. 01. Available at: http://www.viam-works.ru (accessed: June 10, 2015).
  7. Shhetanov B.V., Kuptsov R.S., Svistunov V.I. Metody polucheniya monokristallicheskih volokon oksida alyuminiya dlya sozdaniya kompozicionnyh materialov i vysokotemperaturnoj volokonnoj optiki [Methods of receiving single-crystal fibers of aluminum oxide for creation of composite materials and high-temperature fiber optics] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №4. St. 01. Available at: http://www.viam-works.ru (accessed: June 10, 2015).
  8. Grishina O.I., Kochetov V.N., Shavnev A.A., Serpova V.M. Aspecty primeneniya vysokoprochnyh i vysokomodulnyh voloknistyh metallicheskih kompozitsionnyh materialov aviatsionnogo naznacheniya (obzor) [Aspects of application of high-strength and high-modulus fiber metal composite materials for aeronautical purpose (review)] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №10. St. 05. Available at: http://www.viam-works.ru (accessed: June 10, 2015). DOI: 10.18577/2307-6046-2014-0-10-5-5.
  9. Kompozicionnye materialy: Spravochnik / pod red. D.M. Karpinosa [Composite materials: the directory / ed. by D.M. Karpinosa]. Kiev: Naukova dumka, 1985. C. 110–124.
  10. Itogi nauki i tehniki. Kompozicionnye materialy / pod. red. L.P. Kobets [Science and equipment results. Composite materials / ed. by L.P. Kobets]. M.: VINITI, 1988. T. 3. S. 65–75.
  11. Chawla N., Chawla K.K. Metal Matrix Composites. Springer Sience+Business Media Inc., 2006. 401 p.
  12. Sholoshov M.H., Kolpashnikov A.I., Kostikov V.I. i dr. Voloknistye kompozicionnye materialy s metallicheskoj matricej [Fibrous composite materials with metal matrix]. M.: Mashinostroenie, 1981. C. 12–45.
  13. Vashukov Yu.A. Tehnologiya raketnyh i aerokosmicheskih konstrukcij iz kompozitnyh materialov: multimed. obrazovat. modul [Technology of rocket and space designs from composite materials: multimedical to form. module]. Samara: Izd-vo SGAU. 2012. (CD-R-disk).
  14. Ping Shen, Hidetoshi Fujii, Taihei Matsumoto, Kiyoshi Nog. Critical Factors Affecting the Wettability of α-alumina by Molten Aluminum // J. Am. Ceram. Soc. 2004. V. 87. №11. Р. 2151–2159.
  15. Jonas T.R., Cornie J.A., Russell K.C. Interfaces and Wetting of Alumina Particulates Preforms by Aluminum and Aluminum-Magnesium Alloys // Metall. Trans. A. 1995. V. 26A. P. 1491–1497.
  16. Hallstedt B., Liu Z.K., Agren J. Reactions in Al2О3–Mg Metal-Matrix Composites During Prolonged Heat-Treatment At 400°C, 550°C and 600°C // Mater. Sci. Eng. A. 1993. V. 169. P. 149–157.
  17. Levi C.G., Abbaschian G.L., Mehrabian R. Interface Interactions During Fabrication of Aluminum Alloy – Alumina Fiber Composites // Metall. Trans. 1978. V. 9A. P. 697–710.