Study of the curing processes of electroinsulating varnishes

Nefyodov N.I., Salikhov T.R., Melnikov D.A.
Nefyodov N.I., Salikhov T.R., Melnikov D.A. Study of the curing processes of electroinsulating varnishes // Proceedings of VIAM. 2016. No. 6. DOI: 10.18577/2307-6046-2016-0-6-9-9. URL: https://viam-works.ru/en/journal/2016/6/9
Keywords
fluoropolyurethanes, process of urethane formation, polyisocyanate, conformal coatings.
Abstract

The process of urethane formation of varnish compositions based on fluorinated oligomers was investigated. Reaction of producing conformal coatings based on film-forming fluoropolyurethanes was presented and their adhesion, physical- mechanical, electroinsulating properties and water absorption were investigated in the article. Work is executed within implementation of the complex scientific direction 17.7. «Paint- and- lacquer materials and coatings on polymeric basis» («The strategic directions of development of materials and technologies of their processing for the period till 2030»)

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  2. Malichenko B.F. Ftorsoderzhashhie poliamidy i poliuretany [Fluorinated polyamides and poliuretany]. Kiev: Naukova dumka, 1977. 232 s.
  3. Lipatova T.E., Ivashhenko V.K. Sintez i fiziko-himiya polimerov (poliuretany) [Synthesis and physics chemistry of polymers (poliuretany)]. Kiev: Naukova dumka, 1970. S. 73–96.
  4. Lipatov Yu.S., Kercha Yu.Yu., Sergeeva L.M. Struktura i svojstva poliuretanov [Structure and properties poliuretanov]. Kiev: Naukova dumka, 1970. 280 s.
  5. Kondrashov E.K., Kozlova A.A., Malova N.E. Issledovanie kinetiki otverzhdeniya ftorpoliuretanovyh emalej alifaticheskimi poliizocianatami razlichnyh tipov [Study and curing kinetics of fluoropolyurethane enamels by the use of aliphatic polysocyanates of various types] // Aviacionnye materialy i tehnologii. 2013. №1. S. 48–49.
  6. Istoriya aviacionnogo materialovedeniya. VIAM – 80 let: gody i lyudi / pod obshh. red. E.N. Kablov [History of aviation materials science. VIAM – 80 years: years and people / gen. ed. by E.N. Kablov]. M.: VIAM, 2012. 520 s.
  7. Kablov E.N. Materialy i himicheskie tehnologii dlya aviacionnoj tehniki [Materials and chemical technologies for aviation engineering] // Vestnik Rossijskoj akademii nauk. 2012. T. 82. №6. S. 520–530.
  8. Kondrashov E.K., Kuznetsova V.A., Semenova L.V., Lebedeva T.A., Malova N.E. Razvitie aviacionnyh lakokrasochnyh materialov [Development of aviation paint and varnish materials] // Vse materialy. Enciklopedicheskij spravochnik. 2012. №5. S. 49–54.
  9. Kondrashov Je.K., Kuznetsova V.A., Semenova L.V., Lebedeva T.A. Osnovnye napravleniya povysheniya jekspluatacionnyh, tehnologicheskih i jekologicheskih harakteristik lakokrasochnyh pokrytij dlya aviacionnoj tehniki [The main directions of increase of utilization, technical and ecological properties of paint coatings for aviation engineering] // Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 96–102.
  10. Kuznetsova V.A., Semenova L.V., Kondrashov E.K., Lebedeva T.A. Lakokrasochnye materialy s ponizhennym soderzhaniem vrednyh i toksichnyh komponentov dlya okraski agregatov i konstrukcij iz PKM [Paint-and-lacquer materials with a low content of harmful and design of polymer composite materials] // Trudy VIAM: elektron. nauch-tehnich. zhurn. 2013. №8. St. 05. Available at: http://www.viam-works.ru (accessed: December 17, 2015).
  11. Buznik V.M. Sverhgidrofobnye materialy na osnove ftorpolimerov [Superwaterproof materials on the basis of fluoropolymers] // Aviation materials and technologies] // Aviacionnye materialy i tehnologii. 2013. №1. S. 29–34.
  12. Beider E.Ya., Donskoi A.A., Zhelezina G.F., Kondrashov E.K., Sytyi Y.V., Surnin E.G. An experience of using fluoropolymer materials in aviation engineering // Russian Journal of General Chemistry. 2009. T. 79. №3. P. 548–564.
  13. Semenova L.V., Malova N.E., Kuznetsova V.A., Pozhoga A.A. Lakokrasochnye materialy i pokrytiya [Paint and varnish materials and coatings] // Aviacionnye materialy i tehnologii. 2012. №S. S. 315–327.
  14. Nefedov N.I., Semenova L.V., Onosova L.A. Issledovanie processov otverzhdeniya ftorpolimernyh kompozicij [Research of processes of curing of ftorpolimerny compositions] // Vse materialy. Enciklopedicheskij spravochnik. 2013. №11. S. 23–27.
  15. Nefedov N.I., Salihov T.R., Mel'nikov D.A. Issledovanie processa otverzhdeniya ftorsoderzhashhih oligomerov i konformnyh pokrytij na ih osnove [Research of process of curing of fluorinated oligomers and conformal coverings on their basis] // Lakokrasochnye materialy i ih primenenie. 2015. № 1–2. S. 62–65.
  16. Nefyodov N.I., Semyonova L.V. Nanesenie lakokrasochnyh pokrytij metodom «syroj po syromu» [The application of paint and varnish coatings by method «crude on crude»] // Aviacionnye materialy i tehnologii. 2013. №4. S. 39–42.
  17. Semenova L.V., Kondrashov E.K. Modificirovannyj bromjepoksidnyj lak VL-18 dlya zashhity polimernyh kompozicionnyh materialov [Modified bromepoksidny varnish VL-18 for protection of polymeric composite materials] // Aviacionnye materialy i tehnologii. 2010. №1. S. 29–32.
  18. Nefyodov N.I., Semyonova L.V. Tendencii razvitiya v oblasti konformnyh pokrytij dlya vlagozashhity i elektroizolyacii plat pechatnogo montazha i jelementov radiojelektronnoj apparatury [Development of tendencies in the field of conformal coatings for the moisture protection and electrical insulation of printed circuit boards and electronic element] // Aviacionnye materialy i tehnologii. 2013. №1. S. 50–52.