Effect of Co and Sc on mechanical properties and corrosion resistance of middle-strength Al–Zn–Mg alloy with small addition of Cu

Ryabov D.K., Kolobnev N.I., Ivanova A.O.
Ryabov D.K., Kolobnev N.I., Ivanova A.O. Effect of Co and Sc on mechanical properties and corrosion resistance of middle-strength Al–Zn–Mg alloy with small addition of Cu // Proceedings of VIAM. 2016. No. 6. DOI: 10.18577/2307-6046-2016-0-6-1-1. URL: https://viam-works.ru/en/journal/2016/6/1
Keywords
Al–Zn–Mg(–Cu), Al-Zn-Mg(–Cu), extrusions, ingots, microstructure, alloying, cobalt, scandium.
Abstract

Improvement of characteristics of aluminum alloys is a topical issue because of increasing requirements to weight efficiency of advanced structures for aeronautic and mechanical engineering. One of ways to improve strength of aluminum alloys is the alloying with elements, which modifies structure. This paper deals with the results of research of the influence of scandium and cobalt on microstructure of ingots and extruded profiles of aluminum alloy of 1913 type as well as their influence on tensile strength and corrosion resistance after complete cycle of heat treatment. Work is executed within implementation of the complex scientific direction 8.1 «High-strength welded aluminum and aluminum - lithium alloys with lower density andincreased fracture toughness» («The strategic directions of development of materials and technologies of their processing for the period till 2030»)

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  2. Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace materials science] // Vse materialy. Jenciklopedicheskij spravochnik. 2008. №3. S. 2–14.
  3. Kablov E.N. Sovremennye materialy – osnova innovacionnoj modernizacii Rossii [Modern materials – basis of innovative modernization of Russia] // Metally Evrazii. 2012. №3. S. 10–15.
  4. Kablov E.N., Ospennikova O.G., Vershkov A.V. Redkie metally i redkozemelnye elementy – materialy sovremennyh i budushhih vysokih tehnologij [Rare metals and rare earth elements – materials of modern and future high technologies] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №2. St. 01. Available at: http://www.viam-works.ru (accessed: September 24, 2015).
  5. Kablov E.N., Logunov A.V., Sidorov V.V. Mikrolegirovanie RZM – sovremennaya tehnologiya povysheniya svojstv litejnyh zharoprochnyh nikelevyh splavov [RZM microalloying – modern technology of increase of properties of cast heat resisting nickel alloys] // Perspektivnye materialy. 2001. №1. S. 23–34.
  6. Ryabov D.K., Kolobnev N.I., Mahsidov V.V., Fomina M.A. O stabilnosti peresyshhennogo tverdogo rastvora listov splava 1913 pri zakalke [About stability of super-saturated solid solution of sheets of alloy 1913 when tempering] // Metallurgiya mashinostroeniya. 2012. №3. S. 30–33.
  7. Ryabov D.K., Kolobnev N.I., Samohvalov S.V., Mahsidov V.V. Vliyanie predvaritelnogo estestvennogo stareniya na svojstva splava 1913 v iskusstvenno sostarennom sostoyanii [Influence of preliminary natural aging on properties of alloy 1913 in artificially made old condition] // Aviacionnye materialy i tehnologii. 2013. №2. S. 8–11.
  8. Ryabov D.K., Kolobnev N.I., Samohvalov S.V., Vahromov O.V. Izmenenie mehanicheskih i korrozionnyh svojstv splava 1913 pri iskusstvennom starenii [Change of mechanical and corrosion properties of alloy 1913 at artificial aging] // Voprosy materialovedeniya. 2013. №4 (76). C. 24–29.
  9. Elagin V.I. Legirovanie deformirovannyh alyuminievyh splavov perehodnymi metallami [Alloying of the deformed aluminum alloys transition metals]. M.: Metallurgiya, 1975. 321 s.
  10. Fridlyander I.N. Vysokoprochnye deformiruemye alyuminievye splavy [High-strength deformable aluminum alloys]. M.: Oborongiz, 1960. 290 s.
  11. Fridlyander I.N. Alyuminievye deformiruemye konstrukcionnye splavy [Aluminum deformable structural alloys]. M.: Metallurgiya, 1979. 208 s.
  12. Berezina A.L., Kolobnev N.I., Molebny O.A., Rud A.D., Shmatko O.A. Effect of Sc, Zr on the Al–Cu–Li alloys structure and properties in the dependence of Cu concentration // Proceeding of the International Coonference «Light Alloys and Composites». Poland. Zakopane. 1999. P. 147–155.
  13. Zaharov V.V., Rostova T.D. Uprochnenie alyuminievyh splavov pri legirovanii ih skandiem [Hardening of aluminum alloys at alloying their scandium] // Metallovedenie i termicheskaya obrabotka metallov. 2013. №12 (702). S. 24–29.
  14. Yin Z., Yang L., Pan Q., Jiang F. // Trans. Nonferrous Met. Soc. China. 2001. V. 11. P. 822–825.
  15. Wloka J., Virtanen S. Influence of scandium on the pitting behaviour of Al–Zn–Mg–Cu alloys // Acta Materialia. V. 55 (2007). P. 6666–6672.
  16. Nwambu C.N., Nnuka E.E., Odo J.U., Nwoye C.I., Nwakpa S.O. Effect of molybdenum and cobalt addition on structure and mechanical properties of aluminium-12,5% silicon alloy // International Journal of Engineering Science Invention. 2014. V. 3. Issue 4. P. 20–24.
  17. Sani A.S., Aliyu I., Polycarp E. Effect of chromium and cobalt additions on the corrosion resistance of aluminium silicon iron alloy (Al–Si–Fe) // International Journal of Scientific & Engineering Research. 2012. V. 3. Issue 12. P. 1–10.
  18. Ryabov D.K., Kolobnev N.I., Kochubej A.Ya., Zavodov A.V. Izmenenie mehanicheskih svojstv listov iz splava 1913 pri vvedenii skandiya [Changing of mechanical properties of 1913 alloy sheets after scandium addition] // Aviacionnye materialy i tehnologii. 2014. №4. S. 3–8.
  19. Ryabov D., Kolobnev N., Samohvalov S. Effect of scandium addition on mechanical properties and corrosion resistance of medium strength Al–Zn–Mg(–Cu) alloy // Materials Science Forum. 2014. V. 794–796. P. 241–246.