Underlying factors preventing the introduction of polymer composite materials in Russia (review)

Daskovskiy M.I., Doriomedov M.S., Skripachyov S.Yu.
Daskovskiy M.I., Doriomedov M.S., Skripachyov S.Yu. Underlying factors preventing the introduction of polymer composite materials in Russia (review) // Proceedings of VIAM. 2016. No. 5. DOI: 10.18577/2307-6046-2016-0-5-6-6. URL: https://viam-works.ru/en/journal/2016/5/6
Abstract

The article provides information on the basic factors influencing the widespread implementation and use of composite materials (composites), structures and products from them in various industries in Russia. Since production of composites in Russia is at the initial stage of development, the identification and resolution of problems of implementation of composite materials is an important task. In order to increase the efficiency of production of composite materials and the simultaneous growth of domestic demand for them it is needed to systematize impeding factors and develop preventive measures to address them. Work is executed within implementation of the complex scientific direction 13.2. «Structural PСM» («The strategic directions of development of materials and technologies of their processing for the period till 2030»)

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  2. Dospehi dlya «Burana». Materialy i tehnologii VIAM dlya MKS «Energiya–Buran» / pod obshh. red. E.N. Kablova [Armor for «Buran». VIAM’s materials and technologies for ISS of «Energiya–Buran» / ed. by E.N. Kablova]. M.: Fond «Nauka i zhizn», 2013. 128 s.
  3. Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace materials science] // Vse materialy. Enciklopedicheskij spravochnik. 2008. №3. S. 2–14.
  4. Kablov E.N. Materialy i himicheskie tehnologii dlya aviacionnoj tehniki [Materials and chemical technologies for aviation engineering] // Vestnik Rossijskoj akademii nauk. 2012. T. 82. №6. S. 520–530.
  5. Vlasenko F.S., Raskutin A.E. Primenenie polimernyh kompozicionnyh materialov v stroitelnyh konstrukcijah [Applying FRP in building structures] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №8. St. 03. Available at: http://www.viam-works.ru (accessed: October 24, 2015).
  6. Kablov E.N. Sovremennye materialy – osnova innovacionnoj modernizacii Rossii [Modern materials – basis of innovative modernization of Russia] // Metally Evrazii. 2012. №3. S. 10–15.
  7. Kablov E.N. VIAM: prodolzhenie puti [VIAM: way continuation] // Nauka v Rossii. 2012. №3. S. 36–44.
  8. Kablov E.N. Pravo na rejting. Kak ocenit intellektualnyj resurs Rossii? [Right to rating. How to evaluate intellectual resource of Russia?] // Poisk. 2013. №45–46. S. 11.
  9. Kablov E.N. VIAM. Napravlenie glavnogo udara [Direction of main attack] // Nauka i zhizn. 2012. №6. S. 14–18.
  10. Kablov E.N. Na perekrestke nauki, obrazovaniya i promyshlennosti [At intersection of science, education and the industry] // Ekspert. 2015. №15 (941). S. 49–53.
  11. Kablov E.N. Rossiya na rynke intellektualnyh resursov [Russia in the market of intellectual resources] // Ekspert. 2015. №28 (951). S. 48–51.
  12. Petrov A.V., Doriomedov M.S., Skripachev S.Yu. Tehnologii utilizacii polimernyh kompozicionnyh materialov (obzor) [Recycling technologies of polymer composite materials (review)] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №8. St. 09. Available at: http://viam-works.ru (accessed: October 24, 2015). DOI: 10.18577/2307-6046-2015-0-8-9-9.
  13. Petrov A.V., Doriomedov M.S., Skripachev S.Yu. Zarubezhnyj opyt razvitiya proizvodstva izdelij s ispolzovaniem vtorichno pererabotannyh polimernyh kompozicionnyh materialov [Foreign experience of development of production of products with use for the second time the processed polymeric composite materials] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №12. Ст. 12. URL: http://www.viam-works.ru (accessed: October 24, 2015). DOI: 10.18577/2307-6046-2015-0-12-12-12.
  14. Babin A. N. Svyazujushhie dlya polimernyh kompozicionnyh materialov novogo pokoleniya [Binding for polymeric composite materials of new generation] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №4. St. 11. Available at: http://www.viam-works.ru (accessed: October 24, 2015).
  15. Sharova I. A. Otechestvennyj i zarubezhnyj opyt v oblasti razrabotki epoksidnyh kleev holodnogo otverzhdeniya [Domestic and foreign experience in area of cold curing epoxy adhesive development] // Trudy VIAM : electron. elektron. nauch.-tehnich. zhurn. 2014. №7. St. 05. Available at: http://www.viam-works.ru (accessed: October 24, 2015). DOI: 10.18577/2307-6046-2014-0-7-5-5.