The phase composition and structure of the niobium-silicon composite manufactured by directional solidification in the liquid metal cooler

Kuzmina N.A., Bondarenko Yu.A.
Kuzmina N.A., Bondarenko Yu.A. The phase composition and structure of the niobium-silicon composite manufactured by directional solidification in the liquid metal cooler // Proceedings of VIAM. 2016. No. 5. DOI: 10.18577/2307-6046-2016-0-5-3-3. URL: https://viam-works.ru/en/journal/2016/5/3
Abstract

The research of high-temperature heat-resistant alloy based on niobium-silicon system – Nb–Nb5Si3, obtained in the process of high-gradient directional solidification with a flat growth front without the use of seed has been carried out. The data of metallography and X-ray powder diffraction have been obtained, phase, structural and quantitative analysis has been carried out, crystallographic orientation of the matrix and reinforcing phases of eutectic composite has been determined. The comparative description of structural parameters of the phases at different stages of solidification along the height of the ingot from the beginning of solidification to the residual melt has been provided. Work is executed within implementation of the complex scientific direction 9.4. «Composites on the basis of the refractory metals, strengthened by intermetallic compound» («The strategic directions of development of materials and technologies of their processing for the period till 2030»)

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  2. Tolorajya V.N., Kablov E.N., Orehov N.G. Tehnologii litya monokristallicheskih turbinnyh lopatok GTD i GTU [Casting technologies of single-crystal turbine blades of GTE and GTU] // Aviacionnye materialy i tehnologii. 2003. №1. S. 63–79.
  3. Kablov E.N., Tolorajya V.N., Orehov N.G., Demonis I.M. Razrabotka zharoprochnogo renijsoderzhashhego nikelevogo splava novogo pokoleniya dlya litya monokristallicheskih turbinnyh lopatok sovremennyh GTD [Development of heat resisting rhenium containing nickel alloy of new generation for molding of single-crystal turbine blades of modern GTE] // Aviacionnye materialy i tehnologii. 2004. №1. S. 146–163.
  4. Kablov E.N., Petrushin N.V., Svetlov I.L., Demonis I.M. Nikelevye litejnye zharoprochnye splavy novogo pokoleniya [Nickel foundry heat resisting alloys of new generation] // Aviacionnye materialy i tehnologii. 2012. №S. C. 36–52.
  5. Bazyleva O.A., Bondarenko Yu.A., Timofeeva O.B., Chabina E.B. Intermetallidnye kompozicii na osnove Ni3Al, legirovannye reniem [Intermetallidnye of composition on the basis of Ni3Al, alloyed by rhenium] // Metallurgiya mashinostroeniya. 2011. №4. S. 30–34.
  6. Nazarkin R.M. Rentgenodifrakcionnye metodiki precizionnogo opredeleniya parametrov kristallicheskih reshetok nikelevyh zharoprochnyh splavov (kratkij obzor) [X-ray diffraction techniques for precise determination of lattice constants in Ni-based superalloys: a brief review] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 41–48.
  7. Dimiduk D.M., Mendiratta M.G., Subramanian P.R. Development approach for advanced intermetallic materials // Structural Intermetallics. Warrendale: TMS Publications. 1993. P. 619–630.
  8. Bewlay B.P., Jackson M.R., Sutliffe J.A., Lipsitt H.A., Reeder W.J. Solidification processing of high temperature intermetallic eutectic-based alloys // Mater. Sci. 1995. A192/193. P. 534–543.
  9. Tolorajya V.N., Kablov E.N., Orehov N.G., Chubarova E.N. Metody polucheniya monokristallov nikelevyh zharoprochnyh splavov [Methods of receiving monocrystals of nickel hot strength alloys] // Gornyj informacionno-analiticheskij byulleten. 2005. Tematicheskoe prilozhenie «Funkcionalnye materialy». S. 172–190.
  10. Bewlay B.P., Jacson M.R., Lipsitt H.A. The Balance of Mechanical and Environmental Properties of a Multielement Niobium-Niobium Silicide-Based In-Situ Composite // Metallurgical and Materials Transactions A. 1996. V. 27A. Issues 12. P. 3801–3808.
  11. Bewlay B.P., Jacson M.R., Subramanian P.R. Processing of High-Temperature Refractory-Metal Siliside In-Situ Composites // JOM. 1999. P. 32–36.
  12. Bondarenko Yu.A., Kablov E.N. Napravlennaya kristallizaciya zharoprochnyh splavov s povyshennym temperaturnym gradientom [The directed crystallization of hot strength alloys with the raised temperature gradient] // MITOM. 2002. №7. S. 20–23.
  13. Kablov E.N., Tolorajya V.N., Demonis I.M., Orehov N.G. Napravlennaya kristallizaciya zharoprochnyh nikelevyh splavov [The directed crystallization of heat resisting nickel alloys] // Tehnologiya legkih splavov. 2007. №2. S. 60–70.
  14. Shishkareva L.M., Kuzmina N.A. Obzor metodik opredeleniya kachestva struktury monokristallicheskih otlivok zharoprochnyh splavov [Review of methods for determining the quality of the structure of single-crystal superalloy castings] // Trudy VIAM: elektron. nauch.-tehni. zhurn. 2014. №1. St. 06. Available at: http://www.viam-works.ru (accessed: October 06, 2015). DOI: 10.18577/2307-6046-2014-0-1-6-6.
  15. Timofeyeva O.B., Kolodochkina V.G., Shvanova N.F., Neiman A.V. Issledovanie mikrostruktury vysokotemperaturnogo estestvenno kompozicionnogo materiala na osnove niobija, uprochnennogo intermetallidami silicida niobiya [The microstructure analysis of niobium-based high-temperature natural composite material reinforced with niobium silicide intermetallics] //Aviacionnye materialy i tehnologii. 2015. №1. S. 60–64.