An overview of production methods of master alloy Al–Sr

Pentuykhin S.I., Popov D.A., Ogorodov D.V., Trapeznikov A.V.
Pentuykhin S.I., Popov D.A., Ogorodov D.V., Trapeznikov A.V. An overview of production methods of master alloy Al–Sr // Proceedings of VIAM. 2016. No. 5. DOI: 10.18577/2307-6046-2016-0-5-2-2. URL: https://viam-works.ru/en/journal/2016/5/2
Abstract

This article reviews and analyzes raw materials and production methods of aluminum strontium master alloy, such as the alloying of pure components, metallothermic recovery of strontium from its compounds, electrolytic recovery. Aluminum–strontium master alloy is intended for modifying the microstructure of hypoeutectic and eutectic cast aluminium alloys. To date, the most promising technique of inoculation is the introduction of strontium in the form of double or triple addition alloy. This alloy changes the leaf-shaped aluminum-silicon eutectic for grainy one, which significantly improves the mechanical properties of the casting. Research is executed within implementation of the complex scientific direction 8.4. «High-strength corrosion-resistant weldable magnesium and cast aluminum alloys for products of aerospace engineering of new generation» («The strategic directions of development of materials and technologies of their processing for the period till 2030»)

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  2. Kablov E.N. Materialy i himicheskie tehnologii dlya aviacionnoj tehniki [Materials and chemical technologies for aviation engineering] // Vestnik Rossijskoj akademii nauk. 2012. T. 82. №6. S. 520–530.
  3. Napalkov V.I., Mahov S.V. Legirovanie i modificirovanie alyuminiya i magniya [Alloying and aluminum and magnesium modifying]. M.: MISIS, 2002. 376 s.
  4. Diagrammy sostoyaniya dvojnyh metallicheskih sistem: spravochnik v 3-h tomah / pod obshh. red. N.P. Lyakisheva [Charts of condition of double metal systems: the directory in 3 vol. / ed. by N.P. Lyakishev]. M.: Mashinostroenie, 1996. T. 1. 992 s.
  5. Illarionov E.I., Kolobnev N.I., Gorbunov P.Z., Kablov E.N. Alyuminievye splavy v aviakosmicheskoj tehnike [Aluminum alloys in aerospace equipment]. M.: Nauka, 2001. 192 s.
  6. Belov N.A. Ekonomnolegirovannye zharoprochnye alyuminievye splavy: principy optimizacii fazovogo sostava [Economically alloyed heat resisting aluminum alloys: principles of optimization of phase structure] // Aviacionnye materialy i tehnologii. 2011. №2. S. 6–11.
  7. Antipov V.V., Senatorova O.G., Tkachenko E.A., Vahromov R.O. Alyuminievye deformiruemye splavy [Aluminum deformable alloys] //Aviacionnye materialy i tehnologii. 2012. №S. S. 167–182.
  8. Aluminium-strontium master alloy – produced by adding strontium encased in aluminium foil, to aluminium melt: pat. 2658308 DE. 1978.
  9. Process for preparing a strontium and/or barium alloy: pat. 3567429 US. 1971.
  10. Korс B. Zagaduienie trwaiсj modufikacji siluminow. Praca: Doktorska. Politechnika Warszawska. 1981. 342 p.
  11. Napalkov V.I., Nerubashhenko V.V., Bondarev B.I. i dr. Proizvodstvo ligatur v usloviyah polucheniya jelektrolizom [Production of ligatures in the conditions of receiving by electrolysis] // Tehnologiya legkih splavov. 1976. №2. S. 24–27.
  12. Kornysheva I.S., Volkova E.F., Goncharenko E.S., Muhina I.Yu. Perspektivy primeneniya magnievyh i litejnyh alyuminievyh splavov [Perspectives of application of magnesium and cast aluminum alloys] // Aviacionnye materialy i tehnologii. 2012. №S. S. 212–222.
  13. Kablov E.N. Kontrol kachestva materialov – garantiya bezopasnosti ekspluatacii aviacionnoj tehniki [Quality control of materials – security accreditation of operation of aviation engineering] // Aviacionnye materialy i tehnologii. 2001. №1. S. 3–8.
  14. Lysenko A.P., Chudarev A.A., Logacheva O.A. Sposob polucheniya ligatury alyuminij stroncij [Way of receiving ligature aluminum strontium] // Tsvetnye Metally. 1994. №10. S. 28–31.
  15. Ganiev I.N., Vahobov A.V., Dzhuraev T.D. Diagramma sostoyaniya Al–Si–Sr [Chart of condition of Al–Si–Sr] // Izv. AN SSSR. Ser.: Metally. 1977. №4. S. 215–218.