The role of anti-adhesive coatings in the technological process of PCM molding

Satdinov R.A., Veshkin E.A, Postnov V.I., Abramov P.A.
Satdinov R.A., Veshkin E.A, Postnov V.I., Abramov P.A. The role of anti-adhesive coatings in the technological process of PCM molding // Proceedings of VIAM. 2016. No. 4. DOI: 10.18577/2307-6046-2016-0-4-10-10. URL: https://viam-works.ru/en/journal/2016/4/10
Abstract

Growth of production volume of parts from polymeric composite materials (PCM) causes development of the industry of supporting materials for their manufacturing. Lubricants for creation of anti-adhesive coatings are among the most important of them. Anti-adhesive coatings of different types using for protection of molding surface of tooling when manufacturing parts from polymeric composition materials are studied in this article. Work is conducted on estimations of anti-adhesive coatings for stability and transferring ability on manufactured parts as well as efforts of the removal of parts and binding residue from tooling. Coating is chosen for manufacturing parts with a gel-coat layer. Work is conducted on measuring interfacial angle on the surface of anti-adhesive coatings. Influence of the anti-adhesive coatings on basic properties of polymeric composition materials is investigated Work is executed within implementation of the complex scientific direction 13.2 «Structural PCM» («T

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  2. Prognozy razvitiya mirovogo rynka grazhdanskoj aviacii [Forecasts of development of the world market of civil aviation ] // TI CAGI. 2003. №3–4. S. 6.
  3. Available at: http://www.airbus.com (accessed: August 12, 2015).
  4. Kablov E.N., Kirillov V.N., Zhirnov A.D., Starcev O.V., Vapirov Yu.M. Centry dlya klimaticheskih ispytanij aviacionnyh PKM [The centers for climatic tests of aviation PCM] // Aviacionnaya promyshlennost. 2009. №4. S. 36–46.
  5. Kablov E.N., Grashhenkov D.V., Erasov V.S., Anchevskij I.Je., Il'in V.V., Valter R.S. Stend dlya ispytaniya na klimaticheskoj stancii GCKI krupnogabaritnyh konstrukcij iz PKM [The stand for testing for the GTsKI climatic stations of large-size designs from PCM] / V sb. dokl. IX Mezhdunarod. nauch. konf. po gidroaviacii «Gidroaviasalon–2012». 2012. S. 122–123.
  6. Spravochnik po kompozicionnym materialam [Directory on composite materials ] / pod red. Dzh. Lyubina. M.: Mashinostroenie, 1988. 446 s.
  7. Polimernye kompozicionnye materialy: struktura, svojstva, tehnologiya [Polymeric composite materials: structure, properties, technology] / pod red. A.A. Berlina. SPb.: Professiya, 2009. 556 s.
  8. Praktikum po kolloidnoj himii i jelektronnoj mikroskopii [Workshop on colloid chemistry and electron microscopy ] / pod red. S.S. Voyuckogo, R.M. Panich. M.: Himiya, 1974. 224 s.
  9. Lipatov Yu.S. Kolloidnaya himiya polimerov [Colloid chemistry of polymers]. Kiev: Naukova dumka, 1984. 844 s.
  10. Postnova M.V., Postnov V.I. Opyt razvitija bezavtoklavnyh metodov formovanija PKM [Development experience out-of-autoclave methods of formation PCM] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №4. St. 06. Available at: http://www.viam-works.ru (accessed: August 12, 2015). DOI: 10.18577/2307-6046-2014-0-4-6-6.
  11. Solncev St.S., Rozenenkova V.A., Mironova N.A., Soloveva G.A. Vysokotemperaturnye pokrytiya na osnove zol-gel tehnologii [High-temperature coatings on basis of sol-gel technology] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №1. St. 03. Available at: http://www.viam-works.ru (accessed: September 01, 2015). DOI: 10.18577/2307-6046-2014-0-1-3-3.
  12. Postnov V.I., Petuhov V.I., Makrushin K.V., Yudin A.A. Issledovanie antiadgezionnyh pokrytij pri formovanii panelej inter'era s gelkoutnym sloem [Research of anti-adhesive coverings at formation of panels of interior with gelkoutny layer] // Aviacionnye materialy i tehnologii. 2009. №3. S. 23–25.
  13. Panshin Yu.A., Malkevich L.G., Dunaevskaya D.S. Ftoroplasty [Fluorine layers]. M.: Himiya, 1978. 232 s.
  14. Kuznetsova V.A., Kuznetsov G.V., Shapovalov G.G. Issledovanie vliyaniya molekulyarnoj massy jepoksidnoj smoly na adgezionnye, fiziko-mehanicheskie svojstva i jerozionnuyu stojkost pokrytij [[Investigation of epoxy resin molecular mass influence by physiomechanical property and erosive resistant of coatings] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №8. St. 08. Available at: http://www.viam-works.ru (accessed: August 26, 2015). DOI: 10.18577/2307-6046-2014-0-8-8-8.
  15. Veshkin E.A., Postnov V.I., Strelnikov S.V., Abramov P.A., Satdinov R.A. Opyt primeneniya tehnologicheskogo kontrolya polufabrikatov PKM [Experience of application of technological control of semi-finished products of PCM] // Izvestiya Samarskogo nauchnogo centra RAN. T. 16. №6 (2). 2014. S. 393–398
  16. Savelev I.V. Kurs obshhij fiziki [Course the general physics]. M.: Fizika, 1970. T. 1. S. 263–265.
  17. Adamson A. Fizicheskaya himiya poverhnostej [Physical chemistry of surfaces]. M.: Mir, 1979. 568 s.
  18. Summ B.D. Gisterezis smachivaniya [Wetting hysteresis]. M.: Akademiya, 2006. 239 s.
  19. Fridrihsberg D.A. Kurs kolloidnoj himii [Course of colloid chemistry]. L.: Himiya, 1974. 352 s.
  20. Zimon A.D. Adgeziya plenok i pokrytij [Adhesion of films and coverings]. M.: Himiya, 1977. 352 s.