Panin P.V., Dzunovich D.А., Shiryaev A.A. Research on thermal stability of VT6 titanium alloy structure after thermohydrogen treatment // Proceedings of VIAM. 2016. No. 3 (39). Ст. 06. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2016-0-3-6-6.

Research on thermal stability of VT6 titanium alloy structure after thermohydrogen treatment

Panin P.V., Dzunovich D.А., Shiryaev A.A.
Abstract

Temperature and duration parameters of multiphase (α+α2+β)-structure stability in VT6 (Ti–6.25Al–4.1V, % wt.) titanium alloyformed by thermohydrogen treatment (THT) upon 0.8% wt. hydrogen doping are determined. It is revealed that the structure after THT with the subsequent vacuum annealing at 625 and 650°С possesses the maximal thermal stability during isothermal ageing (more than 100 hours at temperatures up to 650°С).

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  2. Kablov E.N. Shestoj tehnologicheskij uklad [Sixth technological way] // Nauka i zhizn. 2010. №4. S. 2–7.
  3. Kablov E.N. Materialy i himicheskie tehnologii dlya aviacionnoj tehniki [Materials and chemical technologies for aviation engineering] // Vestnik Rossijskoj akademii nauk. 2012. T. 82. №6. S. 520–530.
  4. Horev A.I. Fundamentalnye i prikladnye raboty po konstrukcionnym titanovym splavam i perspektivnye napravleniya ih razvitiya [Fundamental and applied works on structural titanium alloys and perspective directions of their development] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №2. St. 04. Available at: http://www.viam-works.ru (accessed: June 19, 2015).
  5. Nochovnaya N.A. Perspektivy i problemy primeneniya titanovyh splavov [Perspectives and problems of application of titanium alloys] // Aviacionnye materialy i tehnologii: nauch.-tehnich. sb. M.: VIAM, 2007. Vyp. «Perspektivy razvitiya i primeneniya titanovyh splavov dlya samoletov, raket, dvigatelej i sudov». S. 4–8.
  6. Nochovnaya N.A., Panin P.V., Alekseev E.B., Bokov K.A. Ekonomnolegirovannye titanovye splavy dlya sloistyh metallopolimernyh kompozicionnyh materialov [Low-cost alloyed titanium alloys for metal-polymer laminates] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №11. St. 02. // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №11. St. 02. Available at: http://www.viam-works.ru (accessed: June 19, 2015). DOI: 10.18577/2307-6046-2014-0-11-2-2.
  7. Ilin A.A., Kolachev B.A., Nosov V.K., Mamonov A.M. Vodorodnaya tehnologiya titanovyh splavov [Hydrogen technology of titanium alloys]. M.: Izd. dom MISiS. 2002. 392 s.
  8. Kolachev B.A., Ilin A.A., Nosov V.K., Mamonov A.M. Dostizheniya vodorodnoj tehnologii titanovyh splavov [Achievements of hydrogen technology of titanium alloys] // Tehnologiya legkih splavov. 2007. №3. S. 10–26.
  9. Ilin A.A., Skvorcova S.V., Mamonov A.M., Kollerov M.Yu. Fazovye i strukturnye prevrashheniya v titanovyh splavah raznyh klassov pod dejstviem vodoroda [Phase and structural transformations in titanium alloys of different classes under the influence of hydrogen] // Titan. 2007. №1. S. 32–37.
  10. Skvorcova S.V., Panin P.V., Nochovnaya N.A., Grushin I.A., Mitropolskaya N.G. Vliyanie vodoroda na fazovye i strukturnye prevrashheniya v titanovom splave VT6 [Influence of hydrogen on phase and structural transformations in BT6 titanium alloy] // Tehnologiya legkih splavov. 2011. №4. S. 35–40.
  11. Ilin A.A., Skvorcova S.V., Panin P.V., Shalin A.V. Vliyanie termovodorodnoj obrabotki i plasticheskoj deformacii na strukturoobrazovanie v titanovyh splavah raznyh klassov [Influence of thermohydrogen treating and plastic strain on structurization in titanium alloys of different classes] // Aviacionnaya promyshlennost. 2009. №4. S. 31–36.
  12. Panin P.V., Dzunovich D.A., Zasypkin V.V. Sozdanie dvuhfaznoj kompozitnoj struktury v alfa-splave Ti–6Al s pomoshh'yu termovodorodnoj obrabotki [Creation of diphasic composite structure in Ti–6Al alpha alloy by means of thermohydrogen treating] // Nauchnye trudy (Vestnik MATI). 2012. №19 (91). S. 33–37.
  13. Panin P.V., Grushin I.A., Mitropolskaya N.G. Issledovanie zakonomernostej izmeneniya strukturno-fazovogo sostoyaniya titanovogo splava VT6 pri dopolnitelnom legirovanii vodorodom [Research of patterns of change of structural and phase condition of BT6 titanium alloy at additional alloying hydrogen] // Nauchnye trudy (Vestnik MATI). 2013. №20 (92). S. 31–34.
  14. Panin P.V., Dzunovich D.A., Lukina E.A. Upravlenie strukturoj i svojstvami titanovyh splavov pri obratimom legirovanii vodorodom i plasticheskoj deformacii [Management of structure and properties of titanium alloys at reversible alloying hydrogen and plastic strain] / V sb. materialov XIX nauch.-tehnich. konf. molodyh uchenyh i specialistov. RKK «Jenergiya». 2012. Ser. XII. Vyp. 1–2. S. 103–107.
  15. Panin P.V. Zakonomernosti formirovaniya fazovogo sostava i struktury v titanovyh splavah pri termovodorodnoj obrabotke i plasticheskoj deformacii: avtoref. dis. … kand. tehn. nauk [Patterns of forming of phase structure and structure in titanium alloys at thermohydrogen treating and plastic strain: thesis author's abstract Candidate of Technical Sciences.]. M, 2009. 24 s.
  16. Ovchinnikov A.V., Nosov V.K., Afonin V.E., Panin P.V. Osnovnye zakonomernosti deformacii splavov titan–vodorod [Main patterns of deformation of alloys titanium-hydrogen] // Tehnologiya legkih splavov. 2007. №3. S. 96–99.
  17. Ilin A.A. Mehanizm i kinetika fazovyh i strukturnyh prevrashhenij v titanovyh splavah [The mechanism and kinetics of phase and structural transformations in titanium alloys]. M.: Nauka, 1994. 304 s.
  18. Panin P.V., Dzunovich D.A., Alekseev E.B. Sposoby opisaniya fazovogo sostava titanovyh splavov, dopolnitelno legirovannyh vodorodom (obzor) [Ways of phase areas representation in titanium alloys additionally doped with hydrogen (review)] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №3. St. 03. Available at: http://www.viam-works.ru (accessed: June 19, 2015). DOI: 10.18577/2307-6046-2015-0-3-3-3.
  19. Panin P.V., Shiryaev A.A., Dzunovich D.A. Postroenie temperaturno-koncentracionnoj diagrammy fazovogo sostava titanovogo splava VT6, dopolnitelno legirovannogo vodorodom [Creation of the temperature and concentration chart of phase composition of the BT6 titanium alloy which has been in addition alloyed by hydrogen] // Tehnologiya mashinostroeniya. 2014. №3. S. 5–9.