Specifics of production process of VT40 titanium alloy castings

Kochetkov A.S., Nochovnaya N.A., Bokov K.A.
Kochetkov A.S., Nochovnaya N.A., Bokov K.A. Specifics of production process of VT40 titanium alloy castings // Proceedings of VIAM. 2016. No. 3. DOI: 10.18577/2307-6046-2016-0-3-4-4. URL: https://viam-works.ru/en/journal/2016/3/4
Abstract

The basic stages of producing castings of VT40 alloy, doping system, mold, selecting a mode of ingots and forms melting , HIP modes, method of internal defects diagnostics are considered. Particular attention is paid to complex alloying additions of α- and β-stabilizers, as well as additional doping with oxygen and carbon. The effect of doping on the comprehensive strength of the alloy is shown. The advantages of ceramic molds application comparing with graphite ones are considered. It is found that to obtain high-quality castings it is necessary to observe all technological operations.

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  2. Kablov E.N. Tendencii i orientiry innovacionnogo razvitiya Rossii: sb. nauchno-informacionnyh materialov. 3-e izd., pererab. i dop. [Tendencies and reference points of innovative development of Russia: Saturday. scientific information materials. 3rd ed., processed and added]. M.: VIAM, 2015. S. 427–430.
  3. Kablov E.N. Materialy i himicheskie tehnologii dlya aviacionnoj tehniki [Materials and chemical technologies for aviation engineering] // Vestnik Rossijskoj akademii nauk. 2012. T. 82. №6. S. 520–530.
  4. Tarasov Yu.M., Antipov V.V. Novye materialy VIAM – dlya perspektivnoj aviacionnoj tehkniki proizvodstva OAO «OAK» [The VIAM new materials – for perspective aviation engineering of production of JSC «OAK»] // Aviacionnye materialy i tehnologii. 2012. №2. S. 5–6.
  5. Shmotin Yu.N., Starkov R.Yu., Danilov D.V., Ospennikova O.G., Lomberg B.S. Novye materialy dlya perspektivnogo dvigatelya OAO «NPO „Saturn”» [New materials for the perspective engine of JSC «NPO „Saturn”»] // Aviacionnye materialy i tehnologii. 2012. №2. S. 6–8.
  6. Ilin A.A., Kolachev B.A., Polkin I.S. Titanovye splavy. Sostav, struktura, svojstva: spravochnik [Titanium alloys. Structure, structure, properties: directory]. M.: VILS–MATI, 2009. 520 s.
  7. Nochovnaya N.A. Perspektivy i problemy primeneniya titanovyh splavov [Perspectives and problems of application of titanium alloys] // Aviacionnye materialy i tehnologii: nauch.-tehnich. sb. M.: VIAM, 2007. Vyp. «Perspektivy razvitiya i primeneniya titanovyh splavov dlya samoletov, raket, dvigatelej i sudov»: sb. dokladov yubilejnogo soveshhaniya, posvyashhennogo 55-letiyu titanovoj laboratorii. S. 4–8.
  8. Nochovnaya N.A., Panin P.V., Alekseev E.B., Bokov K.A. Ekonomnolegirovannye titanovye splavy dlya sloistyh metallopolimernyh kompozicionnyh materialov [Low-cost alloyed titanium alloys for metal-polymer laminates] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №11. St. 02. Available at: http://www.viam-works.ru (accessed: September 17, 2015). DOI: 10.18577/2307-6046-2014-0-11-2-2.
  9. Kochetkov A. S., Nochovnaya N.A., Bokov K.A. Osobennosti processa plavki ekonomnolegirovannogo litejnogo titanovogo splava VT40L [Features of melting process of economically alloyed cast VT40L titanium alloy] // Metallurg. 2015. №10. S.81–83.
  10. Magnickij O.N. Litejnye svojstva titanovyh splavov [Foundry properties of titanium alloys]. L.: Mashinostroenie, 1968. 65 s.
  11. Kablov D.E., Panin P.V., Shiryaev A.A., Nochovnaya N.A. Opyt ispolzovaniya vakuumno-dugovoj pechi ALD VAR L200 dlya vyplavki slitkov zharoprochnyh splavov na osnove aljuminidov titana [The use of ADL VAR L200 vacuum-arc furnace for ingots fabrication of high-temperature titanium aluminides base alloys] //Aviacionnye materialy i tehnologii. 2014. №2. S. 27–33.
  12. Yasinskij K.K. Vliyanie soderzhaniya kisloroda na mehanicheskie i tehnologicheskie svojstva litejnyh titanovyh splavov [Influence of the oxygen content on mechanical and technological properties of cast titanium alloys] // Titan. 1998. №10. S. 7–12.
  13. Kalachev B.A. Osnovnye principy legirovaniya titanovyh splavov [Basic principles of alloying of titanium alloys] // Izvestiya vuzov. Cvetnaya metallurgiya. 1996. №4. S. 14–23.
  14. Bratuhin A.G., Bibikov E.L., Glazunov S.G. i dr. Proizvodstvo fasonnyh otlivok iz titanovyh splavov [Production of mold castings from titanium alloys]. M.: Izd-vo VILS, 1998. 154 s.
  15. Andreev A.L., Anoshkin N.F., Bochvar G.A. i dr. Titanovye splavy. Plavka i lite titanovyh splavov [Titanium alloys. Melting and molding of titanium alloys]. M.: Metallurgiya, 1978. 383 s.
  16. Horev A.I., Belov S.P., Glazunov S.G. Metallovedenie titana i ego splavov [Metallurgical science of titanium and its alloys]. M.: Metallurgiya, 1992. 352 s.
  17. Niinomi M. Recent trends in titanium research and development in Japan // Proc. 12th World Conf. on Titanium. 2011. V. I. P. 30–37.
  18. Heglei Qu et al. Defects easy occur in VAR titanium ingots // Proc. 12th World Conf. on Titanium. 2011. V. I. P. 126–129.
  19. Davydenko L.V., Belova S.B., Davydenko R.A., Egorova Yu.B. O vozmozhnosti primeneniya titanovyh splavov v avtomobilestroenii [About possibility of application of titanium alloys in automotive industry] // Avtomobilnaya promyshlennost'. 2010. №10.
  20. S. 41–43.
  21. Cui Chunxiang, Hu BaoMin, Zhao Lichen, Liu Shuangjin. Titanium alloy production technology, market prospects and industry development // Materials and Design. 2011. №32. Р. 1684–1691.
  22. Zhu J. et al. Influence of boron addition on microstructure and mechanical properties of dental cast titanium alloys // Mat. Sci. & Eng.: A. 2003. V. 339 (1–2). P. 53–62.
  23. Schevchenko D.M., Ward R.M. Liquid metal pool behavior during the vacuum arc remelting of INCONEL 718 // Metall. Mater. Trans. B. 2009. V. 40B (6). P. 263.
  24. Thamar E. Mora and Swavik A. Spiewak. Prediction of temperature in vacuum arc remelting in the presence of strong disturbances // Journal of Manufacturing Processes. 2003. V. 5. №1. P. 46–53.
  25. Antashev V.G., Nochovnaya N.A., Shiryaev A.A., Izotova A.Yu. Perspektivy razrabotki novyh titanovyh splavov [Perspectives of development of new titanium alloys] // Vestnik MGTU im. N.E. Baumana. Ser. «Mashinostroenie». 2011. №SP2. S. 60–67.
  26. Nochovnaya N.A., Alekseev E.B., Yasinskij K.K., Kochetkov A.S. Specifika plavki i sposoby polucheniya slitkov intermetallidnyh titanovyh splavov s povyshennym soderzhaniem niobiya [Specifics of melting and ways of receiving ingots of intermetallic titanium alloys with the raised content of niobium] // Vestnik MGTU im. N.E. Baumana. Ser. «Mashinostroenie». 2011. №SP2. S. 53–59.
  27. Kashapov O.S., Novak A.V., Nochovnaya N.A., Pavlova T.V. Sostoyanie, problemy i perspektivy sozdaniya zharoprochnyh titanovyh splavov dlya detalej GTD [Condition, problems and perspectives of creation of heat resisting titanium alloys for GTE details]. Available at: http://www.viam-works.ru (accessed: September 17, 2015).