Prospects of non-autoclave technologies for structural materials manufacturing (review)

Khrulkov A.V., Grigoriev M.M., Yazvenko L.N.
Khrulkov A.V., Grigoriev M.M., Yazvenko L.N. Prospects of non-autoclave technologies for structural materials manufacturing (review) // Proceedings of VIAM. 2016. No. 2. DOI: 10.18577/2307-6046-2016-0-2-6-6. URL: https://viam-works.ru/en/journal/2016/2/6
Keywords
polymer composite materials (PCM), carbon fiber, fiberglass, non-autoclave technology.
Abstract

The use of polymer composite materials is becoming increasingly wide spread. Non-autoclave technology has a very high level of attractiveness, as they allow to avoid the use of expensive equipment while ensuring the required level of properties. Global trends in the development of aviation industry show that the non-autoclave technology will be used in the manufacture of structures for UAVs, missiles, commercial and general aviation.

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  2. Kablov E.N., Grashhenkov D.V., Erasov V.S., Anchevskij I.Ee., Ilin V.V., Valter R.S. Stend dlya ispytaniya na klimaticheskoj stancii GCKI krupnogabaritnyh konstrukcij iz PKM [The stand for testing for the GTsKI climatic stations of large-size designs from PCM] / V sb. dokl. IX Mezhdunarod. nauch. konf. po gidroaviacii «Gidroaviasalon–2012». 2012. S. 122–123.
  3. Timoshkov P.N., Kogan D.I. Sovremennye tehnologii proizvodstva polimernyh kompozicionnyh materialov novogo pokoleniya [Modern production technologies of polymeric composite materials of new generation] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №4. St. 07. Available at: http://www.viam-works.ru (accessed: June 09, 2015).
  4. Sokolov I.I., Raskutin A.E. Ugleplastiki i stekloplastiki novogo pokoleniya [Coalplastics and fibreglasses of new generation] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №4. St. 09. Available at: http://viam-works.ru (accessed: June 09, 2015).
  5. Hrulkov A.V., Dushin M.I., Popov Yu.O., Kogan D.I. Issledovaniya i razrabotka avtoklavnyh i bezavtoklavnyh tehnologij formovaniya PKM [Researches and development autoclave and out-of-autoclave technologies of formation of PCM] //Aviacionnye materialy i tehnologii. 2012. №S. S. 292–301.
  6. Dushin M.I., Hrulkov A.V., Platonov A.A., Ahmadieva K.R. Bezavtoklavnoe formovanie ugleplastikov na osnove prepregov, poluchennyh po rastvornoj tehnologii [Out-of-autoclave formation coal plastics on the basis of the prepregs received on solution technology] // Aviacionnye materialy i tehnologii. 2012. №2. S. 43–48.
  7. Babin A. N. Svyazujushhie dlya polimernyh kompozicionnyh materialov novogo pokoleniya [Binding for polymeric composite materials of new generation] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №4. St. 11. Available at: http://www.viam-works.ru (accessed: June 09, 2015).
  8. Kablov E.N. Materialy i tehnologii VIAM v konstrukciyah perspektivnyh dvigatelej razrabotki OAO «Aviadvigatel» [Materials and VIAM technologies in designs of perspective engines of development of JSC «Aviadvigatel»] // Permskie aviacionnye dvigateli. 2014. №31. S. 43–47.
  9. Muhametov R.R., Ahmadieva K.R., Kim M.A., Babin A.N. Rasplavnye svyazujushhie dlya perspektivnyh metodov izgotovleniya PKM novogo pokoleniya [Melt binding for perspective methods of production of PCM of new generation] // Aviacionnye materialy i tehnologii. 2012. №S. S. 260–265.
  10. Chursova L.V., Dushin M.I., Kogan D.I., Panina N.N., Kim M.A., Gurevich Ya.M., Platonov A.A. Plenochnye svyazujushhie dlya RFI-tehnologii [Film binding for RFI technology] // Rossijskij himicheskij zhurnal. 2010. T. LIV. Materialy dlya aviakosmicheskoj tehniki. S. 63–67.
  11. Kablov E.N., Kondrashov S.V., Yurkov G.Ju. Perspektivy ispolzovaniya uglerodsoderzhashhih nanochastic v svyazuyushhih dlya polimernyh kompozicionnyh materialov [Perspectives of use of carbon-containing nanoparticles in binding for polymeric composite materials] // Rossijskie nanotehnologii. 2013. T. 8. №3–4. S. 24–42.
  12. Wang K., Kelly D., Dutton S. Multi-objective Optimisation of Composite Aerospace Structures. Composite Structures. 2002. P. 141–148.
  13. Grashhenkov D.V., Chursova L.V. Strategiya razvitiya kompozicionnyh i funkcionalnyh materialov [Strategy of development of composite and functional materials] // Aviacionnye materialy i tehnologii. 2012. №S. S. 231–242.
  14. Mikheyev S.V., Bourtsev B.N., Danilkina V.L., Ivannikova R.V., Selemenev S.V., Schetinin Y.S. Kamov Composite Blades // Proceedings of 31st European Rotorcraft Forum. Florence. 2005. Р. 20–22.
  15. Grigorev M.M., Kogan D.I., Gusev Yu.A., Gurevich Ya.M. Osobennosti izgotovleniya PKM metodom vakuumnogo formovaniya preprega [Features of producing composites by vacuum molding of prepreg] // Aviacionnye materialy i tehnologii. 2014. №3. S. 67–71.