The origins of flux corrosion in mouldings made of heatproof cast magnesium alloy ML10

Uridiya Z.P., Mukhina I.Y., Duyunova V.A., Kozlov I.A.
Uridiya Z.P., Mukhina I.Y., Duyunova V.A., Kozlov I.A. The origins of flux corrosion in mouldings made of heatproof cast magnesium alloy ML10 // Proceedings of VIAM. 2016. No. 12. DOI: 10.18577/2307-6046-2016-0-12-2-2. URL: https://viam-works.ru/en/journal/2016/12/2
Keywords
magnesium-zirconium ligature, magnesium alloy, microstructure, macrostructure, zirconium molecular entities, flux inclusion, flux corrosion.
Abstract

The given article presents the results of the research of micro- and macrostructure of magnesium-zirconium additional alloy, preliminary alloy MTsr1N3 and alloy ML10 made of the listed batched materials. The alloying is hard for the elements melting points of which are higher than the melting point of magnesium. The zirconia alloying of magnesium alloys is processed through the preliminary magnesium-zirconium additional alloy melting points of which are lower than the melting point for zirconium. The zirconia alloying of light alloys is difficult not only because the melting points for zirconium are too high, but because of its activity as well: zirconium interacts with hydrogen, oxygen, nitrogen, aluminum, ferrum, silicon, carbon and other elements. The origins of contamination of magnesium alloy ML10 with the elements that are infusible with magnesium, such as intermetallides of zirconium and aluminum or ferrum or silicon and molecular entities of zirconium-oxygen and zirconium-hydr

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kornysheva I.S., Volkova E.F., Goncharenko E.S., Muhina I.Yu. Perspektivy primeneniya magnievyh i litejnyh alyuminievyh splavov [Perspectives of application of magnesium and cast aluminum alloys] // Aviacionnye materialy i tehnologii. 2012. №S. S. 212–222.
  3. Kablov E.N. Osnovnye itogi i napravleniya razvitiya materialov dlya perspektivnoj aviacionnoj tehniki [The main results and the directions of development of materials for perspective aviation engineering] // 75 let. Aviacionnye materialy. Izbrannye trudy «VIAM» 1932–2007: yubilejnyj nauch.-tehnich. sb. M.: VIAM, 2007. S. 20–26.
  4. Kablov E.N. Aviacionnoe materialovedenie: itogi i perspektivy [Aviation materials science: results and perspectives] // Vestnik Rossijskoj akademii nauk. 2002. T. 72. №1. S. 3–12.
  5. Kablov E.N. VIAM: prodolzhenie puti [VIAM: way continuation] // Nauka v Rossii. 2012. №3. S. 36–44.
  6. Kablov E.N. Sovremennye materialy – osnova innovacionnoj modernizacii Rossii [Modern materials – basis of innovative modernization of Russia] // Metally Evrazii. 2012. №3. S. 10–15.
  7. Kablov E.N. Himiya v aviacionnom materialovedenii [Chemistry in aviation materials science] // Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 3–4.
  8. Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace materials science] // Vse materialy. Enciklopedicheskij spravochnik. 2008. №3. S. 2–14.
  9. Korchagina V.A. Radi kachestva magnievyh otlivok [For the sake of quality of magnesian otlivka] // Inzhenernaya gazeta. 2006. №33–34. S. 5.
  10. Sadkov V.V., Laponov Yu.L., Ageev A.P., i dr. Perspektivy i usloviya primeneniya magnievyh splavov v samoletah OAO «Tupolev» [Perspectives and conditions of application of magnesium alloys in JSC Tupolev airplanes] // Metallurgiya mashinostroeniya. 2007. №4. S. 19–23.
  11. Antipov V.V., Vahromov R.O., Duyunova V.A., Nochovnaya N.A. Materialy s vysokoj udel'noj prochnost'yu na osnove alyuminiya, magniya, titana i tehnologii ih pererabotki [Materials with high specific strength on the basis of aluminum, magnesium, titanium and technology of their processing] // Boepripasy i spechimiya. 2013. №3. S. 51–55.
  12. Muhina I.Yu., Uridiya Z.P. Magnij – osnova sverhlegkih materialov [Magnesium – basis of extralight materials] // Metallurgiya mashinostroeniya. 2005. №6. S. 29–31.
  13. Duyunova V.A. Metody zashhity magnievyh splavov v otechestvennom litejnom proizvodstve s 1930-h gg. do nastoyashhego vremeni [Methods of protection of magnesium alloys in domestic foundry production since the 1930th till nowadays] // Litejshhik Rossii. 2010. №10. S. 35–37.
  14. Duyunova V.A., Muhina I.Yu., Uridiya Z.P. Novye protivoprigarnye prisadochnye materialy dlya litejnyh form magnievyh otlivok [New nonstick welding materials for casting molds of magnesian casting] // Litejnoe proizvodstvo. 2009. №9. S. 18–21.
  15. Muhina I.Yu., Duyunova V.A., Uridiya Z.P. Perspektivnye litejnye magnievye splavy [Perspective cast magnesium alloys] // Litejnoe proizvodstvo. 2013. №5. S. 2–5.
  16. Duyunova V.A., Goncharenko N.S., Muhina I.Yu., Uridiya Z.P., Volkova E.F. Nauchnoe nasledie akademika I.N. Fridlyandera. Sovremennye issledovaniya magnievyh i litejnyh alyuminievyh splavov v VIAM [Scientific heritage of academician I.N.Fridlyandera. Modern researches of magnesium and cast aluminum alloys in VIAM] // Tsvetnye metally. 2013. №9. S. 71–78.
  17. Frolov A.V., Muhina I.Yu., Duyunova V.A., Uridiya Z.P. Vliyanie tehnologicheskih parametrov plavki na strukturu i svojstva novyh magnievyh splavov [Influence of technological parameters of melting on structure and property of new magnesium alloys] // Metallurgiya mashinostroeniya. 2014. №2. S. 26–29.
  18. Muhina I.Yu. Litejnye splavy i tehprocessy pri proizvodstve magnievyh otlivok [Cast alloys and technical processes by production of magnesian casting] // Litejnoe proizvodstvo. 2003. №4. S. 18–19.
  19. Goncharenko E.S., Trapeznikov A.V., Ogorodov D.V. Litejnye alyuminievye splavy (k 100-letiyu so dnya rozhdeniya M.B. Altmana) [Aluminium casting alloys] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №4. St. 02. Available at: http://www.viam-works.ru (accessed: June 24, 2016). DOI: 10.18577/2307-6046-2014-0-4-2-2.
  20. Altman M.B. i dr. Magnievye splavy: spravochnik [Magnesium alloys: directory]. M.: Metallurgiya, 1978. T. 2. 147 s.
  21. Uridiya Z.P., Muhina I.Yu., Duyunova V.A., Kosarina E.I. Kontrol kachestva litya iz magnievyh splavov i sposoby vosstanovleniya germetichnosti otlivok [Quality control of magnesium alloy casting and methods of restoration of cast products impermeability] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №12. St. 04. Available at: http://www.viam-works.ru (accessed: June 27, 2016). DOI: 10.18577/2307-6046-2014-0-12-4-4.
  22. Leonov A.A., Duyunova V.A., Stupak E.V., Trofimov N.V. Lite magnievyh splavov v razovye formy, poluchennye novymi metodami [Casting of magnesium alloys in disposable moulds produced by new methods] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №12. St. 01. Available at: http://www.viam-works.ru (accessed: June 28, 2016). DOI: 10.18577/2307-6046-2014-0-12-1-1.
  23. Shishkareva L.M., Kuzmina N.A. Obzor metodik opredeleniya kachestva struktury monokristallicheskih otlivok zharoprochnyh splavov [Review of methods for determining the quality of the structure of single-crystal superalloy castings] // Trudy VIAM: elektron. nauch.-tehni. zhurn. 2014. №1. St. 06. Available at: http://www.viam-works.ru (accessed: June 29, 2016).
  24. Postnov V.I., Burhan O.L., Rahmatullin A.E., Kachura S.M. Nerazrushayushhie metody kontrolya soderzhaniya svyazuyushhih v prepregah i PKM (obzor) [Nondestructive control methods of the content of binders in prepregs and PCM (review)] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №12. St. 06 Available at: http://www.viam-works.ru (accessed: June 27, 2016).
  25. Murashov V.V. Nerazrushayushhij kontrol zagotovok i detalej iz uglerod-uglerodnogo kompozicionnogo materiala dlya mnogorazovogo kosmicheskogo korablya «Buran» [Non-destructive testing of preparations and details from carbon - carbon composite material for the reusable «Buran» spacecraft] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №4. St. 05. Available at: http://www.viam-works.ru (accessed: June 29, 2016).
  26. OST1 90427–94. Kachestvo produkcii. Nerazrushayushhij kontrol lityh detalej i polufabrikatov aviacionnoj tehniki iz alyuminievyh i magnievyh splavov radiograficheskim metodom. Obshhie polozheniya [OCT1 90427-94. Quality of products. Non-destructive testing of cast details and semi-finished products of aviation engineering from aluminum and magnesium alloys radiographic method. General provisions]. M.: VIAM, 1994. S. 1–17.
  27. OST1 90121–90. Magnievye litejnye splavy. Rezhimy termicheskoj obrabotki [OCT1 90121-90. Magnesium cast alloys. Modes of thermal processing]. M.: VIAM, 1990. S. 1–10.
  28. Kablov E.N., Muhina I.Yu., Korchagina V.A. Prisadochnye materialy dlya formovochnyh smesej pri lite magnievyh splavov [Binders materials for forming mixes when molding magnesium alloys] // Litejnoe proizvodstvo. 2007. №5. S. 15–18.
  29. Uridiya Z.P., Mukhina I.Y., Frolov A.V., Leonov A.A. Issledovanie mikrostruktury magnievo-cirko-nievoj ligatury i zharoprochnogo litejnogo magnievogo splava ML10 [Study of microstructure of magnesium-zirconium master alloy and heat-resistant magnesium alloy ML10] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №10. St. 06. Available at: http://www.viam-works.ru (accessed: June 29, 2016). DOI: 10.18577/2307-6046-2015-0-10-6-6.