Polycyanurates binding for composites production by impregnation under pressure

Merkulova Yu.I., Mukhametov R.R., Dolgova E.V., Akhmadieva K.R.
Merkulova Yu.I., Mukhametov R.R., Dolgova E.V., Akhmadieva K.R. Polycyanurates binding for composites production by impregnation under pressure // Proceedings of VIAM. 2016. No. 11. DOI: 10.18577/2307-6046-2016-0-11-5-5. URL: https://viam-works.ru/en/journal/2016/11/5
Keywords
cyanate ester oligomer, resin transfer molding (RTM).
Abstract

This article describes preparation of polycyanurate binder, processed by the method of resin transfer molding (RTM). By the methods of HPLC, IR spectroscopy and DSC analysis the reaction of cyclotrimerization cyanate ester resin in the temperature range of 130 to 150°C is studied. The optimum mode of heat treatment is found for cyanate ester oligomer allowed to implement almost 100% conversion of the functional groups to obtain heat-resistant polymer matrix with Tg≥250°C on the basis of the received results. Fiberglass and carbon plastics based on the binder have a high level of strength properties, both at room and at elevated temperatures. The work is executed within the implementation of the complex scientific direction 13.1. «Binding for polymer and composite materials of constructional and special purpose» («The strategic directions of development of materials and technologies of their processing for the period till 2030»)

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Mihajlin Yu.A. Konstrukcionnye polimernye kompozicionnye materialy [Constructional polymeric composite materials]. SPb.: Nauchnye osnovy i tehnologii, 2010. 822 s.
  3. Kablov E.N. Materialy i himicheskie tehnologii dlya aviacionnoj tehniki [Materials and chemical technologies for aviation engineering] // Vestnik Rossijskoj akademii nauk. 2012. T. 82. №6. S. 520–530.
  4. Muhametov R.R., Merkulova Yu.I., Chursova L.V. Termoreaktivnye polimernye svyazuyushhie s prognoziruemym urovnem reologicheskih i deformativnyh svojstv [Thermosetting polymeric binding with predicted level of rheological and deformativny properties] // Klei. Germetiki. Tehnologii. 2012. №5. S. 19–21.
  5. Muhametov R.R., Ahmadieva K.R., Kim M.A., Babin A.N. Rasplavnye svyazujushhie dlya perspektivnyh metodov izgotovleniya PKM novogo pokoleniya [Melt binding for perspective methods of production of PCM of new generation] // Aviacionnye materialy i tehnologii. 2012. №S. S. 260–265.
  6. Kablov E.N. Sovremennye materialy – osnova innovacionnoj modernizacii Rossii [Molten binding for perspective methods of manufacturing of PKM of new generation] // Metally Evrazii. 2012. №3. S.10–14.
  7. Dushin M.I., Muhametov R.R., Platonov A.A., Merkulova Yu.I. Issledovanie filtracionnyh harakteristik armiruyushhih napolnitelej i svyazuyushhih pri razrabotke tehnologii bezavtoklavnogo formovaniya polimernyh kompozicionnyh materialov [Study of filtration characteristics of reinforcing fillers and binders in the development of non-out-autoclave technology for polymer composite material] // Aviacionnye materialy i tehnologii. 2013. №2. S. 22–25.
  8. Hrulkov A.V., Dushin M.I., Popov Yu.O., Kogan D.I. Issledovaniya i razrabotka avtoklavnyh i bezavtoklavnyh tehnologij formovaniya PKM [Researches and development autoclave and out-of-autoclave technologies of formation of PCM] //Aviacionnye materialy i tehnologii. 2012. №S. S. 292–301.
  9. Beckwith S.W. Resin Infusion Technology: Part 3 – A Detailed Overview of RTM and VIP Infusion Processing Technologies // SAMPE Journal. 2007. V. 43. №4. Р. 66–70.
  10. Yung-Tin Cnen, C.W. Macosko. Kinetics and Rheology Characterization During Curing of Dicyanates // Journal of Applied Polymer Science. 1996. V. 62. P. 567–576.
  11. Muhametov R.R., Ahmadieva K.R., Chursova L.V., Kogan D.I. Novye polimernye svyazujushhie dlya perspektivnyh metodov izgotovleniya konstrukcionnyh voloknistyh PKM [New polymeric binding for perspective methods of manufacturing of constructional fibrous PCM] //Aviacionnye materialy i tehnologii. 2011. №2. S. 38–42.
  12. Kuznetsov A.A., Semenova G.K. Perspektivnye vysokotemperaturnye svyazuyushhie dlya polimernyh kompozicionnyh materialov [Perspective high-temperature binding for polymeric composite materials] // Rossijskij himicheskij zhurnal. 2009. T. LIII. №4. S. 86–96.
  13. Muhametov R.R., Shimkin A.A., Dolgova E.V., Merkulova Yu.I. Polifunkcional'nye cianovye efiry dlya izgotovleniya kompozicionnyh materialov [Multifunctional cyanic ethers for manufacturing of composite materials] // Zhurnal prikladnoj himii. 2014. T. 87. Vyp. 12. S. 1836–1840.
  14. Bershtejn V.A., Egorov V.M. Differencialnaya skaniruyushhaya kalorimetriya v fizikohimii polimerov [Differential scanning calorimetry in the physical chemistry of polymers]. L.: Himiya, 1990. 256 s.
  15. Godovskij Yu.K. Teplofizicheskie metody issledovaniya polimerov [Heatphysical methods of research of polymers]. M.: Himiya, 1976. 216 s.