Development and research of porous fiber metal materials for sound-absorbing elements and abradable seals of gas turbine engines

Farafonov D.P., Migunov V.P.
Farafonov D.P., Migunov V.P. Development and research of porous fiber metal materials for sound-absorbing elements and abradable seals of gas turbine engines // Proceedings of VIAM. 2016. No. 11. DOI: 10.18577/2307-6046-2016-0-11-2-2. URL: https://viam-works.ru/en/journal/2016/11/2
Keywords
metal fibers, porous fiber metal materials, abradable seals, sound-proof designs, heat resistance.
Abstract

In the article the main results of research of high-temperature materials developed by FSUE «VIAM» produced from the metal fibers intended for application as essentially new abraded seals of air-gas channel and sound-absorbing materials of gas turbine engines are presented. The work is executed within the implementation of the complex scientific directions: 9.7. «High-temperature deformable alloys and the composite materials strengthened by high-melting metal fibers and particles, abraded sealing materials» and 15.7. «Porous fiber metal materials for sound-proof designs» («The strategic directions of materials and technologies of their processing development for the period till 2030»)

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N. Strategicheskie napravleniya razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda [The strategic directions of development of materials and technologies of their processing for the period to 2030] // Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  3. Migunov V.P., Farafonov D.P. Issledovanie osnovnyh ekspluatacionnyh svojstv novogo klassa uplotnitelnyh materialov dlya protochnogo trakta GTD [Research of the main operational properties of new class of sealing materials for flowing path of GTE] // Aviacionnye materialy i tehnologii. 2011. №3. S. 15–20.
  4. Migunov V.P., Farafonov D.P., Degovets M.L., Stupina T.I. Uplotnitelnye materialy dlya protochnogo trakta GTD [Sealing materials for flowing path of GTE] // Aviacionnye materialy i tehnologii. 2012. №S. S. 94–97.
  5. Migunov V.P., Farafonov D.P., Degovec M.L. Istiraemyj uplotnitelnyj material na osnove volokon iz mednyh splavov [Abradable sealing material made of fibers from copper alloys] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №9. St. 04. Available at: http://viam-works.ru (accessed: March 30, 2016). DOI: 10.18577/2307-6046-2014-0-9-4-2.
  6. Farafonov D.P., Degovets M.L., Serov M.M. Issledovanie svojstv i tehnologicheskih parametrov polucheniya metallicheskih volokon dlya istiraemyh uplotnitelnyh materialov aviacionnyh GTD [The investigation of the properties and technological parameters producing metallic fibers for abradable sealing materials of aircraft GTE] //Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №7. St. 02 Available at: http://viam-works.ru (accessed: March 30, 2016). DOI: 10.18577/2307-6046-2014-0-7-2-2.
  7. Sobolev A.F., Ushakov V.G., Filippova R.D. Zvukopogloshchayushchie konstruktsii gomogennogo tipa dlya kanalov aviatsionnykh dvigateley [Sound-proof designs of homogeneous type for channels of aircraft engines] // Akusticheskiy zhurnal. 2009. T. 55. №6. S. 749–759.
  8. Khaletskiy Yu.D. Effektivnost kombinirovannykh glushiteley shuma aviatsionnykh dvigateley [Efficiency of the combined silencers of noise of aircraft engines] // Akusticheskiy zhurnal. 2012. T. 58. №4. S. 556–562.
  9. Sun F.G., Chen H.L., Wu J.H., Feng K. Sound absorbing characteristics of fibrous metal materials at high temperatures // Appl. Acoust. 2010. V. 711. P. 221–235.
  10. Smarsly W., Zheng N., Buchheim C.S., Nindel C., Silvestro C., Sporer D., Tuffs M., Schreiber K., Langlade-Bomba C., Andersen O., Goehler H., Simms N.J., McColvin G. Advanced High Temperature Turbine Seals Materials and Designs // Material Science Forum. 2005. V. 492–493.P. 21–26.
  11. Simms N.J., Norton J.F., McColvin G. Performance of candidate gas turbine abradeable seal materials in high temperature combustion atmospheres // Materials and Corrosion. 2005. V. 56. P. 765–777.
  12. Serov M.M., Borisov B.V. Poluchenie metallicheskikh volokon i poristykh materialov iz nikh metodom ekstraktsii visyashchey kapli rasplava [Receiving metal fibers and porous materials from them method of ekstraktsiya of hanging drop rasplava] // Tekhnologiya legkikh splavov. 2007. №3. C. 62–65.
  13. Bazyleva O.A., Arginbaeva E.G., Turenko E.Yu. Vysokotemperaturnye intermetallidnye splavy dlya detaley GTD [The high-temperature intermetallic alloys for parts of gas-turbine engines] // Aviacionnye materialy i tehnologii. 2013. №3. S. 26–31.
  14. Buntushkin V.P., Kablov E.N., Bazyleva O.A., Morozova G.I. Splavy na osnove alyuminidov nikelya [Alloys on the basis of nickel aluminides] // MiTOM. 1999. №1. S. 32–34.
  15. Kablov E.N., Solntsev S.S., Rozenenkova V.A., Mironova N.A. Sovremennye polifunktsionalnye vysokotemperaturnye pokrytiya dlya nikelevykh splavov, uplotnitelnykh metallicheskikh voloknistykh materialov i berillievykh splavov [Modern multifunctional high temperature coatings for nickel alloys, sealing metal fibrous materials and beryllium alloys] // Novosti materialovedeniya. Nauka i tekhnika: elektron. nauch.-tekhnich. zhurn. 2013. №1. St. 05. Available at: http://www.materialsnews.ru (accessed: March 30, 2016).
  16. Solntsev S.S., Rozenenkova V.A., Mironova N.A., Gavrilov S.V. Vysokotemperaturnye tonkoplenochnye pokrytiya dlya uplotnitelnyh materialov iz metallicheskih volokon [High-temperature thin-film coverings for sealing materials from metal fibers] // Aviacionnye materialy i tehnologii. 2012. №1. S. 30–36.
  17. Felten E.J. Use of Platinum and Rhodium to Improve Oxide Adherence on Ni–8Cr–6Al Alloys // Oxidation of Metals. 1976. V. 10. №l. P. 23–28.
  18. Allam I.M., Akuezue H.C., Whittle D.P. Influence of Small Pt Additions on Al2O3 Scale Adherence // Oxidation of Metals.1980. V. 14. №6. P. 517–530.
  19. Heidloff A.J., Tang Z., Zhang F., Gleeson B.C. A Сombined Mapping Process for the Development of Platinum-modified Ni-based Superalloys // JOM. 2010. V. 62. P. 48–53.
  20. Ballard D.L., Plichak А.L. The use of Precious-metal-modified Nickel-based Superalloys for Thin Gage Apllications // JOM. 2010. V. 62. P. 45–47.
  21. Amano T., Takezawa Y., Shiino A., Shishido T. Surface morphology of scale on FeCrAl (Pd, Pt, Y) alloys // Journal of alloys and Compounds. 2008. V. 452. Issue 1. P. 16–22.
  22. Amano T. High-temperature oxidation of FeCrAl (Y, Pt) alloys in oxygen-water vapour // Materials at high temperatures. 2011. V. 28. Issue 4. P. 342–348.
  23. Amano T. High-temperature oxidation resistance of Al2O3-forming heat-resisting alloys with noble metal and rare earth additions // Materials and Corrosion. 2011. V. 62. №7. P. 659–667.