Polymer composition on the basis of polydodecanolactam for 3D-printing technology by melted polymer string

Platonov M.M., Petrova G.N., Larionov S.A., Barbotko S.L.
Platonov M.M., Petrova G.N., Larionov S.A., Barbotko S.L. Polymer composition on the basis of polydodecanolactam for 3D-printing technology by melted polymer string // Proceedings of VIAM. 2016. No. 10. DOI: 10.18577/2307-6046-2016-0-10-9-9. URL: https://viam-works.ru/en/journal/2016/10/9
Keywords
polydodecanolactam, fused deposition modeling (FDM), decabromodiphenylether, 3D-printing, characteristics of fire safety.
Abstract

The results of research of the properties of thermoplastic polymer composition on the basis of polydodecanolactam (PA-12 polyamide) for creation of a new material with the lowered fire hazard for FDM of the additive technology are presented. On the basis of the spent researches it is shown that the composition on the basis of PA-12, comprising in its composition a halogenated flame retardant, possesses the viscosity comparable to materials used for 3D-printing, such as ABS plastic and Nylon-618 and also the improved characteristics of fire safety. The factual results can find application in the creation of functional products for aircraft interior by 3D--printing methods meeting the requirements of AP-25 on fire safety characteristics.

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N. Materialy i himicheskie tehnologii dlya aviacionnoj tehniki [Materials and chemical technologies for aviation engineering] // Vestnik Rossijskoj akademii nauk. 2012. T. 82. №6. S. 520–530.
  3. Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace materials science] // Vse materialy. Enciklopedicheskij spravochnik. 2008. № 3. S. 2–14.
  4. Kablov E.N. Tendencii i orientiry innovacionnogo razvitiya Rossii: sb. nauch.-inform. mater. 3-e izd. [Tendencies and reference points of innovative development of Russia: collection of scientific information materials 3rd ed.] M.: VIAM, 2015. 720 s.
  5. Normy letnoj godnosti samoletov transportnoj kategorii: AP-25: utv. Postanovleniem 28-j Sessii po aviacii i ispolzovaniyu vozdushnogo prostranstva 11.12.2008. 3-e izd. s popravkami 1–7 [Standards of the flight validity of airplanes of transport category: AP-25: are approved as the resolution of the 28th Session on aircraft and use of air space 12.11.2008. 3rd ed. with corrections 1-7.]. M.: Aviaizdat. 2014. 278 s.
  6. Petrova G.N., Rumyanceva T.V., Beyder E.Ya. Vliyanie modificiruyushhih dobavok na pozharobezopasnye svojstva i tehnologichnost polikarbonata [Influence of modifying additives on fireproof properties and technological effectiveness of polycarbonate] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №6. St. 06. Available at: http://www.viam-works.ru (accessed: June 15, 2016).
  7. Petrova G.N., Beider E.Ya., Perfilova D.N., Rumyantseva T.V. Pozharobezopasnye litevye termoplasty i termojelastoplastyv [Fire safety of injection molding thermoplastics and TPE materials] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №11. St. 02. Available at: http://www.viam-works.ru (accessed: June 15, 2016).
  8. Gryaznov V.I., Petrova G.N., Yurkov G.Yu., Buznik V.M. Smesevye termojelastoplasty so specialnymi svojstvami [Thermoplastic mixtures with special properties] // Aviacionnye materialy i tehnologii. 2014. №1. S. 25–29. DOI: 10.18577/2071-9140-2014-0-1-25-29.
  9. Barbotko S.L. Pozharobezopasnost aviacionnyh materialov [Fire safety of aviation materials] // Aviacionnye materialy i tehnologii. 2012. №S. S. 431–439.
  10. Barbotko S.L., Volnyj O.S., Kirienko O.A., Shurkova E.N. Osobennosti ispytanij aviacionnyh materialov na pozharoopasnost. Chast 1. Ispytaniya na goryuchest. Vliyanie tolshhiny obrazca na registriruemye harakteristiki [Features of tests of aviation materials on fire danger. Part 1. Tests for combustibility. Influence of thickness of sample on registered characteristics] // Pozharovzryvobezopasnost. 2015. №1. S. 40–49.
  11. Barbot'ko S.L., Volnyj O.S., Kirienko O.A., Shurkova E.N. Osobennosti ispytanij aviacionnyh materialov na pozharoopasnost. Chast 2. Ispytaniya na goryuchest – vliyanie prodolzhitel'nosti ekspozicii plamenem gorelki [Features of tests of aviation materials on fire danger. Part 2. Tests for combustibility – influence of duration of exposure by torch flame] // Pozharovzryvobezopasnost. 2015. №3. S. 13–24.
  12. Barbotko S.L., Volnyj O.S., Kirienko O.A., Shurkova E.N. Osobennosti ispytanij aviacionnyh materialov na pozharoopasnost. Chast 3. Ispytaniya na dymoobrazovanie – vliyanie tolshhiny monolitnogo obrazca polimernogo kompozicionnogo materiala [Features of tests of aviation materials on fire danger. Part 3. Tests on smoke emission – influence of thickness of monolithic sample of polymeric composite material] // Pozharovzryvobezopasnost. 2015. №4. S. 7–23.
  13. Huang S.H., Liu P., Mokasdar A., Hou L. Additive manufacturing and its societal impact: a literature review // Int. J. Adv. Manuf. Technol. 2013. Vol. 67. P. 1191–1203. DOI: 10.1007/s00170-012-4558-5.
  14. Bikas H., Stavropoulos P., Chryssolouris G. Additive manufacturing methods and modeling approaches: a critical review // Int. J. Adv. Manuf. Technol. 2016. Vol. 83. P. 389–405. DOI: 10.1007/s00170-015-7576-2.
  15. Novakova-Marcincinova L., Kuric I. Basic and Advanced Materials for Fused Deposition Modeling Rapid Prototyping Technology // Manuf. and Ind. Eng. 2012. No. 11 (1). P. 24–27.
  16. Hill N., Haghi M. Deposition direction-dependent failure criteria for fused deposition modeling polycarbonate // Rapid Prototyping Journal. 2014. No. 20/3. P. 221–227. DOI: 10.1108/RPJ-04-2013-0039.
  17. Masood S.H., Song W.Q. Development of new metal/polymer materials for rapid tooling using Fused deposition modeling // Materials and Design. 2004. Vol. 25. P. 587–594. DOI: 10.1016/j.matdes.2004.02.009.
  18. Croccolo D., De Agostinis M., Olmi G. Experimental characterization and analytical modelling of the mechanical behavior of fused deposition processed parts made of ABS-M30 // Computational Materials Science. 2013. Vol. 79. P. 506–518. DOI: 10.1016/j.commatsci.2013.06.041.
  19. Turner B., Strong R., Gold S. A review of melt extrusion additive manufacturing processes: I. Process design and modeling // Rapid Prototyping Journal. 2014. No. 20/3. P. 192–204. DOI: 10.1108/RPJ-01-2013-0012.
  20. Durgun I., Ertan R. Experimental investigation of FDM process for improvement of mechanical properties and production cost // Rapid Prototyping Journal. 2014. No. 20/3. P. 228–235. DOI: 10.1108/RPJ-10-2012-0091.
  21. Riddick J.C., Haile M.A., Wahlde R.V., Cole D.P., Bamiduro O., Johnson T.E. Fractographic analysis of tensile failure of acrylonitrile-butadiene-styrene fabricated by fused deposition modeling // Additive Manufacturing. 2016. Vol. 11. P. 49–59. DOI: 10.1016/j.addma.2016.03.007.
  22. Dul S., Fambri L., Pegoretti A. Fused deposition modelling with ABS–graphene nanocomposites // Composites: Part A. 2016. Vol. 85. Р. 181–191. DOI: 10.1016/j.compositesa.2016.03.013.
  23. Domingo-Espin M., Puigoriol-Forcada J. M., Garcia-Granada A.-A., Llumà J., Borros S., Reyes G. Mechanical property characterization and simulation of fused deposition modeling Polycarbonate parts // Materials & Design. 2015. Vol. 83. P. 670–677. DOI: 10.1016/j.matdes.2015.06.074.