The analysis of nanomodified prepreg shelf life by its reactivity at storage

Cherfas L.V., Gunyaeva A.G., Komarova O.A., Antyufeeva N.V.
Cherfas L.V., Gunyaeva A.G., Komarova O.A., Antyufeeva N.V. The analysis of nanomodified prepreg shelf life by its reactivity at storage // Proceedings of VIAM. 2016. No. 1. DOI: 10.18577/2307-6046-2016-0-1-99-106. URL: https://viam-works.ru/en/journal/2016/1/12
Abstract

The experiments have been performed to assess the influence of nano-additives (astralens and thermo-expanded graphite) on the shelf life of prepregs made on basis of carbon full-strength fabric and polycyanurate mortar binder at a room and lower temperatures in an industrial refrigerator. Differential Scanning Calorimetry (DSC) was chosen as a basis of the analysis. The experimental DSC curves with detailed description of a reokinetic behavior of the analyzed prepregs were obtained. The conclusions of the shelf life for the investigated nanomodified prepregs were presented according to the results of the analysis.

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  2. Kablov E.N. Rossii nuzhny materialy novogo pokoleniyya [Materials of new generation are necessary to Russia] // Redkie zemli. 2014. №3. S. 8–13.
  3. Kablov E.N., Gunyaev G.M. Nanomaterialy – proryv v materialovedenie mikromira [Nanomaterials – break in microcosm materials science] / V sb.: 75 let. Aviacionnye materialy. Izbrannye trudy «VIAM» 1932–2007: yubilejnyj nauch.-tehnich. sb. M.: VIAM, 2007. S. 225–232.
  4. Kablov E.N., Kondrashov S.V., Yurkov G.Yu. Perspektivy ispolzovaniya uglerodsoderzhashhih nanochastic v svyazuyushhih dlya polimernyh kompozicionnyh materialov [Perspectives of use of carbon-containing nanoparticles in binding for polymeric composite materials] // Rossijskie nanotehnologii. 2013. №3–4. S. 24–42.
  5. Aleksashin V.M., Gunyaev G.M., Kablov E.N., Ilchenko S.I., Ponomarev A.N. Perspektivy primenenija uglerodnyh nanomaterialov v aviacionnom mashinostroenii [Perspectives of application of carbon nanomaterials in aviation mechanical engineering] / V sb. dokl. 2-j Mezhdunar. konf. «Uglerod: fundamentalnye problemy nauki, materialovedenie, tehnologiya». 2003.
  6. Chursova L.V., Kim M.A., Panina N.N., Shvetsov E.P. Nanomodificirovannoe epoksidnoe svyazuyushhee dlya stroitelnoj industrii [Nanomodified epoxy binder for the construction industry] // Aviacionnye materialy i tehnologii. 2013. №1. S. 40–47.
  7. Bobovich B.B. Polimernye konstrukcionnye materialy (struktura, svojstva, primenenie) [Polymeric constructional materials (structure, properties, application)]. M.: FORUM INFRA-M, 2014. 400 s.
  8. Gunyaeva A.G. Nanomodificirovannye prepregi epoksidnyh ugleplastikov / V sb. tez. dokl. «Nauchnye trudy ХХХVIII Gagarinskih chtenij». M.: MATI, 2012. T.1. S. 28–30.
  9. Gunyaev G.M., Kablov E.N., Aleksashin V.M. Modificirovanie konstrukcionnyh ugleplastikov uglerodnymi nanochasticami [Modifying constructional ugleplastikov carbon nanoparticles ] // Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 5–11.
  10. Gunyaev G.M., Chursova L.V., Komarova O.A., Gunyaeva A.G. Konstrukcionnye ugleplastiki, modificirovannye nanochasticami [Constructional coal the plastics modified by nanoparticles] // Aviacionnye materialy i tehnologii. 2012. №S. S. 277–286.
  11. Babin A. N. Svyazujushhie dlya polimernyh kompozicionnyh materialov novogo pokoleniya [Binding for polymeric composite materials of new generation] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №4. St. 11. Available at: http://www.viam-works.ru (accessed: July 07, 2015).
  12. Kovalenko A.V. Issledovanie svojstv svyazujushhego dlya formovaniya izdelij metodom propitki pod davleniem [Study of resin properties for forming of articles by resin transfer molding] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №1. St. 06. Available at: http://www.viam-works.ru (accessed: July 07, 2015). DOI: 10.18577/2307-6046-2015-0-1-6-6.
  13. Kablov E.N., Startsev O.V., Krotov A.S., Kirillov V.N. Klimaticheskoe starenie kompozicionnyh materialov aviacionnogo naznacheniya. I. Mehanizmy stareniya [Climatic aging of composite materials of aviation assignment. I. Aging mechanisms] // Deformaciya i razrushenie materialov. 2010. №11. S. 19–27.
  14. Antyufeeva N.V., Komarova O.A., Pavlovskij K.A., Aleksashin V.M. Opyt primeneniya kalorimetricheskogo kontrolya reakcionnoj sposobnosti preprega KMU-11tr [Practice of the calorimetric control reactionary ability prepreg KMU-11tr] // Trudy VIAM VIAM: elektron. nauch.-tehnich. zhurn. 2014. №2. St. 06. Available at: http://www.viam-works.ru (accessed: July 07, 2015). DOI: 10.18577/2307-6046-2014-0-2-6-6.
  15. Aleksashin V.M., Aleksandrova L.B., Matveeva N.V., Mashinskaja G.P. Primenenie termicheskogo analiza dlya kontrolya tehnologicheskih svojstv termoreaktivnyh prepregov konstrukcionnyh kompozicionnyh materialov [Application of the thermal analysis for control of technological properties of thermosetting prepregs of constructional composite materials] // Aviacionnaya promyshlennost. 1997. №5–6. S. 38–43.