Effect of small addition of alloying elements with high with high solubility in aluminium on microstructure of ingots and cold-rolled sheets of Al–Mg–Sc alloy

Ryabov D.K., Vakhromov R.O., Ivanova A.O.
Ryabov D.K., Vakhromov R.O., Ivanova A.O. Effect of small addition of alloying elements with high with high solubility in aluminium on microstructure of ingots and cold-rolled sheets of Al–Mg–Sc alloy // Proceedings of VIAM. 2015. No. 9. DOI: 10.18577/2307-6046-2015-0-9-5-5. URL: https://viam-works.ru/en/journal/2015/9/5
Abstract

For advanced aerospace application it is necessary to develop aluminium alloys of new generation with improved service characteristics. For the purpose of increasing mechanical properties of Al–Mg alloys it is purposeful to add small amount of scandium, but small additives of alloying elements with high solubility also can influence microstructure and properties of semi-products. This study deals with effect of small additives of silver, zink and copper in amount not exceeding maximum solubility on microstructure of ingots and cold-rolled sheets of V-1579 type alloy and it’s mechanical properties

Reference list
  1. Kablov E.N. Sovremennye materialy – osnova innovacionnoj modernizacii Rossii [Modern materials – basis of innovative modernization of Russia] //Metally Evrazii. 2012. №3. S. 10–15.
  2. Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace materials science] //Vse materialy. Jenciklopedicheskij spravochnik. 2008. №3. S. 2–14.
  3. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitija materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative development of VIAM Federal State Unitary Enterprise of GNTs Russian Federation on implementation «The strategic directions of development of materials and technologies of their processing for the period till 2030»] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  4. Antipov V.V., Senatorova O.G., Tkachenko E.A., Vahromov R.O. Aljuminievye deformiruemye splavy [Aluminum deformable alloys] //Aviacionnye materialy i tehnologii. 2012. №S. S. 167–182.
  5. Kablov E.N., Lukin V.I., Zhegina I.P., Ioda E.N., Loskutov V.M. Osobennosti i perspektivy svarki aljuminijlitievyh splavov [Features and perspectives of welding of alyuminiylitiyevy alloys] /V sb. Aviacionnye materialy i tehnologii. Vyp. «Tehnologija proizvodstva aviacionnyh metallicheskih materialov». M.: VIAM. 2002. S. 3–12.
  6. Kablov E.N., Ospennikova O.G., Vershkov A.V. Redkie metally i redkozemel'nye jelementy – materialy sovremennyh i budushhih vysokih tehnologij [Rare metals and rare earth elements – materials of modern and future high technologies] //Trudy VIAM. 2013. №2. St. 01 (viam-works.ru).
  7. Rybin V.V., Andreev G.N., Barahtina N.N., Osokin E.P. Nekotorye aspekty sozdanija sovremennyh morskih vysokoprochnyh aljuminievyh splavov so skandiem [Some aspects of creation of modern sea high-strength aluminum alloys with scandium] //Voprosy materialovedenija. 2006. №1. S. 92–102.
  8. Zaharov V.V., Rostova T.D. Uprochnenie aljuminievyh splavov pri legirovanii ih skandiem [Hardening of aluminum alloys at alloying their scandium] //MiTOM. 2013. №12 (702). S. 24–29.
  9. Zaharov V.V. O sovmestnom legirovanii aljuminievyh splavov skandiem i cirkoniem [About joint alloying of aluminum alloys scandium and zirconium] //MiTOM. 2014. №6 (708). S. 3–8.
  10. Ana Alil, Miljana Popović, Tamara Radetić, Milorad Zrilić, Endre Romhanji. Influence of annealing temperature on the baking response and corrosion properties of an Al–4,6 wt% Mg alloy with 0,54 wt% Cu //Journal of Alloys and Compounds. 2015. V. 625. P. 76–84.
  11. Masahiro Kubota, Barry C. Muddle Effect of Trace Additions of Ag on Precipitation in Al–Mg Alloys //Materials Transactions. 2005. V. 46. №12. P. 2968–2974.
  12. Elagin V.I. Legirovanie deformirovannyh aljuminievyh splavov perehodnymi metallami [Alloying of the deformed aluminum alloys transition metals]. M.: Metallurgija. 1975. 321 s.
  13. Rjabov D.K., Kolobnev N.I., Samohvalov S.V., Mahsidov V.V. Vlijanie predvaritel'nogo estestvennogo starenija na svojstva splava 1913 v iskusstvenno sostarennom sostojanii [Influence of preliminary natural aging on properties of alloy 1913 in artificially made old condition] //Aviacionnye materialy i tehnologii. 2013. №2. S. 8–11.
  14. Rjabov D.K., Kolobnev N.I., Samohvalov S.V., Vahromov O.V. Izmenenie mehanicheskih i korrozionnyh svojstv splava 1913 pri iskusstvennom starenii [Change of mechanical and corrosion properties of alloy 1913 at artificial aging] //Voprosy materialovedenija. 2013. №4 (76). C. 24–29.
  15. Kolobnev N.I., Mahsidov V.V., Samohvalov S.V., Rjabov D.K. Vlijanie soderzhanija antirekristallizatorov na strukturu i svojstva listov iz splava 1370 sistemy Al–Mg–Si–Cu–Zn [Influence of the maintenance of antirekristallizator on structure and property of sheets from alloy of the 1370th system Al–Mg–Si–Cu–Zn] //Tehnologija legkih splavov. 2012. №1. S. 18–24.
  16. Rjabov D.K., Kolobnev N.I., Kochubej A.Ja., Zavodov A.V. Izmenenie mehanicheskih svojstv listov iz splava 1913 pri vvedenii skandija [Change of mechanical properties of sheets from alloy 1913 at scandium introduction] //Aviacionnye materialy i tehnologii. 2014. №4. S. 3–8.
  17. Gorelik S.S. Rekristallizacija metallov i splavov [Rekristallizatsiya of metals and alloys]. M.: Metallurgija. 1967. 405 s.
  18. Filatov Ju.A. Splavy sistemy Al–Mg–Sc kak osobaja gruppa deformiruemyh aljuminievyh splavov [Al–Mg–Sc system alloys as special group of deformable aluminum alloys] //Tehnologija legkih splavov. 2014. №2. S. 34–41.
  19. Ryabov D., Kolobnev N., Samohvalov S. Effect of scandium addition on mechanical properties and corrosion resistance of medium strength Al–Zn–Mg–(Cu) alloy //Materials Science Forum. 2014. V. 794–796. P. 241–246.