Structural features and properties of single-crystal Ni-based superalloy produced under conditions of variable temperature gradient on the solidification front
UDC
669.018.44:669.245
DOI
10.18577/2307-6046-2015-0-8-1-1
Article PDF (Russian)
(1.51 MB)
How to cite
Echin A.B., Bondarenko Yu.A. Structural features and properties of single-crystal Ni-based superalloy produced under conditions of variable temperature gradient on the solidification front // Proceedings of VIAM. 2015. No. 8. DOI: 10.18577/2307-6046-2015-0-8-1-1. URL: https://viam-works.ru/en/journal/2015/8/1
Abstract
Research of an influence of the directional crystallization conditions (temperature gradient and crystallization rate) on the dendrite arm spacing, size of strengthening γ'-phase in axes and interdendritic areas, porosity, size of eutectic γ /γ'-phase particles, features of segregation and mechanical properties of cast single-crystal superalloy is described in the article.
Reference list
- Litye lopatki gazoturbinnyh dvigatelej: splavy, tehnologii, pokrytija [Cast blades of gas turbine engines: alloys, technologies, coverings] /Pod obshh. red. E.N. Kablova. 2-e izd. M.: Nauka. 2006. 632 s.
- Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitija materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative development of VIAM Federal State Unitary Enterprise of GNTs Russian Federation on implementation «The strategic directions of development of materials and technologies of their processing for the period till 2030»] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
- Kablov E.N., Petrushin N.V., Svetlov I.L. Komp'juternoe konstruirovanie zharoprochnogo nikelevogo splava IV pokolenija dlja monokristallicheskih lopatok gazovyh turbin [Computer designing of heat resisting nickel alloy IV of generation for single-crystal blades of gas turbines] /V kn. Litejnye zharoprochnye splavy. Jeffekt S.T. Kishkina. M.: Nauka. 2006. S. 98–115.
- Kablov E.N., Petrushin N.V., Svetlov I.L., Demonis I.M. Nikelevye litejnye zharoprochnye splavy novogo pokolenija [Nickel foundry hot strength alloys of new generation] //Aviacionnye materialy i tehnologii. 2012. №S. S. 36–52.
- Versnyder F.F., Guard R.W. Directional Grain Structure for High Temperature Strength //Trans. ASM. 1960. V. 52. P. 485–493.
- Kurc V., Zam P.R. Napravlennaja kristallizacija jevtekticheskih materialov [The directed crystallization of evtektichesky materials]. M.: Metallurgija. 1980. 272 s.
- Bondarenko Ju.A., Kablov E.N., Morozova G.I. Vlijanie vysokogradientnoj napravlennoj kristallizacii na strukturu i fazovyj sostav zharoprochnogo splava tipa Rene N5 [Influence of the high-gradient directed crystallization on structure and phase composition of hot strength alloy of the Rene N5 type] //MiTOM. 1999. №2. S. 15–18.
- Bondarenko Ju.A., Kablov E.N. Napravlennaja kristallizacija zharoprochnyh splavov s povyshennym temperaturnym gradientom [The directed crystallization of hot strength alloys with the raised temperature gradient] //MiTOM. 2002. №7. S. 20–23.
- Echin A.B., Bondarenko Ju.A. Novaja promyshlennaja vysokogradientnaja ustanovka UVNS-6 dlja poluchenija lopatok i drugih detalej GTD iz litejnyh zharoprochnyh i intermetallidnyh splavov s monokristallicheskoj strukturoj [The new commercial UVNS-6 high-gradient unit for receiving blades and other details of GTD from cast heat resisting and intermetallidny alloys with single-crystal structure] //Aviacionnye materialy i tehnologii. 2014. №4. S. 31–36.
- Bondarenko Ju.A., Kablov E.N., Surova V.A., Echin A.B. Vlijanie vysokogradientnoj napravlennoj kristallizacii na strukturu i svojstva renijsoderzhashhego monokristallicheskogo splava [Influence of the high-gradient directed crystallization on structure and property of reniysoderzhashchy single-crystal alloy] //MiTOM. 2006. №8. S. 33–35.
- Kablov E.N., Bondarenko Ju.A., Kablov D.E. Osobennosti struktury i zharoprochnyh svojstv monokristallov 001> vysokorenievogo nikelevogo zharoprochnogo splava, poluchennogo v uslovijah vysokogradientnoj napravlennoj kristallizacii [Features of structure and heat resisting properties of monocrystals of 001> high-rhenium nickel hot strength alloys received in the conditions of high-gradient directed crystallization] //Aviacionnye materialy i tehnologii. 2011. №4. S. 25–31.
- Zharoprochnyj splav na osnove nikelja [Hot strength alloy on the basis of nickel]: pat. №2148099 Ros. Federacija; opubl. 18.01.99 Bjul. 2000. №12.
- Bondarenko Ju.A., Echin A.B., Surova V.A., Narskij A.R. Vlijanie temperaturnogo gradienta na fronte rosta na strukturu zharoprochnogo splava pri napravlennoj kristallizacii [Influence of temperature gradient at the front growth on hot strength alloy structure at the directed crystallization] //Litejshhik Rossii. 2014. №5. S. 24–27.