Regularities of formation microstructure, phase & chemical composition of pyrolytic chrome-carbide coatings

Panarin A.V., Ilyin V.A., Salakhova R.K., Smirnova T.B.
Panarin A.V., Ilyin V.A., Salakhova R.K., Smirnova T.B. Regularities of formation microstructure, phase & chemical composition of pyrolytic chrome-carbide coatings // Proceedings of VIAM. 2015. No. 7. DOI: 10.18577/2307-6046-2015-0-7-6-6. URL: https://viam-works.ru/en/journal/2015/7/6
Abstract

The work presents research results of microstructure deposited on aluminum casting alloys AL25 & AL26 pyrolytic chrome-carbide coating (PCCC). As an etchant was used Murakami’s reagent. Quantitative composition of selected etchant & modes of microsections etching optimized. Chrome-carbide coating's microstructure dependence from conditions of the deposition process showed. Chemical and phase compositions of PCCC identified.

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategi-cheskih napravlenij razvitija materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative development of VIAM Federal State Unitary Enterprise of GNTs Russian Federation on implementation «The strategic directions of development of materials and technologies of their processing for the period to 2030»] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  2. Kablov E.N., Starcev O.V., Medvedev I.M., Panin S.V. Korrozionnaja agressivnost' pri-morskoj atmosfery. Ch. 1. Faktory vlijanija (Obzor) [Corrosion aggression of the seaside atmosphere. P.1. Factors of influence (review)] //Korrozija: materialy, zashhita. 2013. №12. S. 6–18.
  3. Kablov E.N. Aviacionnoe materialovedenie XXI v veke. Perspektivy i zadachi [Aviation materials science of XXI in century. Perspectives and tasks] /V kn. Aviacionnye materialy. Izbrannye trudy «VIAM» 1932–2002: Jubilejnyj nauch.-tehnich. sb. M.: MISiS–VIAM. 2002. S. 23–47.
  4. Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace materials science] //Vse ma-terialy. Jenciklopedicheskij spravochnik. 2008. №3. S. 26.
  5. Shhetanov B.V., Balinova Ju.A., Ljuljukina G.Ju., Solov'eva E.P. Struktura i svojstva nepreryvnyh polikristallicheskih volokon α-Al2O3 [Structure and properties of continuous polycrystalline fibers α-Al2O3] //Aviacionnye materialy i tehnologii. 2012. №1. S. 13–17.
  6. Antipov V.V., Senatorova O.G., Tkachenko E.A., Vahromov R.O. Aljuminievye deform-iruemye splavy [Aluminum deformable alloys] //Aviacionnye materialy i tehnologii. 2012. №S. S. 167–182.
  7. Fridljander I.N., Sister V.G., Grushko O.E., Berstenev V.V., Sheveleva L.M., Ivanova L.A. Aljuminievye splavy – perspektivnyj material v avtomobilestroenii [Aluminum alloys – perspective material in automotive industry] //MiTOM. 2002. №9. S. 3–9.
  8. Lahtin Ju.V., Dushik V.V., Kuz'min V.P., Rozhanskij N.V. Nanostrukturirovannye tverdye pokrytija – kljuch k bezopasnosti jekspluatacii oborudovanija v jekstremal'nyh uslovijah [The nanostructured hard coatings – key to safety of operation of the equipment in extreme conditions] //Korrozija: materialy, zashhita. 2014. №3. S. 21–26.
  9. Gribov B.G., Domracheev G.A., Zhuk B.V. i dr. Osazhdenie plenok i pokrytij razlozheniem metalloorganicheskih soedinenij [Sedimentation of films and coverings decomposition of organometallic compounds]. M.: Nauka. 1981. 322 s.
  10. Panarin A.V., Il'in V.A. Aljuminirovanie konstrukcionnyh stalej metodom termicheskogo razlozhenija metalloorganicheskoj zhidkosti [Aluminizing constructional staly method of thermal decomposition of metalloorganic liquid] //Aviacionnye materialy i tehnologii. 2014. №1. S. 20–24.
  11. Sokolov V.F. i dr. Zashhitnoe piroliticheskoe hromovoe pokrytie. Tehnologija, svojstva, primenenie: Obzor [Protective pyrolitic chrome plating. Technology, properties, application: review]. M.: CNIIatominform. 1989. 72 s.
  12. Panarin A.V. Piroliticheskie karbidohromovye pokrytija. Tehnologija poluchenija i svoj-stva [Pyrolitic karbidokhromovy coverings. Technology of receiving and property] //Aviacionnye materialy i tehnologii. 2011. №4. S. 14–18.
  13. Kornysheva I.S., Volkova E.F., Goncharenko E.S., Muhina I.Ju. Perspektivy primenenija magnievyh i litejnyh aljuminievyh splavov [Perspectives of application of magnesium and cast aluminum alloys] //Aviacionnye materialy i tehnologii. 2012. №.S. S. 212–222.
  14. Panarin A.V. Piroliticheskie karbidohromovye pokrytija: poluchenie, svojstva i appara-turnoe obespechenie processa [Pyrolitic karbidokhromovy coverings: receiving, properties and hardware ensuring process] //Aviacionnye materialy i tehnologii. 2009. №2. S. 14–19.
  15. Kostenko V.A., Krasheninnikov V.N. Jekspluatacionnye svojstva piroliticheskih kar-bidohromovyh pokrytij [Operational properties of pyrolitic karbidokhromovy coverings] /V sb. Primenenie metalloorganicheskih soedinenij dlja poluchenija neorganicheskih pokrytij i materialov. M.: Nauka, 1986. S. 233–243.
  16. Mel'nikov V.V., Maksimov G.A., Kaverin B.S. i dr. Sostav i struktura pokrytij, osa-zhdennyh iz parovoj fazy pri term raspade bis-arenhromovyh kompleksov [Structure and structure of the coverings besieged from vapor phase at term disintegration encore-arenkhromovykh of complexes] //Dokladyꞌ AN SSSR. 1974. T. 219. №4. S. 929–931.