Methodological aspects of the phase morphology analysis in materials based on synthetic resins modified by thermoplastics (review)

Gulyaev A.I., Juravleva P.L.
Gulyaev A.I., Juravleva P.L. Methodological aspects of the phase morphology analysis in materials based on synthetic resins modified by thermoplastics (review) // Proceedings of VIAM. 2015. No. 6. DOI: 10.18577/2307-6046-2015-0-6-9-9. URL: https://viam-works.ru/en/journal/2015/6/9
Abstract

Modifying of synthetic resins with thermoplastics efficiently increases fracture toughness of polymer composite. Structurization in thermoset-thermoplastic blends is accompanied by reaction-induced micro-phase separation with forming of characteristic phase morphology. The current state of electron microscopy researches of phase morphology of thermoset-thermoplastic blends and composite materials on their basis is considered in this work. The following methodological problems of electron microscopy research of phase morphology are considered: information provided by research method, contrasting efficiency of characteristic elements of microstructure, justification of key morphological parameters choice and methods of their measurement

Reference list
  1. Solodilov V.I., Gorbatkina Ju.A. Svojstva odnonapravlennyh ugleplastikov na osnove jepoksidnoj smoly, modificirovannoj polisul'fonom ili jepoksiuretanovym oligomerom [Properties unidirectional ugleplastikov on the basis of the epoxy modified by polysulphone or epoksiuretanovy oligomer] //Mehanika kompozicionnyh materialov i konstrukcij. 2008. T. 14. №2. S. 217–227.
  2. Zheleznjak V.G., Chursova L.V. Modifikacija svjazujushhih i matric na ih osnove s cel'ju povyshenija vjazkosti razrushenija [Updating binding and matrixes on their basis for the purpose of fracture toughness increase] //Aviacionnye materialy i tehnologii. 2014. №1. S. 47–50.
  3. Erasov V.S., Nuzhnyj G.A., Grinevich A.V., Terehin A.L. Treshhinostojkost' aviacionnyh materialov v processe ispytanija na ustalost' [Treshchinostoykost of aviation materials in the course of fatigue test] //Trudy VIAM. 2013. №10. St. 06 (viam-works.ru)
  4. Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki na period do 2030 goda [The strategic directions of development of materials and technolo-gies of their processing for the period till 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  5. Kablov E.N. Himija v aviacionnom materialovedenii [Chemistry in aviation materials sci-ence] //Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 3–4.
  6. Kablov E.N. Shestoj tehnologicheskij uklad [Sixth technological way] //Nauka i zhizn'. 2010. №4. S. 2–7.
  7. Budylin N.Ju., Shapagin A.V., Chalyh A.E., Hasbiullin R.R. Modelirovanie formirovanija gradientnyh dispersnyh struktur v smesjah termo- i reaktoplastov [Modeling of forming of gradient disperse structures in mixes thermo- and thermosets] //Plasticheskie massy. 2011. №3. S. 51–56.
  8. Zhang Y. et al. Dynamically asymmetric phase separation and morphological structure for-mation in the epoxy/polysulfone blends //Macromolecules. 2011. V. 44. №18. P. 7465–7472.
  9. Liu Y. Polymerization-induced phase separation and resulting thermomechanical properties of thermosetting/reactive nonlinear polymer blends: a review //Journal of applied polymer science. 2013. V. 127. №5. P. 3279–3292.
  10. Kablov E.N., Kondrashov S.V., Jurkov G.Ju. Perspektivy ispol'zovanija uglerod-soderzhashhih nanochastic v svjazujushhih dlja polimernyh kompozicionnyh materialov [Perspectives of use of carbon-containing nanoparticles in binding for polymeric composite materials] //Rossijskie nanotehnologii. 2013. T. 8. №3–4. S. 24–42.
  11. Guljaev A.I. Issledovanie polimernyh materialov metodom rentgenovskoj fotojelektronnoj spektroskopii [Research of polymeric materials by method of x ray photoelectronic spec-troscopy] //Trudy VIAM. 2013. №7. St. 04 (viam-works.ru).
  12. Zhuravleva P.L., Zajcev D.V. Issledovanie struktury uglerodnyh volokon s primeneniem difrakcionnyh metodov [Research of structure of carbon fibers using diffraction methods] //Aviacionnye materialy i tehnologii. 2012. №S. S. 448–455.
  13. Guljaev A.I., Ishodzhanova I.V., Zhuravleva P.L. Primenenie metoda opticheskoj mikros-ko-pii dlja kolichestvennogo analiza struktury PKM [Application of method of optical microscopy for the quantitative analysis of structure of PKM] //Trudy VIAM. 2014. №7. St. 07 (viam-works.ru).
  14. Deev I.S., Kablov E.N., Kobec L.P., Chursova L.V. Issledovanie metodom skanirujushhej jelektronnoj mikroskopii deformacii mikrofazovoj struktury polimernyh matric pri me-hanicheskom nagruzhenii [Research by method of scanning electron microscopy of defor-mation of microphase structure of polymeric matrixes at mechanical loading] //Trudy VIAM. 2014. №7. St. 06 (viam-works.ru).
  15. Huang K. et al. Preparation of a light color cardanol-based curing agent and epoxy resin composite: Cure-induced phase separation and its effect on properties //Progress in organic coatings. 2012. V. 74. №1. P. 240–247.
  16. Zhang Y. et al. Ubiquitous nature of the three-layered structure formation in the asymmetric phase separation of the epoxythermoplastic blends //Polymer. 2012. V. 53. №2. P. 588–594.
  17. Mimura K. et al. Improvement of thermal and mechanical properties by control of mor-phologies in PES-modified epoxy resins //Polymer. 2000. V. 41. №12. P. 4451–4459.
  18. Mezhikovskij S.M., Irzhak V.I. Himicheskaja fizika otverzhdenija oligomerov [Chemical physics of curing of oligomers]. M.: Nauka. 2008. 269 s.
  19. Polimernye smesi. T. 1. Sistematika [Polymeric mixes. V. 1. Systematics]: Per. s angl. /Pod red. D.R. Pola, K.B. Baknella. SPb.: Nauchnye osnovy i tehnologii. 2009. 618 s.
  20. Williams R.J.J., Rozenberg B.A., Pascault J.P. Reaction-induced phase separation in modified thermosetting polymers //Advances in polymer science. 1997. V. 128. P. 95–156.
  21. Rozenberg B.A. Mikrofazovoe razdelenie v otverzhdajushhihsja mnogokomponentnyh polimer-oligomernyh sistemah [Microphase division in otverzhdayushchikhsya multicom-ponent polymer - oligomerous systems] //Rossijskij himicheskij zhurnal. 2001. T. XLV. №5–6. S. 23–31.
  22. Wilkinson S.P. et al. Effect of thermoplastic modifier variables on toughening a bis-maleimide matrix resin for high-performance composite materials //Polymer. 1993. V. 34. №4. P. 870–884.
  23. Zhang J. et al. Study on thermoplastic-modified multifunctional epoxies: Influence of heating rate on cure behaviour and phase separation //Composites Science and Technology. 2009. V. 69. №7–8. P. 1172–1179.
  24. Rico M. et al. Phase separation and morphology development in a thermoplastic-modified toughened epoxy //European Polymer Journal. 2012. V. 48. №10. P. 1660–1673.
  25. Cano L. et al. Morphological and mechanical study of nanostructured epoxy systems mod-ified with amphiphilic poly(ethylene oxide-b-propylene oxide-b-ethylene oxide)triblock copolymer //Polymer. 2014. V. 55. №3. P. 738–745.
  26. Cong H. et al. Formation of nanostructures in thermosets containing block copolymers: From self-assembly to reaction-induced microphase separation mechanism //Polymer. 2014. V. 55. №5. P. 1190–1201.
  27. Min H.S. et al. Fracture toughness of polysulfone/epoxy semi-IPN with morphology spec-trum //Polymer Bulletin. 1999. V. 42. №2. P. 221–227.
  28. Poncet S. et al. Monitoring phase separation and reaction advancement in situ in thermo-plastic/epoxy blends //Polymer. 1999. V. 40. №24. P. 6811–6820.
  29. Chalyh A.E., Aliev A.D., Rubcov A.E. Jelektronno-zondovyj mikroanaliz v issledovanii polimerov [The electronic and probe microanalysis in research of polymers]. M.: Nauka. 1990. 192 s.
  30. Chalyh A.E. i dr. Analiticheskaja jelektronnaja mikroskopija v issledovanii struktury priv-ityh polimerov [Analytical electron microscopy in research of structure of vaccinated polymers] //Vysokomolekuljarnye soedinenija. Ser. A. 2010. T. 52. №4. S. 653–658.
  31. Heitzmann M.T. et al. Microanalysis techniques for the investigation of interphases formed between thermoset and thermoplastic polymers: Scanning electron microscopy and energy dispersive x-ray analysis //Key Engineering Materials. 2011. №471–472. P. 309–314.
  32. Liao Y. et al. Reaction-induced phase decomposition of thermoset/thermoplastic blends investigated by energy filtering transmission electron microscopy //Polymer. 2007. V. 48. №13. P. 3749–3758.
  33. Mezzenga R. et al. Morphology build-up in dendritic hyperbranched polymer modified epoxy resin: modeling and characterization //Polymer. 2001. V. 42. №1. P. 305–317.
  34. Tribut L. et al. Rheological behavior of thermoset/thermoplastic blends during isothermal curing: Experiments and modeling //Polymer. 2007. V. 48. №22. P. 6639–6647.
  35. Fernandez-Francos X. et al. Novel thermosets based on DGEBA and hyperbranched pol-ymers modified with vinyl and epoxy end groups //Reactive & Functional Polymers. 2010. V. 70. №10. P. 798–806.
  36. Saltykov S.A. Stereometricheskaja metallografija [Stereometric metallography]. M.: Met-allurgija. 1976. 270 s.
  37. Kulkami A.S., Beaucage G. Reaction induced phase-separation controlled by molecular topology //Polymer. 2005. V. 46. №12. P. 4454–4464.
  38. Polimernye smesi. T. 2: Funkcional'nye svojstva [Polymeric mixes. V. 2: Functional properties]: Per. s angl. /Pod red. D.R. Pola, K.B. Baknella. SPb.: Nauchnye osnovy i tehnologii. 2009. 606 s.
  39. Pearson R.A., Yee A.F. Toughening mechanisms in thermoplastic-modified epoxies: 1. Modification using poly(phenylene oxide) //Polymer. 1993. V. 34. №17. P. 3658–3670.
  40. Turmel D.J.-P., Partridge I.K. Heterogeneous phase separation around fibres in epoxy/PEI blends and its effect on composite delamination resistance //Composites Science and Technology. 1997. V. 57. №8. P. 1001–1007.
  41. Varley R.J., Hodkin J.H. Effect of reinforcing fibres on the morphology of a toughened epoxy/amine system //Polymer. 1997. V. 38. №5. P. 1005–1009.
  42. Olmos D., Gonzalez-Benito J. Visualization of the morphology at the interphase of glass fibre reinforced epoxy-thermoplastic polymer composites //European Polymer Journal. 2007. V. 43. №4. P. 1487–1500.
  43. Zhang J. et al. Interphase study of thermoplastic modified epoxy matrix composites: Phase behavior around a single fibre influenced by heating rate and surface treatment //Composites: Part A. 2010. V. 41. №6. P. 787–794.