Materials for high-temperature sealants (review)

Ivakhnenko Yu.A., Varrik N.M.
Ivakhnenko Yu.A., Varrik N.M. Materials for high-temperature sealants (review) // Proceedings of VIAM. 2015. No. 6. DOI: 10.18577/2307-6046-2015-0-6-2-2. URL: https://viam-works.ru/en/journal/2015/6/2
Abstract

Materials for high-temperature sealants are reviewed in the article. High-temperature movable sealants with acceptable wear resistance, chemical resistance in aggressive envi-ronment and high elastic properties are uses for sealing of flap doors and hatches and control means of flying vehicles. Generally, butt end sealants and/or stuffing box sealants are used as movable sealants. A wide range of organic, metal, ceramic and combined ma-terials can be used as sealing materials; their choice depends on service conditions.

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitija materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative development of VIAM Federal State Unitary Enterprise of GNTs Russian Federation on implementation «The strategic directions of development of materials and technologies of their processing for the period till 2030»] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  2. Krenkel W., Lamon J. High-Temperature Ceramic Materials and Composites /In: 7-th International Conference on High-Temperature Ceramic Matrix Composites (HT-CMC 7). Bayreuth. 2010. P. 938.
  3. Grashchenkov D.V., Balinova Yu.A., Tinyakova E.V. Aluminum Oxide Ceramic Fibers and Materials Based on them //Glass and Ceramics. 2012. V. 69. №3–4. P. 130–133.
  4. Kablov E.N., Shhetanov B.V., Ivahnenko Ju.A., Balinova Ju.A. Perspektivnye armirujushhie vysokotemperaturnye volokna dlja metallicheskih i keramicheskih kompozicionnyh materialov [Perspective reinforcing high-temperature fibers for metal and ceramic compo-site materials] //Trudy VIAM. 2013. №2. St. 05 (viam-works.ru).
  5. Shhetanov B.V., Balinova Ju.A., Ljuljukina G.Ju., Solov'eva E.P. Struktura i svojstva nepreryvnyh polikristallicheskih volokon α-Al2O3 [Structure and properties of continuous polycrystalline fibers α-Al2O3] //Aviacionnye materialy i tehnologii. 2012. №1. S. 13–17.
  6. Shhetanov B.V., Ivahnenko Ju.A., Babashov V.G. Teplozashhitnye materialy [Heat-protective materials] //Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 12–19.
  7. Ivahnenko Ju.A., Babashov V.G., Zimichev A.M., Tinjakova E.V. Vysokotemperaturnye teploizoljacionnye i teplozashhitnye materialy na osnove tugoplavkih soedinenij [High-temperature heatinsulating and heat-protective materials on the basis of high-melting connections] //Aviacionnye materialy i tehnologii. 2012. №S. S. 380–386.
  8. Babashov V.G., Ivahnenko Ju.A., Judin A.V., Zimichev A.M. Keramicheskij material dlja detalej ustanovok nepreryvnoj razlivki cvetnyh splavov [Ceramic material for details of installations of continuous razlivka of color alloys] //Trudy VIAM. 2014. №12. St. 05 (viam-works.ru).
  9. Zimichev A.M., Varrik N.M. K voprosu primenenija diskretnyh volokon iz tugoplavkih oksidov dlja formirovanija serdechnika termostojkih uplotnitel'nyh shnurov [To question of application of discrete fibers from high-melting oxides for forming of the core of heat-resistant sealing cords] //Trudy VIAM. 2015. №2. St. 07 (viam-works.ru).
  10. Maksimov V.G., Basargin O.V., Shheglova T.M., Nikitina V.Ju. O projavlenii sverhplastichnosti v polidispersnoj keramike mullit–oksid cirkonija s razmerom kristallov bolee 10 mkm [About superplasticity manifestation in unequigranular ceramics mullit-zirconium oxide with size of crystals more than 10 microns] //Trudy VIAM. 2013. №6. St. 04 (viam-works.ru).
  11. Tonkoslojnoe keramicheskoe pokrytie, sposob ego poluchenija, poverhnost' trenija na osnove tonkoslojnogo keramicheskogo pokrytija i sposob ee poluchenija [Tonkosloynoye ce-ramic coating, way of its receiving, friction surface on the basis of tonkosloyny ceramic coating and way of its receiving]: pat. №2165484 Ros. Federacija; opubl. 20.04.2001.
  12. Tonkoslojnoe keramicheskoe pokrytie, sposob ego poluchenija, poverhnost' trenija na osnove tonkoslojnogo keramicheskogo pokrytija i sposob ee poluchenija [Tonkosloynoye ceramic coating, way of its receiving, friction surface on the basis of tonkosloyny ceramic coating and way of its receiving]: pat. №2453640 Ros. Federacija; opubl. 20.10.2011.
  13. Torcevoe uplotnenie vrashhajushhegosja vala [Face seal of rotating shaft]: pat. №2168086 Ros. Federacija; opubl. 27.05.2001.
  14. Varrik N.M., Ivahnenko Ju.A., Maksimov V.G. Oksid-oksidnye kompozicionnye materialy dlja gazoturbinnyh dvigatelej (obzor) [Oksid-oksidnye composite materials for gas turbine engines (review)] //Trudy VIAM. 2014. №8. St. 03 (viam-works.ru).
  15. Zimichev A.M., Varrik N.M., Shheglova T.M., Nikitina V.Ju. Issledovanie prochnostnyh svojstv rovinga iz volokon sostava 85%Al2O3–15%SiO2 pri temperature 1000°С [Research of strength properties of roving from structure fibers 85%Al2O3–15%SiO2 at temperature 1000°С] //Vse materialy. Jenciklopedicheskij spravochnik s Prilozheniem «Kommentarii k standartam, TU, sertifikatam». 2015. №1. S. 30–35.
  16. Butakov V.V., Basargin O.V., Babashov V.G., Ivahnenko Ju.A. Model' povedenija voloknistogo materiala pri izgibe [Model of behavior of fibrous material at bend] //Trudy VIAM. 2014. №12. St. 06 (viam-works.ru).
  17. http://sealing.su/
  18. http://uplotnenia.ru
  19. http://garlock.kz/services/catalog/
  20. www.pgn.su
  21. http://technomixcenter.by/
  22. http://www.seals.highexpert.ru/materials.html
  23. http://chemindtec.ru/catalogue/2/29/
  24. Kablov E.N., Grashhenkov D.V., Isaeva N.V., Solncev S.S., Sevast'janov V.G. Vysokotemperaturnye konstrukcionnye kompozicionnye materialy na osnove stekla i keramiki dlja perspektivnyh izdelij aviacionnoj tehniki [High-temperature constructional composite materials on the basis of glass and ceramics for perspective products of aviation engineering] //Steklo i keramika. 2012. №4. S. 7–11.
  25. Kablov E.N., Grashhenkov D.V., Isaeva N.V., Solncev S.S., Sevast'janov V.G. Perspektivnye vysokotemperaturnye keramicheskie kompozicionnye materialy [Perspective high-temperature ceramic composite materials] //Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 20–24.