Reactive magnetron deposition of ITO coating on the polymer film using a sectionalized gas feed system

Khokhlov Y.A., Bogatov V.A., Berezin N.M., Krynin A.G.
Khokhlov Y.A., Bogatov V.A., Berezin N.M., Krynin A.G. Reactive magnetron deposition of ITO coating on the polymer film using a sectionalized gas feed system // Proceedings of VIAM. 2015. No. 5. DOI: 10.18577/2307-6046-2015-0-5-7-7. URL: https://viam-works.ru/en/journal/2015/5/7
Abstract

The distribution of thickness and properties (transmission coefficient, surface resistance) of an ITO coating fabricated by the reactive magnetron deposition on a polymer film using a sectionalized reactive gas feed system was investigated. It was shown that the uniformity of coating thickness and properties can be enhanced by optimizing the oxygen flow rate through different sections of the gas feed system.

Reference list
  1. Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki na period do 2030 goda [The strategic directions of development of materials and technologies of their processing for the period till 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  2. Kablov E.N. Materialy i himicheskie tehnologii dlja aviacionnoj tehniki [Materials and chemical technologies for aviation engineering] //Vestnik Ros-sijskoj akademii nauk. 2012. T. 82. №6. S. 520–530.
  3. Kablov E.N. Shestoj tehnologicheskij uklad [Sixth technological way] //Nauka i zhizn'. 2010. №4. S. 2–7.
  4. Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace materials science] //Vse materialy. Jenciklopedicheskij spravochnik. 2008. №3. S. 2–14.
  5. Kablov E.N. Aviacionnoe materialovedenie v XXI veke. Perspektivy i zadachi [Aviation materials science in the XXI century. Perspectives and tasks] /V kn. Aviacionnye materialy. Izbrannye trudy «VIAM» 1932–2002. M.: MISiS–VIAM. 2002. S. 23–47.
  6. Davydova I.F., Kablov E.N., Kavun N.S. Termostojkie negopjuchie poliimidnye steklotekstolity dlja izdelij aviacionnoj i paketnoj tehniki [Heat-resistant nonflammable polyimide glass fiber laminate for products of aviation and rocket engineering] //Vse materialy. Jenciklopedicheskij spravochnik. 2009. №7. S. 2–11.
  7. Bogatov V.A., Kondrashov S.V., Hohlov Ju.A. Mnogofunkcional'nye opticheskie pokrytija i materialy [Multifunction optical coatings and materials] //Aviacionnye materialy i tehnologii. 2012. №S. S. 343–348.
  8. Kisljakov P.P., Hohlov Ju.A., Krynin A.G., Kondrashov S.V. Poluchenie i primenenie polimernoj plenki s prozrachnym jelektroprovodjashhim pokrytiem na osnove oksida indija, legirovannogo olovom [Receiving and application of polymer film with transparent electroconducting coating on the basis of the indium oxide alloyed by tin] //Trudy VIAM. 2013. №11. St. 06 (viam-works.ru).
  9. Krynin A.G., Hohlov Ju.A., Bogatov V.A., Kisljakov P.P. Prozrachnye interferencionnye pokrytija dlja funkcional'nyh materialov osteklenija [Transparent interferential coatings for functional materials of glazing] //Trudy VIAM. 2013. №11. St. 05 (viam-works.ru).
  10. Bogatov V.A., Hohlov Ju.A. Mnogofunkcional'nye opticheskie pokrytija, poluchaemye metodami plazmennoj tehnologii, i sposoby kontrolja ih optiko-fizicheskih harakteristik [The multifunction optical coatings received by methods of plasma technology, and ways of control of their optiko-physical characteristics] /V sb. Aviacionnye materialy i tehnologii. Vyp. «Metody ispytanij i kontrolja kachestva metallicheskih i nemetallicheskih materialov». M.: VIAM. 2001. S. 93–99.
  11. Kuz'michev A.I. Magnetronnye raspylitel'nye sistemy. Kn. 1. Vvedenie v fiziku i tehniku magnetronnogo raspylenija [Magnetronnye spraying systems. Book 1. Introduction in physics and equipment of magnetron sputtering]. K.: Avers. 2008. 244 s.
  12. Komlev A.E., Shapovalov V.I., Shutova N.S. Magnetronnyj razrjad v srede argona i kisloroda pri osazhdenii plenki oksida titana [Magnetronny discharge in the environment of argon and oxygen at titanium oxide film deposition] //ZhTF. 2012. T. 82. №7. S. 134–136.
  13. Bogatov V.A., Kondrashov S.V., Hohlov Ju.A. Poluchenie gradientnogo pokrytija oksinitrida aljuminija metodom reaktivnogo magnetronnogo raspylenija [Receiving gradient covering oksinitrida aluminum method of reactive magnetron sputtering] //Aviacionnye materialy i tehnologii. 2010. №3. S. 19–21.
  14. Kurdesau F., Khripunov G., da Cunha A.F. et al. Comparative study of ITO layers deposited by DC and RF magnetron sputtering at room temperature //Journal of Non-Crystalline Solids. 2006. V. 352. №19–20. P. 1466–1470.
  15. Marchenko V.A. Processy na poverhnosti misheni pri reaktivnom raspylenii V v Ar–O2 sredah [Processes on target surface at reactive spraying of V in Ar–O2 Wednesdays] //Izvestija RAN. Serija fizicheskaja. 2009. T. 73. №7. S. 920–923.
  16. Hohlov Ju.A., Krynin A.G., Bogatov V.A., Kisljakov P.P. Opticheskie konstanty tonkih plenok oksida indija, legirovannogo olovom, osazhdennyh na polijetilentereftalatnuju plenku metodom reaktivnogo magnetronnogo raspylenija (blizhnjaja infrakrasnaja oblast' spektra) [Optical constants of thin films of the indium oxide alloyed by tin, besieged on polietilentereftalatny film method of reactive magnetron sputtering (near infrared region of range)] //Aviacionnye materialy i tehnologii. 2013. №1. S. 24–28.
  17. Hohlov Ju.A., Bogatov V.A., Berezin N.M. Stabilizacija reaktivnogo magnetronnogo osazhdenija magnitnym polem [Stabilization of reactive magnetronny sedimentation by magnetic field] //Fizika i himija obrabotki materialov. 2012. №5. S. 46–50.
  18. Hohlov Ju.A., Berezin N.M., Bogatov V.A., Krynin A.G. Reaktivnoe magnetronnoe osa-zhdenie oksida indija, legirovannogo olovom, s kontrolem rabochego davlenija [Reactive magnetronny sedimentation of the indium oxide alloyed by tin, with control of working pressure] //Aviacionnye materialy i tehnologii. 2015 (v pechati).
  19. Hohlov Ju.A., Berezin N.M., Bogatov V.A., Krynin A.G. Kontrol' reaktivnogo osazhdenija ITO pokrytija po jemissionnomu spektru plazmy magnetronnogo razrjada [Control of reactive sedimentation of ITO of covering on emission spectrum of plasma of magnetronny discharge] //Aviacionnye materialy i tehnologii. 2015 (v pechati).
  20. Hohlov Ju.A., Bogatov V.A., Krynin A.G. Vlijanie raspredelenija magnitnogo polja na svojstva ITO pokrytija, poluchaemogo na polimernoj plenke metodom reaktivnogo magnetronnogo osazhdenija [Influence of distribution of magnetic field on ITO properties of the covering received on polymer film by method of reactive magnetronny sedimentation] //Trudy VIAM. 2014. №12. St. 11 (viam-works.ru).
  21. Bogatov V.A., Hohlov Ju.A., Sytyj Ju.V., Zhadova N.S. Vlijanie obrabotki v razrjade s za-mknutym drejfom jelektronov na adgezionnye svojstva i prochnost' kleevyh soedinenij polimerov [Processing influence in discharge with the closed drift of electrons on adhesive properties and durability of glued joints of polymers] //Klei. Germetiki. Tehnologii. 2011. №9. S. 27–31.
  22. Krylova T.N. Interferencionnye pokrytija [Interferential coverings]. L.: Mashinostroenie. 1973. 224 s.
  23. Krynin A.G., Hohlov Ju.A. Opticheskie harakteristiki termostabilizirovannoj polijetilen-tereftalatnoj plenki, ispol'zuemoj dlja funkcional'nyh materialov osteklenija [Optical characteristics of the thermostabilized polietilentereftalatny film used for functional materials of glazing] //Aviacionnye materialy i tehnologii. 2013. №4. S. 31–34.
  24. Tehnologija tonkih plenok [Technology of thin films] /Pod red. L. Majssela, R. Glenga. M.: Sovetskoe radio. 1977. S. 305–344.