Choosing ceramic materials for thermal barrier coating of GTE turbine blades on working temperatures up to 1400°С

Chubarov D.A., Budinovskiy S.A.
Chubarov D.A., Budinovskiy S.A. Choosing ceramic materials for thermal barrier coating of GTE turbine blades on working temperatures up to 1400°С // Proceedings of VIAM. 2015. No. 4. DOI: 10.18577/2307-6046-2015-0-4-7-7. URL: https://viam-works.ru/en/journal/2015/4/7
Keywords
YSZ
Abstract

The article considers advantages and disadvantages of currently used ZrO2–(7–8)%Y2O3 (yttrium-stabilized zirconia – YSZ) ceramic layer, widely used now in serial coatings to protect turbine blades of gas turbine engines. The systems and some properties of new ceramic materials based on zirconium oxide with the addition of one or more rare earth elements which are currently being developed abroad are represented. The ceramic layers developed by VIAM brought on by magnetron midrange targets sputtering based on zirconium alloys with rare earth metals with following plasma chemical ceramics deposition in the argon oxygen environment are shown. The microstructure of the surface of the deposited layers, thermal conductivity and the prospects of their use in the development of a new thermal barrier coating (TBC) generation are investigated.

Reference list
  1. Budinovskij S.A., Mubojadzhjan S.A., Gajamov A.M. Sovremennoe sostojanie i osnovnye tendencii razvitija vysokotemperaturnyh teplozashhitnyh pokrytij dlja rabochih lopatok turbin aviacionnyh GTD [Current state and the main tendencies of development of high-temperature heat-protective coverings for working blades of turbines of aviation GTD] //Aviacionnaja promyshlennost'. 2008. №4. S. 33–37.
  2. Kuznecov V.P., Lesnikov V.P., Konakova I.P. i dr. Struktura i fazovyj sostav monokristallicheskogo splava VZhM4 s gazocirkuljacionnym zashhitnym pokrytiem [Structure and phase composition of VZhM4 single-crystal alloy with gazotsirkulyatsionny protecting cover] //MiTOM. 2011. №3. S. 28–32.
  3. Kos'min A.A., Budinovskij S.A., Mubojadzhjan S.A., Bulavinceva E.E. Zharostojkoe pokrytie dlja novogo perspektivnogo intermetallidnogo splava VIN3 [Heat resisting covering for new perspective intermetallidny alloy of VIN3] //Svarochnoe proizvodstvo. 2013. №6. S. 35–37.
  4. Budinovskij S.A., Kablov E.N., Mubojadzhjan S.A. Primenenie analiticheskoj modeli opredelenija uprugih naprjazhenij v mnogoslojnoj sisteme pri reshenii zadach po sozdaniju vysokotemperaturnyh zharostojkih pokrytij dlja rabochih lopatok aviacionnyh turbin [Application of analytical model of determination of elastic stresses in multi-layer system at the solution of tasks on creation of high-temperature heat resisting coverings for working blades of aviation turbines] //Vestnik MGTU im. N.Je. Baumana. Ser. «Mashinostroenie». 2011. №SP2. S. 26–37.
  5. Kablov E.N., Ospennikova O.G., Bazyleva O.A. Materialy dlja vysokoteplonagruzhennyh detalej gazoturbinnyh dvigatelej [Materials for the high-heatloaded details of gas turbine engines] //Vestnik MGTU im. N.Je. Baumana. Ser. «Mashinostroenie». 2011. №SP2. S. 13–19.
  6. Kablov E.N., Mubojadzhjan S.A. Ionnoe travlenie i modificirovanie poverhnosti otvetstvennyh detalej mashin v vakuumno-dugovoj plazme [Ion etching and modifying of surface of responsible details of machines in vacuum and arc plasma] //Vestnik MGTU im. N.Je. Baumana. Ser. «Mashinostroenie». 2011. №SP2. S. 149–163.
  7. Kablov E.N., Mubojadzhjan S.A., Budinovskij S.A., Pomelov Ja.A. Ionno-plazmennye zashhitnye pokrytija dlja lopatok gazoturbinnyh dvigatelej [Ion-plasma protecting covers for blades of gas turbine engines] //Konversija v mashinostroenii. 1999. №2. S. 42–47.
  8. Muboyadzhyan S.A., Kablov E.N. Vacuum plasma technique of protective coatings production of complex alloys//MiTOM. 1995. №2. S. 15–18.
  9. Kablov E.N., Ospennikova O.G., Vershkov A.V. Redkie metally i redkozemel'nye jelementy – materialy sovremennyh i budushhih vysokih tehnologij [Rare metals and rare earth elements – materials of modern and future high technologies] //Trudy VIAM. 2013. №2. St. 01 (viam-works.ru).
  10. Matveev P.V., Budinovskij S.A., Mubojadzhjan S.A., Kos'min A.A. Zashhitnye zharostojkie pokrytija dlja splavov na osnove intermetallidov nikelja [Protective heat resisting coverings for alloys on the basis of nickel intermetallic compound] //Aviacionnye materialy i teh-nologii. 2013. №2. S. 12–15.
  11. Budinovskij S.A., Mubojadzhjan S.A., Gajamov A.M., Matveev P.V. Razrabotka ionno-plazmennyh zharostojkih metallicheskih sloev teplozashhitnyh pokrytij dlja ohlazhdaemyh rabochih lopatok turbin [Development of ion-plasma heat resisting metal layers of heat-protective coverings for cooled working blades of turbines] //MiTOM. 2013. №11. S. 16–21.
  12. Budinovskij S.A., Mubojadzhjan S.A., Gajamov A.M., Stepanova S.V. Ionno-plazmennye zharostojkie pokrytija s kompozicionnym bar'ernym sloem dlja zashhity ot okislenija splava ZhS36-VI [Ion-plasma heat resisting coverings with composition barrier layer for protection against oxidation of alloy ZhS36-VI] //MiTOM. 2011. №1. S. 34–40.
  13. Kablov E.N., Mubojadzhjan S.A., Budinovskij S.A., Lucenko A.N. Ionno-plazmennye zashhitnye pokrytija dlja lopatok gazoturbinnyh dvigatelej [Ion-plasma protecting covers for blades of gas turbine engines] //Metally. 2007. №5. S. 23–34.
  14. Gajamov A.M., Budinovskij S.A., Mubojadzhjan S.A., Kos'min A.A. Vybor zharostojkogo po-krytija dlja zharoprochnogo nikelevogo renij-rutenijsoderzhashhego splava marki VZhM4 [Choice of heat resisting covering for heat resisting nickel reny-ruteniysoderzhashchy alloy of the VZhM4 brand] //Trudy VIAM. 2014. №1. St. 01 (viam-works.ru).
  15. Budinovskij S.A. Primenenie analiticheskoj modeli opredelenija uprugih mehanicheskih i termicheskih naprjazhenij v mnogoslojnoj sisteme v reshenii zadach po sozdaniju zharostojkih aljuminidnyh pokrytij [Application of analytical model of determination of elastic mechanical and thermal stresses in multi-layer system in the solution of tasks on creation of heat resisting alyuminidny coverings] //Uprochnjajushhie tehnologii i pokrytija. 2013. №3. S. 3–11.
  16. Mubojadzhjan S.A., Budinovskij S.A., Gajamov A.M., Matveev P.V. Vysokotemperaturnye zharostojkie pokrytija i zharostojkie sloi dlja teplozashhitnyh pokrytij [High-temperature heat resisting coverings and heat resisting layers for heat-protective coverings] //Aviacionnye materialy i tehnologii. 2013. №1. S. 17–20.
  17. Chubarov D.A., Matveev P.V. Novye keramicheskie materialy dlja teplozashhitnyh pokrytij rabochih lopatok GTD [New ceramic materials for heat-protective coverings of working blades of GTD] //Aviacionnye materialy i tehnologii. 2013. №4. S. 43–46.
  18. Tsipas Sofia. Thermophysical properties of Plasma Sprayed thermal Barrier Coatings. University of Cambridge. 2005. P. 1–25.
  19. Levi C.G. Emerging materials and processes for thermal barrier systems //Current Opinion in Solid State and Materials Science. 2004. №8. P. 77–91.
  20. Clarke D.R., Phillpot S.R. Thermal barrier coating materials //Materialstoday. 2005. V. 8. №6. P. 22–29.
  21. Narottam P. Bansal, Dongming Zhu, Maryam Eslamloo-Grami. Effects of Doping on Thermal Conductivity of Pyrochlore Oxides for Advanced Thermal Barrier Coatings, NASA/TM–2006-214483.
  22. Kablov E.N., Mubojadzhjan S.A. Teplozashhitnye pokrytija dlja lopatok turbiny vysokogo davlenija perspektivnyh GTD [Heat-protective coverings for turbine blades of high pressure of perspective GTD] //Metally. 2012. №1. S. 5–13.
  23. Kablov E.N., Mubojadzhjan S.A. Zharostojkie i teplozashhitnye pokrytija dlja lopatok turbiny vysokogo davlenija perspektivnyh GTD [Heat resisting and heat-protective coverings for turbine blades of high pressure of perspective GTD] //Aviacionnye materialy i tehnologii. 2012. №S. S. 60–70.
  24. Mubojadzhjan S.A., Budinovskij S.A., Gajamov A.M., Smirnov A.A. Poluchenie keramich-eskih teplozashhitnyh pokrytij dlja rabochih lopatok turbin aviacionnyh GTD magnetronnym metodom [Receiving ceramic heat-protective coatings for working blades of turbines of aviation GTD magnetronny method] //Aviacionnye materialy i tehnologii. 2012. №4. S. 3–8.