Environmental effects on properties of CFRP manufactured by RTM method

Voinov S.I., Zhelezina G.F., Solovjova N.A., Yamshchikova G.A., Timoshina L.N.
Voinov S.I., Zhelezina G.F., Solovjova N.A., Yamshchikova G.A., Timoshina L.N. Environmental effects on properties of CFRP manufactured by RTM method // Proceedings of VIAM. 2015. No. 2. DOI: 10.18577/2307-6046-2015-0-2-7-7. URL: https://viam-works.ru/en/journal/2015/2/7
Abstract

An influence of climatic factors and working fluids on properties of CFRP VKU-35 manufactured by RTM technology was studied. It was shown that CFRP VKU-35 has a high stability of properties under an influence of environmental factors (at least 75% of the initial value) and in this respect is not worse than the typical structural CFRP KMU-11tr manufactured by autoclave molding.

Reference list
  1. Kablov E.N. Sovremennye materialy – osnova innovacionnoj modernizacii Rossii [Modern materials – the basis of innovative modernization of Russia] //Metally Evrazii. 2012. №3. S. 10–15.
  2. Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki na period do 2030 goda [Strategic directions of development of materials and technologies to process them for the period up to 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  3. Gunjaev G.M., Krivonos V.V., Rumjancev A.F., Zhelezina G.F. Polimernye kompozicionnye materialy v konstrukcijah letatel'nyh apparatov [Polymer composite materials in aircraft structure] //Konversija v mashinostroenii. 2004. №4(65). S. 65–69.
  4. Kablov E.N. Materialy i himicheskie tehnologii dlja aviacionnoj tehniki [Materials and chemical technologies, aircraft] //Vestnik Rossijskoj akademii nauk. 2012. T. 82. №6. S. 520–530.
  5. Guljaev I.N., Zelenina I.V., Raskutin A.E. Ugleplastiki na osnove uglerodnyh tkanej importnogo proizvodstva i rossijskih rastvornyh svjazujushhih [Carbon composites based on carbon fabrics imported and Russian mortar binders] //Voprosy materialovedenija. 2014. №1(77). S. 116–125.
  6. Kogan D.I., Chursova L.V., Petrova A.P. Tehnologija izgotovlenija PKM sposobom propitki plenochnym svjazujushhim [Manufacturing technology PKM impregnation method bonding film] //Klei. Germetiki. Tehnologii. 2011. №6. S. 25–29.
  7. Dushin M.I., Hrul'kov A.V., Muhametov R.R. Vybor tehnologicheskih parametrov avtoklavnogo formovanija detalej iz polimernyh kompozicionnyh materialov [The choice of process parameters autoclave molding parts from polymeric composite materials] //Aviacionnye materialy i tehnologii. 2011. №3. S. 20–26.
  8. Kogan D.I., Chursova L.V., Petrova A.P. Polimernye kompozicionnye materialy, poluchennye putem propitki plenochnym svjazujushhim [Polymer composite materials obtained by impregnating the film binder] //Vse materialy. Jenciklopedicheskij spravochnik. Kompozicionnye materialy. 2011. №11. S. 2–6.
  9. Chursova L.V., Dushin M.I., Hrul'kov A.V., Muhametov R.R. Osobennosti tehnologii izgotovlenija detalej iz kompozicionnyh materialov metodom propitki pod davleniem [Features of technology manufacturing parts made of composite materials by pressure impregnation] /V sb. tezisov dokladov mezhotraslevoj nauch.-tehnich. konf. «Kompozicionnye materialy v aviakosmicheskom materialovedenii». M.: VIAM. 2009. S. 17.
  10. Hrul'kov A.V., Dushin M.I., Popov Ju.O., Kogan D.I. Issledovanija i razrabotka avto-klavnyh i bezavtoklavnyh tehnologij formovanija PKM [Research and development autoclave and non-autoclave molding technology PKM] //Aviacionnye materialy i tehnologii. 2012. №S. S. 292–301.
  11. Timoshkov P.N., Kogan D.I. Sovremennye tehnologii proizvodstva polimernyh kompozicionnyh materialov novogo pokolenija [Modern production technology of polymer composite materials of new generation] //Trudy VIAM. 2013. №4 (viam-works.ru).
  12. Muhametov R.R., Ahmadieva K.R., Kim M.A., Babin A.N. Rasplavnye svjazujushhie dlja perspektivnyh metodov izgotovlenija PKM novogo pokolenija [Melt binders promising methods of manufacture of a new generation of PCM] //Aviacionnye materialy i tehnologii. 2012. №S. S. 260–265.
  13. Muhametov R.R., Ahmadieva K.R., Chursova L.V., Kogan D.I. Novye polimernye svjazujushhie dlja perspektivnyh metodov izgotovlenija konstrukcionnyh voloknistyh PKM [New polymeric binders for advanced manufacturing methods of structural fiber PKM] //Aviacionnye materialy i tehnologii. 2011. №2. S. 38–42.
  14. Babin A.N. Svjazujushhie dlja polimernyh kompozicionnyh materialov novogo pokolenija [Binders for polymeric composite materials of new generation] //Trudy VIAM. 2013. №4 (viam-works.ru).
  15. Efimov V.A., Shvedkova A.K., Koren'kova T.G., Kirillov V.N. Issledovanie polimernyh konstrukcionnyh materialov pri vozdejstvii klimaticheskih faktorov i nagruzok v laboratornyh i naturnyh uslovijah [The study of polymeric structural materials under the influence of climatic factors and stress in laboratory and field conditions] //Aviacionnye materialy i tehnologii. 2013. №S2. S. 68–73.
  16. Kablov E.N., Starcev O.V., Krotov A.S., Kirillov V.N. Klimaticheskoe starenie kompozicionnyh materialov aviacionnogo naznachenija. III. Znachimye faktory starenija [Climatic aging of composite materials aviation applications. III. Significant factors of aging] //Deformacija i razrushenie materialov. 2011. №1. S. 34–40.
  17. Kablov E.N., Starcev O.V., Krotov A.S., Kirillov V.N. Klimaticheskoe starenie kompozicionnyh materialov aviacionnogo naznachenija. I. Mehanizmy starenija [Climatic aging of composite materials aviation applications. I. Mechanisms of aging] //Deformacija i razrushenie materialov. 2010. №11. S. 19–27.
  18. Kirillov V.N., Starcev O.V., Efimov V.A. Klimaticheskaja stojkost' i povrezhdaemost' polimernyh kompozicionnyh materialov, problemy i puti reshenija [Weather resistance and defectiveness of polymer composite materials, problems and solutions] //Aviacionnye materialy i tehnologii. 2012. №S. S. 412–423.
  19. Kirillov V.N., Efimov V.A., Shvedkova A.K., Nikolaev E.V. Issledovanie vlijanija klimaticheskih faktorov i mehanicheskogo nagruzhenija na strukturu i mehanicheskie svojstva PKM [Investigation of the influence of climatic factors and mechanical loading on the structure and mechanical properties of the PKM] //Aviacionnye materialy i tehnologii. 2011. №4. S. 41-45.