Abstract

VKS-180-ID steel is recommended for production of high-loaded parts, landing gears, airframe and engine. Metallurgical characteristics of high-strength maraging steel VKS-180-ID melt in a vacuum induction furnace (VI) with the subsequent remelting in a vacuum arc furnace (VA) using the chosen system of REM-based micro-alloying and addition of nickel oxide were studied. The technology allows production of steels with a low content of gases and impurities (carbon ≤0.005%; oxygen ≤0.004%; nitrogen ≤0.003%) providing a high level of mechanical properties both in longitudinal and in transverse directions (tensile strength, impact strength, ductility).

Reference list
  1. Kablov E.N., Ospennikova O.G., Bazyleva O.A. Materialy dlja vysokoteplonagruzhennyh detalej gazoturbinnyh dvigatelej [Materials for high-thermal components of gas turbine engines] //Vestnik MGTU im. N.Je. Baumana. Ser. «Mashinostroenie». 2011. №SP2. S. 13–19.
  2. Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih perera-botki na period do 2030 goda [Strategic directions of development of materials and technologies to process them for the period up to 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  3. Kablov E.N. Sovremennye materialy – osnova innovacionnoj modernizacii Rossii [Modern materials – the basis of innovative modernization of Russia] //Metally Evrazii. 2012. №3. S. 10–15.
  4. Kablov E.N. Shestoj tehnologicheskij uklad [Sixth technological way] //Nauka i zhizn'. 2010. № 4. S. 2–7.
  5. Kablov E.N., Ospennikova O.G., Vershkov A.V. Redkie metally i redkozemel'nye jelementy – materialy sovremennyh i budushhih vysokih tehnologij [Rare metals and rare earth elements – materials of current and future high-tech] //Trudy VIAM. 2013. №2. St. 01 (viam-works.ru).
  6. Kablov E.N., Ospennikova O.G., Lomberg B.S., Sidorov V.V. Prioritetnye napravlenija razvitija tehnologij proizvodstva zharoprochnyh materialov dlja aviacionnogo dvigatelestroenija [Priority areas for the development of production technology of high-temperature materials for aircraft engine] //Problemy chernoj metallurgii i materialovedenija. 2013. №3. S. 47–54.
  7. Salahova R.K. Korrozionnaja stojkost' stali 30HGSA s «trehvalentnym» hromovym pokrytiem v estestvennyh i iskusstvennyh sredah [The corrosion resistance of steel 30KhGSA with «trivalent» chrome plated in natural and artificial environments] //Aviacionnye materialy i tehnologii. 2012. №2. S. 59–66.
  8. Kablov E.N., Lomberg B.S., Ospennikova O.G. Sozdanie sovremennyh zharoprochnyh materialov i tehnologij ih proizvodstva dlja aviacionnogo dvigatelestroenija [The creation of modern high-temperature materials and production technologies for aviation engine] //Kryl'ja Rodiny. 2012. №3–4. S. 34–38.
  9. Lomberg B.S., Pokrovskij A.A., Topilin V.V., Shherbakov A.I. Vlijanie sposoba pereplava na kachestvo martensitostarejushhej vysokoprochnoj stali [Influence of remelting method on the quality of high-strength steel martensitostareyuschey] //Stal'. 1973. №8 S. 725.
  10. Shherbakov A.I., Lomberg B.S., Oborenkova A.S. Nekotorye zakonomernosti kristallizacii pri JeLP i VDP [Some regularities of crystallization at ELP and VDR] //Special'naja jelektrometallurgija. 1978. № 22. S. 22–40.
  11. Shalin R.E., Shherbakov A.I., Lomberg B.S., Kachanov E.B. Jelektronno-luchevoj pereplav – progressivnyj metod poluchenija vysokokachestvennyh stalej i zharoprochnyh splavov [Electron beam melting – progressive method of obtaining high-quality steels and superalloys] /V sb. Aviacionnye materialy. M.: VIAM. 1978. №3. S. 46–59.
  12. Revjakina O.K. Sklonnost' k teplovomu ohrupchivaniju nerzhavejushhih martensitostarejushhih stalej [Propensity to thermal embrittlement of stainless steels martensitostareyuschih] //MiTOM. 1981. №4. S. 36–39.
  13. Bratuhin A.G., Demchenko O.F., Dolzhenkov N.N., Krivonogov G.S. Vysokoprochnye korrozionnostojkie stali sovremennoj aviacii [High-strength corrosion-resistant steel of modern aviation]. M.: MAI. 2006. S. 112–121, 130–143.
  14. Savvina N.A., Kosarina E.I., Miroshin K.G., Stepanov A.V. Teoreticheskij raschet i prakticheskie sposoby opredelenija verojatnosti obnaruzhenija defektov v aviacionnyh materialah [Theoretical calculations and practical ways to determine the probability of detection of defects in aircraft materials] /V sb. Aviacionnye materialy i tehnologii. M.: VIAM. 2005. №1. S. 16–22.
  15. Krivonogov G.S., Kablov E.N. Granicy zeren i ih rol' v ohrupchivanii vysokoprochnyh korrozionnostojkih stalej [Grain boundaries and their role in the embrittlement of high strength corrosion resistant steels] //Metally. 2002. №1. S. 35–45.
  16. Krivonogov G.S., Kablov E.N. Matematicheskaja model' strukturnoj diagrammy malouglerodistyh korrozionnostojkih stalej i ee primenenie pri razrabotke novyh materialov [A mathematical model of the structural diagram of low carbon stainless steels and its application in the development of new materials] //Metally. 2001. №5. S. 42–48.
  17. Djubanov V.G., Lomberg B.S., Gerasimov T.N., Bol'shov L.A., Shherbakov A.I. Issledovanie vozmozhnosti obezuglerozhivanija stali, raskislennoj titanom i aljuminiem v vakuume [Study of possible decarburization steel deoxidized with titanium and aluminum in vacuo] /V sb. trudov konf. «Sovremennye problemy jelektrometallurgii stali». Cheljabinsk. 1971. S. 53–56.
  18. Erasov V.S., Grinevich A.V., Senik V.Ja., Konovalov V.V., Trunin Ju.P., Nesterenko G.I. Raschetnye znachenija harakteristik prochnosti aviacionnyh materialov [The calculated values of the strength characteristics of aircraft materials] //Aviacionnye materialy i tehnologii. 2012. №2. S. 14–16.
  19. Tonysheva O.A., Voznesenskaja N.M., Eliseev Je.A., Shal'kevich A.B. Novaja vysokoprochnaja jekonomnolegirovannaja azotsoderzhashhaja stal' povyshennoj nadezhnosti [New high sparingly nitrogen-containing steel of high reliability] //Aviacionnye materialy i tehnologii. 2012. №S. S. 84–88.
  20. Vylezhnev V.P., Kokovjakina S.A., Simonov Ju.N., Suhih A.A. Povyshenie harakteristik nadezhnosti martensitostarejushhej stali 03N18K9M5T putem sozdanija struktury tipa «nanotripleks» [Improving the reliability characteristics martensitostareyuschey steel 03N18K9M5T by creating structures such as «nanotripleks»] //MiTOM. 2010. №11. S. 36–39.
  21. Markova E.S., Pokrovskaja N.G., Shal'kevich A.B., Gromov V.I. Martensitostarejushhie stali ‒ novye perspektivnye materialy dlja valov GTD [Martensitostareyuschie steel – new promising materials for turbine engine shafts] //Aviacionnye materialy i teh-nologii. 2012. №S. S. 81–84.
  22. Pokrovskaja N.G., Markova E.S., Shal'kevich A.B. Vysokoprochnye konstrukcionnye martensitostarejushhie stali v aviastroenii [High-strength structural steel in aircraft martensitostareyuschie] //Aviacionnaja promyshlennost'. 2014. №1. S. 24–28.
  23. Markova E.S., Jakusheva N.A., Pokrovskaja N.G., Shal'kevich A.B. Tehnologicheskie osobennosti proizvodstva martensitostarejushhej stali VKS-180 [Technological features of steel production martensitostareyuschey VKS-180] //Trudy VIAM. 2013. №7. St. 01 (viam-works.ru).